U.S. patent application number 13/764956 was filed with the patent office on 2013-08-22 for apparatus for treating a cellulosic feedstock.
This patent application is currently assigned to MASCOMA CANADA INC.. The applicant listed for this patent is MASCOMA CANADA INC.. Invention is credited to Murray J. Burke, Sunalie N. Hillier.
Application Number | 20130213390 13/764956 |
Document ID | / |
Family ID | 41569962 |
Filed Date | 2013-08-22 |
United States Patent
Application |
20130213390 |
Kind Code |
A1 |
Burke; Murray J. ; et
al. |
August 22, 2013 |
APPARATUS FOR TREATING A CELLULOSIC FEEDSTOCK
Abstract
An apparatus for pre-treating a cellulosic feedstock are
disclosed. Embodiments of the apparatus comprise a shell defining a
treatment chamber having a lower inner surface. The treatment
chamber has an inlet and an outlet spaced longitudinally apart from
the inlet to define an axial length. A conveyance member is housed
within the shell and is configured to sweep the lower inner
surface. A plurality of injection ports are provided in at least
one of the shell and the conveyance member.
Inventors: |
Burke; Murray J.;
(Georgetown, CA) ; Hillier; Sunalie N.;
(Georgetown, ON) |
|
Applicant: |
Name |
City |
State |
Country |
Type |
MASCOMA CANADA INC.; |
|
|
US |
|
|
Assignee: |
MASCOMA CANADA INC.
Georgetown
CA
|
Family ID: |
41569962 |
Appl. No.: |
13/764956 |
Filed: |
February 12, 2013 |
Related U.S. Patent Documents
|
|
|
|
|
|
Application
Number |
Filing Date |
Patent Number |
|
|
12181666 |
Jul 29, 2008 |
8449680 |
|
|
13764956 |
|
|
|
|
Current U.S.
Class: |
127/1 |
Current CPC
Class: |
B01J 19/18 20130101;
D21B 1/22 20130101; C12M 45/20 20130101; Y02E 50/16 20130101; D21B
1/16 20130101; C08B 1/00 20130101; C12M 45/02 20130101; C12P
2201/00 20130101; Y02E 50/10 20130101; C12P 7/10 20130101; C13K
1/02 20130101 |
Class at
Publication: |
127/1 |
International
Class: |
B01J 19/18 20060101
B01J019/18 |
Foreign Application Data
Date |
Code |
Application Number |
Jul 24, 2008 |
CA |
2638152 |
Claims
1. An apparatus for treating a cellulosic fiber feedstock,
comprising: a) a shell defining a treatment chamber having a lower
inner surface, the shell having an inlet and an outlet spaced
longitudinally apart from the inlet to define an axial length; b) a
conveyance member housed within the shell and configured to sweep
the lower inner surface; and, c) a plurality of injection ports
provided in at least one of the shell and the conveyance
member.
2. The apparatus of claim 1, wherein the plurality of injection
ports comprises about 1 to 20 injection ports.
3. The apparatus of claim 1, wherein the plurality of injection
ports are positioned along at least a first portion of the axial
length of the shell, the first portion extending from the inlet
towards the outlet.
4. The apparatus of claim 1, wherein the conveyance member
comprises at least a first rotary shaft and a plurality of paddles
joined to the first shaft and extending radially outwardly
therefrom.
5. The apparatus of claim 4, wherein the paddles and the lower
inner surface are configured to maintain a minimum space between
the paddles and the lower inner surface of less than 6.5 mm.
6. The apparatus of claim 4, wherein the paddles comprise blades,
and the blades are generally planar members, having a radially
inner edge attached to stem, a radially outer edge opposite the
radially inner edge, and opposing first and second side edges
extending between the radially inner and outer edges and the
radially outer edge is curved to match an arc swept by the outer
edge when the first shaft rotates.
7. The apparatus of claim 6, wherein each blade is canted, wherein
the first side edge is axially nearer the outlet and rotationally
trailing relative to a second side edge.
8. The apparatus of claim 7, wherein axially adjacent paddles
extend from the shaft at different angular positions around to the
shaft axis.
9. The apparatus of claim 7, wherein the first side edge of one
paddle axially overlaps the second side edge of a next adjacent
paddle.
10. The apparatus of claim 4, wherein the conveyance member
comprises a second shaft, spaced transversely apart from and
extending generally parallel to the first shaft and the lower inner
surface is scallop shaped in transverse section.
11. The apparatus of claim 4, wherein the conveyance member
comprises a second shaft, spaced transversely apart from and
extending generally parallel to the first shaft, each shaft having
a plurality of paddles attached thereto, and the lower inner
surface has a first portion below the first shaft and a second
portion below the second shaft wherein, when viewed in transverse
cross section, each the first portion defines an arc at a constant
distance to the first shaft and the second portion defines an arc
at a constant distance to the second shaft.
12. The apparatus of claim 11, wherein the second shaft rotates in
an opposite direction to the first shaft.
13. The apparatus of claim 4, further comprising a first heated
fluid supply in fluid communication with the injection ports.
14. The apparatus of claim 13, wherein the first heated fluid
supply comprises water heated to from about 60 to about 70.degree.
Celsius.
15. The apparatus of claim 14, wherein the first heated fluid
supply comprises a catalyst.
16. The apparatus of claim 14, further comprising a jacket
surrounding at least a portion of the shell and defining an
enclosure between the jacket and the shell.
17. The apparatus of claim 16, further comprising a second heated
fluid supply associated with the enclosure.
18. The apparatus of claim 17, wherein the second heated fluid
supply comprises steam.
19. The apparatus of claim 17, wherein the shaft comprises a
conduit extending longitudinally therethrough.
20. The apparatus of claim 19, wherein the conveyance member
includes injection ports.
21. The apparatus of claim 20, wherein at least one of the stem and
the paddles comprise injection ports.
22. The apparatus of claim 1, further comprising a moisture sensor
that measures the moisture content of the cellulosic fiber
feedstock and a controller operatively controlling to an amount of
moisture introduced through the injection ports whereby a
predetermined moisture content of the cellulosic fiber feedstock is
obtained at the outlet.
23. The apparatus of claim 22, wherein the moisture sensor is
upstream of the inlet.
24. The apparatus of claim 22, wherein the predetermined moisture
content of the cellulosic fiber feedstock is from 45 to 55 wt %.
Description
CROSS REFERENCE TO RELATED APPLICATIONS
[0001] This application is a division of U.S. patent application
Ser. No. 12/181,666 filed on Jul. 29, 2008, which itself claims the
benefit of priority from Canadian Patent Application No. 2,638,152
filed on Jul. 24, 2008, the specifications of which are
incorporated herein by reference.
FIELD
[0002] The invention relates to a method and apparatus for
preparing a cellulosic feedstock for the subsequent production of a
fermentable sugar stream from the cellulose and hemicellulose in
the cellulosic feedstock wherein the fermentable sugar stream may
be used for subsequent ethanol production. More specifically, the
invention relates to a method and apparatus for treating a
cellulosic feedstock by moistening and heating the cellulosic
feedstock.
BACKGROUND
[0003] Several processes for the production of ethanol are known.
Generally, the production of fuel ethanol involves the fermentation
of sugars with yeast. Typically, the sugars are derived from
grains, such as corn and wheat. The starches in the grains are
subjected to enzymatic hydrolysis in order to produce the sugars,
which are then subjected to fermentation to produce ethanol.
[0004] Plant materials are a significant source of fermentable
sugars, such as glucose that can be transformed into biofuels.
However, the sugars in plant materials are contained in long
polymeric chains of cellulose and hemicellulose. Utilizing current
fermentation processes, it is necessary to break down these
polymeric chains into monomeric sugars, prior to the fermenting
step.
[0005] Recently, processes have been developed for utilizing plant
materials, such as corncobs, straw, and sawdust, to produce sugars
for ethanol fermentation. Such processes typically comprise
pre-treating the feedstock to increase the accessibility of the
cellulose to hydrolysis enzymes, and subjecting the cellulose to
cellulase enzyme systems to convert the cellulose into glucose.
[0006] Methods of converting plant biomass into fermentable sugars
are known in the art and in general comprise two main steps: a
pre-treatment step to activate the plant structure, and an
enzymatic or chemical hydrolysis step to convert the polymeric
chains of cellulose and hemicellulose into monomeric sugars.
Several approaches have been used for the pre-treatment step, e.g.,
autohydrolysis, acid hydrolysis, ammonia activation, kraft pulping,
organic solvent pulping, hot water pre-treatment, ammonia
percolation, lime pre-treatment, caustic soda pulping, or alkali
peroxide pre-treatment. Early pre-treatment steps included grinding
or milling the feedstock into a powder, which was then mixed with
water to form a slurry.
[0007] More recently, solvent based pre-treatments, alkali
pre-treatments, and acidic pre-treatments have also been described.
PCT publication WO/2007/009463 to Holm Christensen describes an
alternate pre-treatment, which does not involve the addition of
acids, bases, or other chemicals. This pre-treatment process
involves soaking the cellulosic material in water, conveying the
cellulosic material through a heated and pressurized reactor, and
pressing the cellulosic material to produce a fiber fraction and a
liquid fraction. During the soaking step, approximately 2.5-3.5 kg
of liquid per 1 kg of fiber is added, and is removed again during
pressing. The overall pre-treatment process can take about 27
minutes.
[0008] Each pre-treatment technology has a different mechanism of
action on the plant structure, inducing either physical and/or
chemical modifications. However, the main objective of the
pre-treatment is to provide accessibility of the plant material to
the enzymes.
SUMMARY
[0009] The commercial viability of a hydrolysis process is
dependent on the character of the feedstock provided to the
hydrolysis unit. Typically, this requires that a feedstock is
activated such that a significant portion (e.g., greater then 75%)
of the cellulose and hemicellulose of the feedstock is accessible
to hydrolysis enzymes. If such an activated feedstock is provided
to an enzymatic hydrolysis unit, then at least 60%, preferably more
than 75% and more preferably over 90% of the cellulose and
hemicelluloses may be converted to monomeric sugars. This sugar
rich process stream may subsequently be subjected to fermentation
to produce an alcohol stream. The alcohol stream from the
fermentation stage (i.e., the raw alcohol stream) may have an
ethanol content of about 3-22% v/v, preferably about 5-15% and more
preferably more about 8-12%.
[0010] An activated feedstock for enzymatic hydrolysis is
preferably prepared by autohydrolysis, which is preferably
conducted in a steam explosion reactor also known as a hydrolyzer,
(also known as a digester). Autohydrolysis is a process of breaking
down hemicellulose and cellulose by exposure to high temperatures,
steam and pressure. When performed in the presence of an added
acid, the reaction is known as acid hydrolysis.
[0011] During autohydrolysis, the degree of polymerization of
cellulose may be reduced from about 10,000 to about 1,500-1,000.
This process is preferably carried out above the glass transition
temperature of lignin (120-160.degree. C.). Depending upon the
severity of the reaction, degradation products may be produced,
such as furfural, hydroxyl-methylfurfural, formic acid, levulinic
acid and other organic compounds.
[0012] During a steam explosion treatment (more commonly called
autohydrolysis if no externally added catalyst), a cellulosic
feedstock is subjected to elevated heat (e.g., 180.degree. C. to
220.degree. C.) and pressure (e.g., 131 psig to 322 psig)
optionally in the presence of suitable chemicals (e.g., organic/
and/or inorganic acids, ammonia, caustic soda, sulfur dioxide,
solvents etc.) in a pressurized vessel. Preferably, external
chemical addition is not utilized, in which case, the only catalyst
that may be present may be acetic acid that is generated in situ.
The treated cellulosic feedstock is then released from the
pressurized vessel such that the pressure is rapidly reduced (e.g.,
1 second or less). The biomass may exit the hydrolyzer into a
reduced pressure, preferably atmospheric pressure and, more
preferably into a vacuum. The rapid decrease in pressure results in
the biomass separating into individual fibers or bundles of fibers.
This step opens the fiber structure and increases the surface area.
The lignin remains in the fiber along with cellulose and residual
hemicellulose. Accordingly, the explosive release of pressure,
combined with the high temperature and pressure treatment results
in the physicochemical modification of the cellulosic feedstock
that is then suitable for feeding to an enzymatic hydrolysis
unit.
[0013] In order for the steam explosion process to be able to
produce an activated feedstock that is capable of producing such a
sugar rich process stream, the temperature and moisture level of
the cellulosic feedstock that is fed to a steam explosion reactor
preferably is relatively uniform and preferably has a temperature
from about 50 to about 70.degree. C., and more preferably
50-65.degree. C., and a moisture content from about 30 to 60 wt %
(preferably 45 to about 55 wt %).
[0014] Without being limited by theory, it is believed that an
unexpected increase in the conversion of the feedstock to
fermentable sugars may be achieved if the moisture content of the
feedstock fed to the steam explosion reactor is lower, provided
that sufficient water is present for hydrolyzing and/or activating
the feedstock. If the feedstock is too dry, then there may be
insufficient water molecules present in the fiber and hence not all
of the feedstock will be activated and/or hydrolyzed (i.e., the
hydrolysis reaction/activation will not occur at all possible
sites). Accordingly, it might be presumed that a substantial excess
of water should be used to ensure water molecules are available at
each hydrolysis/activation site. Surprisingly, it has been
determined that if the cellulosic feedstock that is fed to a steam
explosion reactor has an excess of moisture, then a smaller
percentage of the available sites of the feedstock are activated
and/or hydrolyzed than would be expected. It is believed that this
is due to the high moisture content acting as a barrier to heat
transfer through the fiber structure. The external fiber reaches
the process temperature far in advance to the internal fiber, hence
resulting in very uneven heat transfer and the resulting uneven
autohydrolysis reaction. Further, during the autohydrolysis process
additional water may be provided to the process by way of direct
injected steam in order to raise the fiber temperature from the
inlet temperature to the outlet temperature of the reactor. If the
inlet moisture content of the fiber is at saturation, then the
additional water will be free water in the autohydrolysis reactor
resulting in washing of the soluble hemicellulose from the fiber
and causing subsequent accumulation of hemicellulose within the
reactor. Over time, the accumulated hemicellulose will tend to
break down to inhibitor compounds and deposit degraded sugars on
the internal components of the reactor. These deposits will become
and obstruction to the flow of the biomass.
[0015] It has also been determined that if the cellulosic feedstock
that is fed to a hydrolyzer has a temperature that is too high,
then some percentage of the hemicellulose sugars will be degraded
to inhibitory compounds prior to starting the autohydrolysis
reaction and further amounts during the autohydrolysis reaction
itself. Conversely, if the fiber is too cold entering the
hydrolyzer, the first one third to one half of the reactor vessel
may act as a preheating device rather than as a hydrolyzer,
resulting in incomplete autohydrolysis. Accordingly, it is
preferred to have very consistent fiber temperature year round as
well as from night to day time operation, for the fiber that is fed
to the hydrolyzer reactor. Further, it is preferred that the fiber
in the feedstock fed to the autohydrolysis unit have a relatively
uniform temperature profile. For example, it is preferred that the
core of the blocks of material have a temperature that is within
80%, preferably 90% of the temperature of the exterior surface of
the material. Accordingly, for example, if the temperature of the
exterior surface of the material is from 50 to 70.degree. C., then
the temperature of the core of the material is preferably from 45
to 63.degree. C.
[0016] It has also been determined that the fiber requires time for
the moisture that is added to become equilibrated throughout the
entire fiber particle. It has been determined that under laboratory
conditions, it may take from 5 to 9 minutes to equilibrate the
moisture content of the fiber. Under industrial conditions it will
be longer. Preferably, the autohydrolysis reaction time in the
vessel is typically about 5 to 6 minutes or less. It is preferred
that the fiber in the feedstock fed to the autohydrolysis unit have
a relatively uniform moisture profile. For example, it is preferred
that the core of the blocks of material have a moisture content
that is within 80%, preferably 90% of the moisture content of the
exterior surface of the material. Accordingly, for example, if the
moisture content of the exterior surface of the material is from 45
to 55 wt %, then the moisture content of the core of the material
is preferably from 40.5 to 49.5 wt %.
[0017] Accordingly, embodiments of the present invention relate to
a cellulosic feedstock pre-treatment process, which comprises the
addition of moisture to a cellulosic feedstock, while mixing the
feedstock, to prepare the feedstock for hydrolysis. Subsequent to
this soaking or impregnation stage, it is preferred to subject the
feedstock to an autohydrolysis reaction.
[0018] In one broad aspect, a method is provided for treating a
cellulosic feedstock, such as for subsequent ethanol production.
The method comprises conveying the cellulosic feedstock through an
enclosed volume. The method further comprises adding moisture to
the cellulosic feedstock simultaneously at multiple spaced-apart
moisture injection points as the cellulosic feedstock travels
through the volume, and heating the cellulosic feedstock as it
travels through the volume to obtain a heated moistened feedstock.
In some embodiments, the heated moistened feedstock is subsequently
subjected to hydrolysis, preferably autohydrolysis followed by
enzymatic hydrolysis.
[0019] In some embodiments, the volume comprises an impregnation
chamber defined by chamber walls having an inner surface, and the
impregnation chamber extends longitudinally along an axial length
from an intake to an outlet, and the cellulosic feedstock is urged
through the chamber by a conveyance member.
[0020] In some embodiments, the step of adding moisture comprises
adding moisture to increase the moisture content of the cellulosic
feedstock from about 5-15 wt % to about 45-55 wt %. In some
embodiments, the method further comprises adding heated water as at
least part of the moisture. In some embodiments, the method further
comprises adding a catalyst with the moisture. Preferably, the
heated water is at a temperature up to 70.degree. C. and preferably
about 50-60.degree. C.
[0021] In some embodiments, the step of heating the cellulosic
feedstock comprises heating the cellulosic feedstock from less than
about 30.degree. Celsius at the inlet, to at least about 65.degree.
Celsius at the outlet.
[0022] In some embodiments, the plurality of injection points
comprises a plurality of ports extending through the chamber wall
commencing proximate the inlet and the method further comprising
introducing moisture to the cellulosic feedstock at least during
its initial travel through the impregnation chamber. In some
further embodiments, the injection points are provided in a first
third of the axial length of the impregnation chamber.
[0023] In some embodiments, the step of heating the cellulosic
feedstock comprises heating the cellulosic feedstock to about
50-70.degree. Celsius at the outlet. In some embodiments, the step
of heating the cellulosic feedstock comprises heating the moisture
prior to contacting the moisture with the feedstock.
[0024] In some embodiments, the step of heating the cellulosic
feedstock comprises indirectly heating the cellulosic feedstock by
heating at least one of the chamber walls and the conveyance
member.
[0025] In some embodiments, the conveyance member extends
longitudinally through the impregnation chamber and is configured
to urge the cellulosic feedstock axially through the impregnation
chamber as the conveyance member rotates.
[0026] In some embodiments, the conveyance member comprises a
rotary shaft extending longitudinally through the impregnation
chamber and a plurality of paddles extending radially outwardly
from the shaft, and the method further comprises rotating the shaft
to urge the cellulosic feedstock axially through the impregnation
chamber.
[0027] In some embodiments, the conveyance member includes moisture
injection points, and the method further comprises introducing
moisture to the volume as the conveyance member rotates.
[0028] In some embodiments, the conveyance member includes a fluid
conduit extending longitudinally through the shaft and a plurality
of paddle ducts in communication with the fluid conduit and
extending through the paddle to an outer surface thereof, and the
step of adding moisture to the cellulosic feedstock comprises
injecting moisture into the feedstock through the paddle ducts.
[0029] In some embodiments, the conveyance member comprises a
rotary shaft extending longitudinally through the impregnation
chamber, and a plurality of paddles extending radially outwardly
from the shaft, and the paddles are configured relative to the
impregnation chamber to sweep at least a lower circumferential
portion of the inner surface of the chamber walls when the
feedstock is conveyed through the chamber.
[0030] In some embodiments, the conveyance member comprises a
rotary shaft extending longitudinally through the impregnation
chamber and a plurality of paddles extending radially outwardly
from the shaft and the paddles are spaced and configured such that
the lower circumferential portion of the chamber is swept along
generally the entire axial length of the chamber as the feedstock
is conveyed through the chamber.
[0031] In some embodiments, the volume has a residence time of less
than about ten minutes. Such embodiments may be advantageous
because the process may be substantially fast, and may prevent
overheating of the fibers, thereby preventing degradation of the
fibers.
[0032] In some embodiments, the method further comprises monitoring
the moisture content of the feedstock and introducing an amount of
moisture to produce a predetermined moisture content of the heated
moistened feedstock.
[0033] In some embodiments, the method further comprises providing
a feedstock comprising cellulosic material that has a moisture
content of less than about 50 wt % and comprises fibers that have a
length in the range of about 4 mm to about 7 mm. More preferably,
the feedstock comprises a moisture content from 5 to 45 wt % and
more preferably from 10 to 30 wt %.
[0034] In some embodiments, the method further comprises
subsequently subjecting the cellulosic feedstock to a downstream
hydrolysis process.
[0035] In another broad aspect, an apparatus for treating a
cellulosic fiber feedstock is provided. The apparatus comprises a
shell defining a treatment chamber having a lower inner surface.
The treatment chamber has an inlet and an outlet spaced
longitudinally apart from the inlet to define an axial length. A
conveyance member is housed within the shell and is configured to
sweep the lower inner surface. A plurality of injection ports are
provided in at least one of the shell and the conveyance
member.
[0036] In some embodiments, the plurality of injection ports
comprises about 1 to 20 injection ports.
[0037] In some embodiments, the plurality of injection ports are
positioned along at least a first portion of the axial length of
the shell, wherein the first portion extends from the inlet towards
the outlet.
[0038] In some embodiments, the conveyance member comprises at
least a first rotary shaft and a plurality of paddles joined to the
first shaft and extending radially outwardly therefrom.
[0039] In some embodiments, the paddles and the lower inner surface
are configured to maintain a minimum space between the paddles and
the lower inner surface of less than 6.5 mm.
[0040] In some embodiments, the paddles comprise blades, and the
blades are generally planar members, having a radially inner edge
attached to a stem, a radially outer edge opposite the radially
inner edge, and opposing first and second side edges extending
between the radially inner and outer edges. The radially outer edge
may be curved to match an arc swept by the outer edge when the
first shaft rotates.
[0041] In some embodiments, each blade is canted, wherein the first
side edge is axially nearer the outlet and rotationally trailing
relative to a second side edge.
[0042] In some embodiments, axially adjacent paddles extend from
the shaft at different angular positions around to the shaft
axis.
[0043] In some embodiments, the first side edge of one paddle
axially overlaps the second side edge of a next adjacent
paddle.
[0044] In some embodiments, the conveyance member comprises a
second shaft, spaced transversely apart from and extending
generally parallel to the first shaft and the lower inner surface
is scallop shaped in transverse section.
[0045] In some embodiments, the conveyance member comprises a
second shaft, spaced transversely apart from and extending
generally parallel to the first shaft, each shaft has a plurality
of paddles attached thereto, and the lower inner surface has a
first portion below the first shaft and a second portion below the
second shaft wherein, when viewed in transverse cross section, the
first portion defines an arc at a constant distance to the first
shaft and the second portion defines an arc at a constant distance
to the second shaft.
[0046] In some embodiments, the second shaft rotates in an opposite
direction to the first shaft.
[0047] In some embodiments, the apparatus further comprises a first
heated fluid supply in fluid communication with the injection
ports. In some embodiments, the first heated fluid supply comprises
water heated to a temperature from about 60 to about 70.degree. C.
In some embodiments, the first heated fluid supply comprises a
catalyst.
[0048] In some embodiments, the apparatus further comprises a
jacket surrounding at least a portion of the shell and defining an
enclosure between the jacket and the shell. In some embodiments,
the apparatus further comprises a second heated fluid supply
associated with the enclosure. In some embodiments, the second
heated fluid supply comprises steam.
[0049] In some embodiments, the shaft comprises a conduit extending
longitudinally therethrough. In some further embodiments, the
conveyance member includes injection ports. In yet further
embodiments, at least one of the stem and the paddles comprise
injection ports.
[0050] In some embodiments, the apparatus further comprises a
moisture sensor that measures the moisture content of the
cellulosic fiber feedstock and a controller operatively controlling
an amount of moisture introduced through the injection ports.
Accordingly, a predetermined moisture content of the cellulosic
fiber feedstock is obtained at the outlet. In some embodiments, the
moisture sensor is upstream of the inlet. In some embodiments, the
predetermined moisture content of the cellulosic fiber feedstock is
from 45 to 55 wt %.
[0051] An advantage of this process is that the temperature of the
feedstock may be kept sufficiently low to prevent charring of the
fibers. Charring of the fibers results in degradation of the sugars
in the cellulose and hemicellulose. This degradation reduces the
percentage of sugars that may be liberated for fermentation,
thereby decreasing the possible yield of the process. Further, the
degradation may produce by products that are undesirable in
downstream process streams. Charring may be reduced or prevented by
using a lower temperature water supply to the heating jacket of the
treatment chamber, a lower temperature of the water that is used to
provide moisture and/or by avoiding fibers being retained too long
in contact with a heated wall of the treatment chamber. For
example, if steam is not used to provide moisture to the fibers in
the treatment chamber, but water at, e.g., 50-60.degree. C. is
used, the feedstock will be heated but will not be raised to a
temperature at which degradation may occur.
BRIEF DESCRIPTION OF THE DRAWINGS
[0052] These and other advantages of the present invention will be
more fully and particularly understood in connection with the
following description of the preferred embodiments of the invention
in which:
[0053] FIG. 1 is a perspective illustration of an embodiment of an
apparatus of the present invention;
[0054] FIG. 2 is a front plan view of the apparatus of FIG. 1;
[0055] FIG. 3 is a top plan view of the apparatus of FIG. 1;
[0056] FIG. 4 is a cutaway top plan view of the mixing vessel of
FIG. 1, wherein the upper portion of the shell has been removed
showing a preferred embodiment of a conveyance member;
[0057] FIGS. 5A and 5B are transverse cross-sections taken along
line 5-5 in FIG. 2, showing various rotational positions of an
embodiment of a conveyance member of the present invention;
[0058] FIG. 6 is a perspective illustration of the conveyance
member of FIG. 4;
[0059] FIG. 7A is a perspective illustration of an embodiment of a
paddle of the present invention;
[0060] FIG. 7B is a front plan view of the paddle of FIG. 7A;
[0061] FIG. 7C is a side plan view of the paddle of FIG. 7A;
[0062] FIG. 7D is a top plan view of the paddle of FIG. 7B;
[0063] FIG. 8A is a partial perspective illustration of an
embodiment of a conveyance member of the present invention, wherein
the paddle of the conveyance member comprises injection ports;
[0064] FIG. 8B is a partial front plan view of the paddle of FIG.
8A;
[0065] FIG. 8C is a partial side plan view of the paddle of FIG.
8A; and,
[0066] FIG. 8D is a transverse cross-section taken along line D-D
in FIG. 8A.
DETAILED DESCRIPTION
[0067] Embodiments of the present invention provide a method and
apparatus for treating a cellulosic feedstock for subsequent
ethanol production. The method and apparatus of the preferred
embodiment serve to heat and moisten the cellulosic feedstock to
obtain a relatively uniform temperature and moisture level of the
feedstock, while reducing, and preferably essentially preventing,
the charring or other degradation of the cellulose and
hemicellulose during this heating stage. Accordingly, the method
and apparatus provide a cellulosic feedstock, which is suitable for
the production of a fermentation precursor stream. The cellulosic
feedstock may be subsequently treated to liberate sugars in the
cellulose and hemicellulose and produce a sugar stream that may
then be subjected to fermentation to obtain a high yield alcohol
stream. An embodiment of an apparatus of the present invention is
shown in FIGS. 1-8. It will be appreciated that although the method
is described with reference to apparatus 200 and vice versa, the
method may be carried out with an alternate apparatus, and
apparatus 200 may be used according to an alternate method.
Furthermore, although the method is described as a continuous
process, it will be appreciated that the method may be carried out
as a semi-continuous or batch process.
[0068] The cellulosic feedstock treated according to the method
and/or utilizing apparatus 200 may be preferably a lignocellulosic
feedstock. A lignocellulosic feedstock is derived from plant
materials. As used herein, a "lignocellulosic feedstock" refers to
plant fiber containing cellulose, hemicellulose and lignin. In some
embodiments, the feedstock may be derived from trees, preferably
deciduous trees such as poplar (e.g., wood chips). Alternately or
in addition, the feedstock may also be derived from agricultural
residues such as, but not limited to, corn stover, wheat straw,
barley straw, rice straw, switchgrass, sorghum, bagasse, rice hulls
and/or corn cobs. Preferably, the lignocellulosic feedstock
comprises agricultural residues and wood biomass, more preferably
wood biomass and most preferably deciduous. The applicants
contemplate other sources of plant materials comprising cellulose,
hemicellulose and/or lignin, such as algae, for use in deriving
cellulosic feedstocks and any of those may be used.
[0069] The lignocellulosic feedstock is preferably cleaned, e.g.,
to remove ash, silica, metal strapping (e.g., from agricultural
products), stones and dirt. The size of the components of the
lignocellulosic feedstock may also be reduced. The size of the
components of the feedstock may be from about 0.05 to about 2
inches, preferably from about 0.1 to about 1 inch, and more
preferably from about 0.125 to about 0.5 inches in length. For
example, the cellulosic feedstock may comprise fibers, e.g.,
chopped straw, of a length of between about 4 mm and about 7 mm.
Any process machinery that is able to crush, grind or otherwise
decrease the particle size may be utilized.
[0070] Generally, when the cellulosic feedstock is provided, it
will have an initial or starting moisture content. The initial
moisture content may depend on numerous factors, such as the nature
of the cellulosic feedstock, and any upstream storage conditions.
In some embodiments, the initial moisture content is less than
about 15 wt % and, preferably, from 5-15 wt %. In some embodiments,
at least some moisture may be provided in advance of the
apparatus.
[0071] The method comprises conveying the cellulosic feedstock
through an enclosed volume. The enclosed volume may be of a variety
of configurations. Referring to FIGS. 1-5, in the embodiment shown,
chamber 204 of apparatus 200 comprises an enclosed volume 202.
Chamber 204 may be referred to as an impregnation chamber, or a
treatment chamber.
[0072] In the embodiment shown, chamber 204 is defined by a shell
206, which preferably is provided with a heating jacket 260.
Accordingly, shell 206 preferably comprises an inner wall 208 and a
spaced apart outer wall 209 defining a volume 207 therebetween.
Accordingly, chamber 204 may be a double walled chamber having a
volume 207 through which a heated fluid may be passed from, e.g.,
inlet to the volume 207 to the outlet from the volume. Wall 208 has
an inner surface 210 that encloses chamber 204. It will be
appreciated that a single walled vessel may be used. It will be
appreciated that heating jacket 260 may surround only part of
chamber 204 and may be of any design.
[0073] In some embodiments, an impregnator feeder 262, namely a
feeder that conveys feedstock into chamber 204, is preferably
positioned upstream of mixing or impregnation chamber 204. Feeder
262 may be of any design. Preferably, feeder 262 is of a design
that inhibits, and preferably prevents, the flow of moisture
upstream of feeder 262. For example, a rotating valve or the like
may be provided to segment such upstream flow. Preferably
impregnation feeder is a screw feeder comprising a motor 264
drivingly connected to a screw or auger 266 positioned below an
inlet, such as via a transmission or gear reduction assembly
provided in housing 268. The shaft on which screw 266 is provided
may be rotatably mounted in housing 270 such that auger 266 is a
cantilevered plug screw conveyor. Accordingly, feeder 262 produces
a plug of material that prevents upstream migration of moisture.
The plug may be conveyed into inlet housing 272 that is mounted,
e.g., to outer wall 209 and positioned above inlet 211 to volume
202. The feedstock may then pass downwardly into chamber 204.
[0074] Chamber 204 comprises at least one feedstock inlet 211, and
at least one treated feedstock outlet 213, which may be positioned
above outlet passage 218. Inlet 211 and outlet 213 are spaced
axially apart to define a length L. Length L may vary depending on
the particular embodiment, however, in some embodiments, length L
may be between about 8 ft and about 12 ft. In the embodiment shown,
inlet 211 is defined in upper portion of shell 206, and outlet 213
is defined in lower portion of shell 206. Accordingly, the
cellulosic feedstock is deposited into inlet 211, is conveyed along
the length of chamber 204 and drops out of outlet 213 into optional
outlet passage 1218, which is upstream of optional heated holding
tank 221. In alternate embodiments, inlet 211 and outlet 213 may be
positioned elsewhere, for example at opposed ends of chamber
204.
[0075] In one aspect of the invention, chamber 204 may be of any
configuration that provides a residence time for the feedstock to
be treated (heated and/or provided with moisture) so as to obtain a
treated feedstock having a moisture level and a temperature within
a predetermined range, and which is preferably uniform for the
feedstock exiting the chamber.
[0076] In one particularly preferred aspect, and preferably in
combination with the forgoing aspect, the chamber and a conveyance
member 222 are configured such that the feedstock is moved through
the chamber with a relatively constant residence time. Preferably,
the chamber and a conveyance member 222 are configured such that
the lower surface on which the feedstock may rest under the
influence of gravity is swept such that feedstock will be
continually urged through the chamber.
[0077] As exemplified in FIGS. 1-3, conveyance members 222 are
rotatably mounted in chamber 204 and are drivenly connected to a
motor 278. As exemplified, motor 278 is drivingly connected to
conveyance members 222 via a transmission or gear reduction
assembly provided in housing 280. The gear reduction assembly may
be drivingly connected to ends 225, 227 of conveyance members 222
that are positioned inside housing 282.
[0078] In accordance with this particularly preferred aspect,
chamber 204 extends longitudinally along axis 220 and has an upper
portion that may be substantially cylindrical and a lower portion
formed by wall section 214 that is preferably scallop shaped in
transverse section (see FIGS. 6A and 6B). An advantage of having a
scallop shaped lower section is that a rotary mounted conveyance
member 222 may sweep adjacent all of, or at least much of, lower
wall section 214 to reduce the likelihood of material having an
increased residence time by not being conveyed along wall section
214. In alternate embodiments that are less preferred, chamber 204
may be otherwise shaped. For example, the upper portion may also be
scallop shaped. Alternately, in combination with other aspect of
this invention, the lower portion may be substantially
cylindrical.
[0079] In accordance with this particularly preferred aspect
conveyance member 222 is configured, in conjunction with the
configuration of lower wall section 214, to urge the cellulosic
feedstock through chamber 204 by sweeping lower wall section 214.
That is, conveyance member 222 is preferably configured such that
at least a portion thereof passes over lower inner surface in a
continuous motion to push the cellulosic material forwardly.
Furthermore, conveyance member 222 is preferably configured to
sweep lower wall section 214 along generally the entire axial
length of the chamber. It will be appreciated that, in less
preferred embodiments, lower wall section 214 and conveyance member
222 need not be configured to sweep lower wall section 214 and may
be of a variety of other configurations.
[0080] In the exemplified embodiments, in order to sweep lower wall
section 214 and urge the cellulosic material through chamber 204,
conveyance member 222 comprises first rotary shaft 224 and second
rotary shaft 226, which extend longitudinally through chamber 204,
and which are preferably spaced transversely apart and are
preferably parallel. In alternate embodiments, conveyance member
may comprise only one rotary shaft, or more than two rotary
shafts.
[0081] Shafts 224, 226 may be provided with an auger, a plurality
of paddles or the like. As exemplified, a plurality of paddles 228
extend radially outwardly from each rotary shaft. In addition, as
exemplified in FIGS. 8A-8D, paddles 228 may each comprise a blade
232 and a stem 230, which couples the blade 232 to one of rotary
shafts 226 and 228. Each blade 232 may be generally planar, and
comprise a radially inner edge 234, a radially outer edge 236, and
opposing first 238 and second 240 side edges, which extend between
inner edge 234, and outer edge 236. In other embodiments, the
paddles may be otherwise configured. For example, the blade may
extend directly from the shaft, and a stem may not be provided.
Alternatively, the stem may extend outwardly from the shaft, such
that a space is provided between each blade and the shaft.
[0082] Blade 232 may be secured to one end of stem 230 by any means
known in the art, such as welding, or mechanical affixation members
such as rivets, or screws. The other end of stem 230 may be
provided with a screw thread 276 on which bolt 274 may be received.
Stem 230 may be secured to shaft 224, 226 such as by extending
transversely through shaft 224, 226 from one side to the other and
bolt 274 secured thereon. Suitable packing, gaskets or the like may
be provided to limit or prevent moisture leaking out of shaft 224,
226 past stem 230. Stem 230 may be provided with one or more
openings 258 in fluid communication with volume 256 inside shaft
224, 226. Accordingly, moisture may flow through shaft 224, 226,
through stem 230 to paddle 228 and out through ports 252 into
volume 204. However, paddles 228 may be directly secured to shafts
224, 226 or may be secured by any other means known in the art.
[0083] Preferably, as exemplified in FIG. 7, paddles 228 are
arranged such that they generally define a longitudinally extending
helix extending around each rotary shaft. In other words, a helix
would be defined if the radially outer edge 236 of paddles were
connected by a line extending from the inlet end of a rotary shaft
to the outlet end thereof. Accordingly, helically adjacent paddles
228, for example paddles 228a and 228b, extend from the shaft at
different angular positions around the shaft axis, as can be seen
in FIG. 5.
[0084] Preferably, blades 232 of each paddle 228 are canted. That
is, a first side edge 238 of each blade 232 is axially nearer the
outlet 213 and rotationally trailing relative to a second side edge
240 (see FIG. 5).
[0085] Preferably, when viewed axially along the length of a rotary
shaft, the first side edge of one paddle axially overlaps the
second side edge of a next adjacent paddle.
[0086] In alternate embodiments, the paddles may be otherwise
configured. For example, they may not be canted, and may be wedge
shaped. Additionally, they may, for example, be arranged in a grid
around shafts 226 and 224, rather than in a helix. It will be
appreciated that in a particularly preferred embodiment, the
paddles are arranged to define a helix, the blades are canted and
the first side edge of one paddle axially overlaps the second side
edge of a next adjacent paddle. However, these features may be used
in any particular sub-combination with any aspect of this
invention.
[0087] Accordingly, in the embodiment shown, the step of conveying
the cellulosic feedstock through the enclosed volume 202 comprises
rotating each shaft 224, 226, such that the paddles 228 engage the
cellulosic feedstock and urge the cellulosic feedstock axially
through the chamber 204. Furthermore, in this embodiment, when the
rotary shafts 224, 226 rotate, paddles 228 pass over inner lower
wall section 214 in a continuous motion to push the cellulosic
material forwardly. An advantage of the exemplified design is that
the outer radial edges of the blades are configured to travel a
generally consistent distance above lower wall section 214, thereby
being able to effectively sweep lower wall section 214.
[0088] It will be appreciated that, in alternate embodiments,
conveyance member 222 may be otherwise configured. For example,
conveyance member 222 may comprise an auger which extends along
enclosed volume 202, and which is rotated to urge the cellulosic
feedstock through chamber 204 and sweep lower wall section 214.
[0089] In accordance with this particularly preferred aspect,
paddles 228 and lower wall section 214 are configured such that
when a given paddle is adjacent and passing over lower wall section
214, a substantially constant distance is maintained between the
outer edge 236 of the paddle 228, and lower wall section 214. Such
embodiments may aid in ensuring that the cellulosic material is
urged forwardly at a substantially constant rate, and that the
cellulosic material is not retained in the chamber.
[0090] For example, in the embodiments shown, the outer edge 236 of
each paddle is curved or arcuate in shape (see for example FIG.
7B), and the curve preferably matches an arc 242 swept or defined
by the outer edge 236 as the shafts rotate (see for example FIG.
5A). Accordingly, when shafts 224 and 226 rotate, the outer edge
236 of each paddle 228 will describe a circle. That is, outer edge
236 of each blade 232 is curved to define a sector of a circle
having a radius R1. It will be appreciated that in embodiments
wherein the blades 232 are canted, the arc 242 swept by outer edge
236 will be 3-dimensional (i.e. will have a depth). When shafts 224
and 226 rotate, the outer edge 236 of each blade 232 will describe
a circle having a radius R2 define R2 on the drawings. In
embodiments wherein blades 232 are not canted, R2 will equal R1. In
embodiments wherein blades 232 are canted, R2 will be less than
R1.
[0091] Further, in a preferred aspect, lower wall section 214 is
configured such that in transverse section, as shown in FIGS.
5A-5B, lower wall section 214 defines at least one arc 244 and more
preferably two or more arcs. In the embodiment shown, wherein
conveyance member comprises two rotary shafts, lower wall section
214 defines two arcs 244a, 244b. That is, when viewed in transverse
section, lower wall section 214 is scalloped. In alternate
embodiments, wherein conveyance member comprises a different number
of shafts, lower portion may define a different number of arcs,
preferably one per shaft. Preferably, each shaft is centered above
an arc 244.
[0092] Arcs 244a and 244b have a radius R3. Arc 244a comprises
first portion 246 of lower wall section 214, and arc 244b comprises
second portion 248 of lower wall section 214. First portion 246 is
below first shaft 224, and second portion is below second shaft
226. Blades 232 and portions 246 and 248 are configured such that
R3 is of a slightly greater radius than R2, for example less than
about 6.5 mm greater than R2. Accordingly, when shafts 224 and 226
rotate, the paddles associated with shaft 224 will sweep along
first portion 246, and the paddles associated with shaft 226 will
sweep along second portion 248, such that a distance preferably
less than about 6.5 mm is maintained between outer edge 236 of
paddles 228 and first 246 and second 248 portions of lower wall
section 214 as the paddles pass adjacent to lower wall section 214.
The spacing between radial outer edge 236 and arc 244 may be from 2
to 15 mm. The spacing may vary depending upon the size of the
particulate matter in the feedstock. The larger the size of the
particulate matter, the larger the spacing may be. Preferably, the
spacing is less than the maximum particle size and, more
preferably, less than the median particle size. Accordingly, as the
shafts rotate, particulate matter will be continually moved through
the chamber. Further, if wall section 214 is heated, then the
particulate matter will be inhibited from staying in the same
location and being possibly overheated such that cellulose or
hemicellulose is degraded by heat.
[0093] It will be appreciated that shafts 224, 226 may rotate in
the same direction, or in opposite directions. Further, it will be
appreciated that the rotation of shafts 224, 226 may be driven by a
motor as exemplified, or another suitable means.
[0094] In accordance with a preferred embodiment, moisture is added
to the cellulosic feedstock as the feedstock travels through the
enclosed volume. Preferably, this step comprises adding moisture to
increase the moisture content of the cellulosic feedstock from
between about 5% and about 15 wt % to between about 30 to 60 wt %,
preferably to between 45% and 55 wt %. The moisture may be added as
liquid water, and/or may alternately be added as steam. If liquid
water is used, it is preferably heated, for example, the liquid
water may be heated to between about 50 to 70.degree. C.,
preferably about 60.degree. C. to about 70.degree. C., and more
preferably about 65.degree. C. to about 70.degree. C. It is
preferred not to use steam since steam may result in the
overheating of the cellulose and hemicellulose, causing degradation
thereof. However, if the particularly preferred design exemplified
herein is used, then higher temperatures may be used with reduced
risk of degradation of the feedstock.
[0095] Additionally, the water may comprise additionally
components. For example, one or more catalysts, including but not
limited to mineral and organic acids, bases such as sodium
hydroxide, organic solvents such as ethanol, and oxidizing agents
such as hydrogen peroxide, may be added with the water.
[0096] The moisture may be added upstream from the chamber and/or
in the chamber. The moisture may be added in a variety of ways, and
is preferably added simultaneously at multiple spaced apart
injection points. For example, referring to FIGS. 8A-8D, the
injection points 250 may comprise a plurality of injection ports
252, which are provided in conveyance member 222 and/or in the
inner wall 208 of the shell 206. In the embodiment of FIGS. 8A-8D,
injection ports 252 are defined in blades 232 of paddles 228.
[0097] Alternately, or in addition, injection ports 252 may be
provided in stems 230 and/or in shafts 224, 226. For example, in
some embodiments, injection ports 252 are provided along the entire
length L of chamber 204. In other embodiments, moisture injection
ports 252 are preferably provided only in an upstream portion of
chamber 204, preferably in the upstream half of the length L of
chamber 204 and, more preferably in the first or upstream third
L.sub.1/3 of the length L of chamber 204 (see FIG. 4). For example,
as exemplified in FIG. 1, a plurality of injection ports may be
provided in the upper portion of chamber 204. As shown therein, one
or more conduits 284 may convey water to a plurality of branch
conduits 286 extending to different locations on the upper portion
of chamber 204. The end of these conduits are in fluid flow
communication with the interior of chamber 204, via a moisture
addition member such as a nozzle or an open ended pipe or the like.
As exemplified, six ports are provided. However additional or fewer
ports may be used. Accordingly, moisture injection ports may
additionally or alternately be provided in shell 206 of chamber
204. That is, injection points 250 may extend through wall 208,
which defines inner surface of chamber 204 and/or wall section
214.
[0098] As shown, injection ports 252 of blades 232 are in fluid
communication with one or more paddle ducts 254 provided within
paddles 228. The one or more paddle ducts 254 are in fluid
communication with a fluid conduit 256, which may extend through
shafts 224, 226, for example via ports 258 provided in stem 230.
Fluid conduits 256 are in fluid communication with a moisture
source (not shown), for example at the ends 225, 227, of shafts
224, 226. Accordingly, as the conveyance member rotates, moisture
is introduced into volume 202 by passing from a moisture source
into fluid conduit 256, through ports 258 in stem 230, through
paddle ducts 254, and out of ports 252.
[0099] In the above embodiments, the injection points may be
positioned in a variety of configurations. In some embodiments, the
injection points may be provided such that moisture is introduced
into the cellulosic feedstock during its entire travel through
chamber 204. For example, injection ports may be provided in shell
206 and/or in conveyance member 222 along the entire length of
chamber 204. Preferably, the injection points may be provided such
that moisture is introduced into the cellulosic feedstock during
its initial travel through chamber 204. For example, the injection
points may be provided only in a first portion, for example a first
half and, more preferably, the first third, of the axial length of
the impregnation chamber.
[0100] Furthermore, the number of injection points may vary
depending on the particular embodiment. In some embodiments,
wherein the injection points are provided in blades 232, each blade
preferably comprises at least one injection port. In other
embodiments, only some blades may comprise injection ports.
Furthermore, in some embodiments, each blade comprises two
injection ports; however in alternate embodiments, each blade may
comprise one injection port, or greater than two injection ports.
In some particular embodiments, chamber 204 is provided with a
total of between 1 and 10 injection points.
[0101] In the preferred embodiment, the method optionally further
comprises monitoring the moisture content of the feedstock as it
passes through the volume. Accordingly, the amount of moisture
introduced may be controlled in order to produce a feedstock having
a predetermined moisture content. For example, one or more moisture
sensors (not shown) may be positioned within chamber 204, for
example upstream from inlet 211. As the feedstock passes through
the chamber, the moisture sensors may measure the moisture content
at various positions along the length of the chamber. When the
moisture content of the feedstock reaches a predetermined value,
for example between about 45% and about 55%, the addition of
moisture to the chamber may be halted or reduced. In a further
preferred embodiment, a controller (not shown) is operatively
coupled to the moisture sensor(s) and controls the amount of
moisture introduced based on the moisture content measured by the
moisture sensor.
[0102] Alternately, and preferably in addition, the method also
comprises heating the cellulosic feedstock as it travels through
the volume. In some embodiments, the cellulosic feedstock is heated
such that, when the feedstock exits the volume, the feedstock is at
a temperature of between about 50 to about 65.degree. C.,
preferably about 50.degree. C. to about 70.degree. C. when it exits
outlet 213. Preferably, the cellulosic feedstock is provided to
inlet 211 at less than about 30.degree. C., and is heated to at
least about 65.degree. C. as it travels through the volume.
[0103] The cellulosic feedstock may be heated in a variety of ways.
In some embodiments, the cellulosic feedstock may be heated
directly. For example, as previously mentioned, in some
embodiments, the moisture may be added as heated water. In such
embodiments, in addition to providing moisture to the cellulosic
feedstock, the heated water may serve to heat the cellulosic
feedstock. Accordingly, in such embodiments, the method may
comprise heating the moisture prior to contacting the moisture with
the feedstock.
[0104] In other embodiments, the cellulosic feedstock may be heated
indirectly. For example, the chamber walls 208 and/or the
conveyance member may be heated. Referring to FIGS. 4 and 5, in the
embodiments shown, the chamber walls 208 are heated by providing an
outer wall 209, which surrounds at least a portion of shell 206. An
enclosure 207 is defined between outer wall 209 and inner wall 208,
and a heated fluid supply is associated with the enclosure.
Enclosure 207 is in fluid communication at one end with one or more
inlets, to which a heated fluid is supplied, and at the other end
with one or more outlets, to which spent heated fluid is directed.
Accordingly, the heated fluid circulates within enclosure 207, and
provides heat to the cellulosic feedstock. The heated fluid may be
water, for example, or steam. Any heating jacket or the like known
in the art may be used.
[0105] The conveyance member preferably rotates at from 40 to 150
rpm and, more preferably, 45 to 75 rpm. Alternately, or in
addition, the chamber may operate at a low fill factor, for example
from 10 to 50 and preferably about 30%. Accordingly, a majority of
the volume in chamber 204 may be filled with air. For example, if
the fill factor is about 15-30%, then only 30% of the volume of
chamber 204 is filled with feedstock, the rest being filled with,
preferably air. As the conveyance member rotates, preferably at a
relatively high speed, the feedstock will be thrown up into the
empty upper portion of chamber 204 thereby mixing the feedstock to
provide a more uniform distribution of heat and/or moisture
throughout the feedstock. It will be appreciated that the use of a
high rotational speed, combined with a low fill factor permits the
use of a higher temperature in the heating jacket and/or in the
temperature of the moisture provided to the feedstock in the
chamber with reduced risk of heat degradation of the feedstock.
[0106] Accordingly, in one aspect, heat and/or moisture may be
added in a chamber 204 and/or upstream thereof, wherein the
conveyance member and the floor of the chamber are configured to
permit the conveyance member to sweep the floor.
[0107] In another aspect, a chamber is utilized with a low fill
volume and preferably a high rotational rate of the conveyance
member to permit a higher heating temperature to be used with
reduced risk of degradation of the cellulose and hemicellulose in
the feedstock.
[0108] The cellulosic feedstock is preferably then subjected to
activation and hydrolysis. The activation is preferably conducted
by autohydrolysis. Autohydrolysis may be carried out directly after
the treated feedstock exits the chamber or after a number of
intermediate steps. For example, from outlet, the cellulosic
feedstock may be directed to a holding tank 221 where it is stored
for a period of time at an elevated temperature to further enhance
the uniformity of the moisture and heat distribution, prior to
being passed to an autohydrolysis reactor.
[0109] Accordingly, embodiments of the present invention provide a
method and apparatus for heating and moistening a cellulosic
feedstock, such that the cellulose of the feedstock is
substantially accessible to hydrolysis enzymes. Furthermore,
embodiments of the present invention provide a method and apparatus
for heating and moistening a cellulosic feedstock while requiring
substantially small amounts of heat and water. Accordingly, the
process is substantially cost effective and energy efficient.
[0110] It will be appreciated that certain features of the
invention, which are, for clarity, described in the context of
separate embodiments or separate aspects, may also be provided in
combination in a single embodiment. Conversely, various features of
the invention, which are, for brevity, described in the context of
a single embodiment or aspect, may also be provided separately or
in any suitable sub-combination.
[0111] Although the invention has been described in conjunction
with specific embodiments thereof, if is evident that many
alternatives, modifications and variations will be apparent to
those skilled in the art. Accordingly, it is intended to embrace
all such alternatives, modifications and variations that fall
within the spirit and broad scope of the appended claims. In
addition, citation or identification of any reference in this
application shall not be construed as an admission that such
reference is available as prior art to the present invention.
* * * * *