U.S. patent application number 12/653465 was filed with the patent office on 2013-06-20 for uniform field magnetization and targeting of therapeutic formulations.
This patent application is currently assigned to The Trustees of the University of Pennsylvania. The applicant listed for this patent is Michael Chorny, Elizabeth Hood, Robert J. Levy, Vladimir Muzykantov. Invention is credited to Michael Chorny, Elizabeth Hood, Robert J. Levy, Vladimir Muzykantov.
Application Number | 20130156792 12/653465 |
Document ID | / |
Family ID | 44167649 |
Filed Date | 2013-06-20 |
United States Patent
Application |
20130156792 |
Kind Code |
A9 |
Levy; Robert J. ; et
al. |
June 20, 2013 |
Uniform field magnetization and targeting of therapeutic
formulations
Abstract
Systems and methods for magnetic targeting of therapeutic
particles are provided. Therapeutic particles comprise one or more
magnetic or magnetizable materials and at least one therapeutic
agent. Therapeutic particles are specifically targeted using
uniform magnetic fields capable of magnetizing magnetizable
materials, and can be targeted to particular locations in the body,
or can be targeted for capture, containment, and removal.
Therapeutic particles can comprise antioxidant enzymes, and can be
targeted to cells to protect the cells from oxidative damage.
Inventors: |
Levy; Robert J.; (Merion
Station, PA) ; Chorny; Michael; (Huntingdon Valley,
PA) ; Muzykantov; Vladimir; (Warwick, PA) ;
Hood; Elizabeth; (Philadelphia, PA) |
|
Applicant: |
Name |
City |
State |
Country |
Type |
Levy; Robert J.
Chorny; Michael
Muzykantov; Vladimir
Hood; Elizabeth |
Merion Station
Huntingdon Valley
Warwick
Philadelphia |
PA
PA
PA
PA |
US
US
US
US |
|
|
Assignee: |
The Trustees of the University of
Pennsylvania
Philadelphia
PA
The Children's Hospital of Philadelphia
Philadelphia
PA
|
Prior
Publication: |
|
Document Identifier |
Publication Date |
|
US 20100260780 A1 |
October 14, 2010 |
|
|
Family ID: |
44167649 |
Appl. No.: |
12/653465 |
Filed: |
December 15, 2009 |
Related U.S. Patent Documents
|
|
|
|
|
|
Application
Number |
Filing Date |
Patent Number |
|
|
12150864 |
May 1, 2008 |
|
|
|
12653465 |
|
|
|
|
PCT/US07/09603 |
Apr 20, 2007 |
|
|
|
12150864 |
|
|
|
|
11250948 |
Oct 14, 2005 |
7846201 |
|
|
PCT/US07/09603 |
|
|
|
|
11250948 |
Oct 14, 2005 |
7846201 |
|
|
11250948 |
|
|
|
|
PCT/US04/11861 |
Apr 16, 2004 |
|
|
|
11250948 |
|
|
|
|
60941058 |
May 31, 2007 |
|
|
|
60794191 |
Apr 21, 2006 |
|
|
|
60546233 |
Feb 20, 2004 |
|
|
|
Current U.S.
Class: |
424/172.1 ;
424/130.1; 424/178.1; 424/94.4; 435/173.5; 600/12; 604/500;
623/1.42 |
Current CPC
Class: |
A61K 9/5169 20130101;
A61K 47/59 20170801; A61L 2300/624 20130101; C12N 2710/10343
20130101; A61K 9/5146 20130101; A61K 47/6921 20170801; A61K 48/0083
20130101; A61P 39/06 20180101; A61K 47/6455 20170801; A61K 47/6937
20170801; A61K 9/5094 20130101; A61L 2300/416 20130101; C12N
2320/32 20130101; A61L 2300/60 20130101; A61K 9/5115 20130101; A61L
31/16 20130101; A61K 9/5192 20130101; A61P 43/00 20180101; A61K
47/645 20170801; A61K 47/6849 20170801; A61K 9/5123 20130101; A61K
48/0041 20130101; A61K 9/5153 20130101; A61K 47/42 20130101; A61P
9/00 20180101; A61K 48/0008 20130101; C12N 15/86 20130101; C12N
15/111 20130101 |
Class at
Publication: |
424/172.1 ;
600/12; 623/1.42; 604/500; 424/94.4; 424/130.1; 424/178.1;
435/173.5 |
International
Class: |
A61K 39/44 20060101
A61K039/44; A61F 2/82 20060101 A61F002/82; C12N 13/00 20060101
C12N013/00; A61K 38/44 20060101 A61K038/44; A61P 43/00 20060101
A61P043/00; A61N 2/10 20060101 A61N002/10; A61M 31/00 20060101
A61M031/00 |
Goverment Interests
STATEMENT OF GOVERNMENT SUPPORT
[0002] Research leading to the disclosed inventions was funded, in
part, with funds from the National Institutes of Health, Grant No.
HL72108, The National Heart Lung and Blood Institute, and the
National Science Foundation, Grant No. 9984276. Accordingly, the
United States Government may have certain rights in the invention.
Claims
1. A therapeutic particle comprising a magnetic or magnetizable
material, a stabilizer, a fatty acid or salt thereof, and a
protein.
2. The therapeutic particle of claim 1, wherein the magnetic or
magnetizable material is a superparamagnetic material.
3. The therapeutic particle of claim 1, wherein the fatty acid is
oleic acid or a salt thereof.
4. The therapeutic particle of claim 1, wherein the protein is an
antioxidant enzyme.
5. The therapeutic particle of claim 4, wherein the antioxidant
enzyme is catalase, superoxide dismutase, or glutathione
peroxidase.
6. The therapeutic particle of claim 1, wherein the stabilizer is
biotinylated.
7. The therapeutic particle of claim 1, further comprising an
antibody.
8. The therapeutic particle of claim 7, wherein the antibody is
joined to the stabilizer.
9. The therapeutic particle of claim 7, wherein the antibody
specifically binds to an antigen on the surface of an endothelial
cell.
10. A method for protecting a cell from oxidative damage,
comprising contacting the cell with a particle comprising a
magnetic or magnetizable material and at least one antioxidant
enzyme, and generating a uniform magnetic field capable of
magnetizing the magnetic or magnetizable material proximal to the
cell for a period of time sufficient to permit the cell to
internalize the particle.
11. The method of claim 10, wherein the cell is an endothelial
cell.
12. The method of claim 11, wherein the endothelial cell is a
vascular endothelium cell.
13. The method of claim 10, wherein the antioxidant enzyme is
catalase, superoxide dismutase, or glutathione peroxidase.
14. The method of claim 10, wherein the particle further comprises
an antibody that specifically binds to an antigen on the surface of
the cell.
15. The method of claim 10, wherein the cell is in the body of a
mammal.
16. A method for magnetically targeting a protein to an implanted
device, comprising the steps of: (a) administering to a subject
having an implanted device a plurality of particles comprising a
first magnetic or magnetizable material and the protein; (b)
generating a uniform magnetic field capable of magnetizing
magnetizable materials, the uniform magnetic field generating a
magnetic field gradient proximal to the implanted device, the
implanted device comprising a second magnetic or magnetizable
material, wherein the gradient targets one or more of the plurality
of particles to the implanted device; and (c) optionally removing
one or more of the plurality of particles that are not delivered to
the implanted device from the subject.
17. The method of claim 16, further comprising the step of removing
spent particles from the subject.
18. The method of claim 16, wherein the protein is an antioxidant
enzyme.
19. The method of claim 18, wherein the antioxidant enzyme is
catalase, superoxide dismutase, or glutathione peroxidase.
20. The method of claim 16, wherein each of the plurality of
particles is the particle of claim 1.
21. The method of claim 16, wherein the implanted device is a
stent.
22. The method of claim 21, wherein the stent is formed of 304
stainless steel.
23. The method of claim 16, wherein the step of generating a
uniform magnetic field comprises using a pair of electromagnets to
generate the uniform magnetic field.
24. The method of claim 16, wherein the step of generating a
uniform magnetic field comprises using a permanent magnet to
generate the uniform magnetic field.
25. The method of claim 16, wherein the first magnetic or
magnetizable material comprises a superparamagnetic material.
26. The method of claim 16 further comprising the steps of: (a)
removing the uniform magnetic field and magnetic field gradient;
(b) administering to the subject another plurality of particles
comprising the first magnetic or magnetizable material and the
protein; (c) repeating the step of generating a uniform magnetic
field to generate a magnetic field gradient proximal to the
implanted device to target one or more of the second plurality of
particles to the implanted device and deliver an additional
quantity of the protein to the device.
27. The method of claim 16 further comprising the step of
administering to the subject a plurality of particles comprising
the first magnetic or magnetizable material and paclitaxel.
28. The method of claim 16 wherein the plurality of particles
comprising the first magnetic or magnetizable material further
comprises paclitaxel.
29. The therapeutic particle of claim 1, further comprising
paclitaxel.
Description
CROSS REFERENCE TO RELATED APPLICATIONS
[0001] This application is a continuation-in-part of U.S.
application Ser. No. 12/150,864, filed May 1, 2008, which claims
priority to U.S. Application No. 60/941,058, filed May 31, 2007 and
which is a continuation-in-part of PCT application US2007/009603,
filed Apr. 20, 2007, which claims priority to U.S. Application No.
60/794,191, filed Apr. 21, 2006, and a continuation-in-part of U.S.
application Ser. No. 11/250,948, filed Oct. 14, 2005. The
disclosures of each of these applications are incorporated by
reference herein, in their entirety and for all purposes.
FIELD OF THE INVENTION
[0003] This invention relates generally to the field of biotherapy.
More specifically, the invention relates to the use of uniform
magnetic fields to induce magnetization of magnetizable objects and
generate magnetic field gradients. The resultant gradients can be
used for magnetic targeting of magnetized or magnetizable
nanoparticle therapeutic agents within the body of a subject.
BACKGROUND OF THE INVENTION
[0004] Various publications, including patents, published
applications and scholarly articles, are cited throughout the
specification. Each of these publications is incorporated by
reference herein, in its entirety.
[0005] Therapeutic agents delivered in a conventional or
non-specific manner often are distributed to non-designated areas
of the body. As a consequence, the agent may be metabolized, for
example, through first pass metabolism of the liver, thereby
resulting in diminished bioavailability and the possibility for
increased dosing at a higher cost and with the risk of adverse side
effects. In addition, non-specific distribution of therapeutic
agents may result in adverse effects and unwanted pharmacological
responses in the subject to which they are administered. As a
result, certain agents may be contraindicated in certain subjects
or under certain conditions.
[0006] Implanting medical devices within a subject may necessitate
follow-up chemotherapy, for example, to lessen the possibility for
infection, to reduce inflammation, to repair tissue, or to prevent
further local tissue damage. Drug-eluting devices, including
stents, are increasingly used in a variety of biomedical
applications to effectuate targeted delivery of drugs to the area
of the implant. Drug-containing implants are limited, however,
insofar as they generally contain only a small dose of a single
therapeutic agent, and therefore lack the possibility for
re-administration of the same or different therapeutic agent
through the implanted device.
[0007] Nanoparticles and microparticles have shown potential as
carrier systems for a variety of therapeutic agents, including
enzymes for enzyme replacement therapy, hormones, cell modifying
agents and genetic material as well as for imaging. Initial
attempts to use nanoparticles and microparticles for site-specific
delivery have shown potential to lower adverse effects in the
patients to which they are administered, attributed in part to
lower doses of therapeutic agents being required.
[0008] The foregoing discussion indicates that carrier systems show
promise for optimizing agent administration, and as a possible
vehicle for targeted drug delivery. Such technology is limited,
however, in its capacity to actually effectuate optimized targeted
delivery. In this regard, magnet targeting is considered an
attractive way to achieve optimized targeted delivery of agents,
particularly those formulated as a nanoparticle carrier.
Preliminary attempts to deliver magnetized therapeutic agents or
agent-containing magnetic carriers to specific locations in the
body have shown promise, see U.S. Pat. No. 5,921,244. These
methodologies, however, suffer from a major drawback, namely that
this approach is restricted to targets that are close to the
surface of the body.
[0009] Thus, a need exists for an optimized and efficacious
targeting using magnetic carriers. It is desired that therapeutic
systems allow for peripheral as well as local administration, and
that the therapeutic system allow practioners to administer doses
of agents that lessen untoward effects in patients, as well as
allow administration of agents to patients in situations where they
may otherwise be contraindicated due to the possibility of
non-specific distribution or of high dose requirements. There is a
further need to be able to remove unused or spent magnetic carriers
to further lessen the possibility for untoward effects on the
patient.
SUMMARY OF THE INVENTION
[0010] The invention features systems for magnetically targeting
therapeutic particles. Generally, the systems comprise a particle
comprising at least one therapeutic agent and a first magnetic or
magnetizable material, an implantable device such as a stent
comprising a second magnetic or magnetizable material, and a
retrieval system comprising a third magnetic or magnetizable
material capable of being reversibly connected to a subject. In
some aspect, the systems further comprise at least one magnetic
field generator configured to generate a uniform magnetic field
capable of magnetizing magnetizable material. The uniform magnetic
field can generates at least one directable magnetic field
gradient. The gradient can direct the particle to the device as
well as direct any spent particles or particles that are not
delivered to the device to the retrieval system. The magnetic field
gradient can be generated proximal to the device and/or proximal to
the retrieval system. The therapeutic agent can be any agent
suitable to the therapeutic purpose to which it is being used, and
can comprise a pharmaceutical, biomolecule, or cell, among other
things. In some highly preferred aspects, the agent is a
biomolecule such as a nucleic acid, and in particular a regulatory
nucleic acid such as siRNA, shRNA, or miRNA. In some highly
preferred aspects, the agent is a biomolecule such as a protein,
preferably an enzyme, and more preferably an antioxidant enzyme. In
some highly preferred aspects, the agent is a cell such as an
endothelial cell, and in particular, a vascular endothelium
cell.
[0011] The invention also features methods for magnetically
targeting a therapeutic particle to an implanted device such as a
stent. Generally, the methods can comprise administering to a
subject having an implanted device a particle comprising at least
one therapeutic agent and a first magnetic or magnetizable
material, generating a uniform magnetic field capable of
magnetizing magnetizable materials, and, optionally, removing
particles not delivered to the implanted device. In some aspects,
the uniform magnetic field generates a magnetic field gradient
proximal to the implanted device comprising a second magnetic or
magnetizable material. In some aspects, the gradient targets the
particle to the implanted device. The methods can further comprise
removing spent particles. The therapeutic agent can be any agent
suitable to the therapeutic purpose to which it is being used, and
can comprise a pharmaceutical, biomolecule, or cell, among other
things. In some highly preferred aspects, the agent is a
biomolecule such as a nucleic acid, and in particular a regulatory
nucleic acid such as siRNA, shRNA, or miRNA. In some highly
preferred aspects, the agent is a biomolecule such as a protein,
preferably an enzyme, and more preferably an antioxidant enzyme. In
some highly preferred aspects, the agent is a cell such as an
endothelial cell, and in particular, a vascular endothelium
cell.
[0012] In some aspects of the inventive methods, removing particles
not delivered to the implanted device comprises reversibly
connecting a third magnetic or magnetizable material to the subject
and generating a second magnetic field gradient proximal to the
third magnetic or magnetizable material. The second magnetic field
gradient can target the particles to the third magnetic or
magnetizable material. It is highly preferred that the third
magnetic or magnetizable material is reversibly connected to at
least one blood vessel of the subject. In other aspects, removing
particles not delivered to the implanted device can comprise
removing the blood of the subject, contacting the blood with a
third magnetic or magnetizable material, generating a second
magnetic field gradient proximal to the third magnetic or
magnetizable material, and returning the blood to the subject. The
second magnetic field gradient can target particles to the third
magnetic or magnetizable material. Preferably, the returned blood
is substantially free of particles, and more preferably is free of
particles.
[0013] In some aspects of the inventive methods, removing spent
particles can comprise reversibly connecting a third magnetic or
magnetizable material to the subject and generating a second
magnetic field gradient proximal to the third magnetic or
magnetizable material. The second magnetic field gradient targets
the spent particles to the third magnetic or magnetizable material.
In other aspects, removing spent particles can comprise removing
the blood of the subject, contacting the blood with a third
magnetic or magnetizable material, generating a second magnetic
field gradient proximal to the third magnetic or magnetizable
material, and returning the blood to the subject. The second
magnetic field gradient targets the spent particles to the third
magnetic or magnetizable material. Preferably, the returned blood
is substantially free of the spent particles.
[0014] The invention also features methods for preparing
nanoparticles. The methods can comprise providing a first aqueous
solution comprising a water soluble salt of a mono-carboxylic fatty
acid or a lipid mono-phosphate, a stabilizer such as albumin or
Pluronic F-127.RTM., and at least one therapeutic agent, and adding
to the first aqueous solution a second aqueous solution comprising
a polyvalent biocompatible cation such as calcium or zinc. The
therapeutic agent can be taxol or all-trans retinoic acid. The
water soluble salt of the fatty acid or the lipid mono-phosphate
can be sodium oleate. The first aqueous solution can further
comprise magnetic nanocrystals. The second aqueous solution can
further comprise at least one cationic polypeptide such as
poly-L-arginine. In some aspects, the methods further comprise
forming the magnetic nanocrystals in the first aqueous
solution.
[0015] The invention further provides therapeutic particles. These
particles can comprise a stabilizer, a magnetic or magnetizable
material, a fatty acid or salt thereof, and a protein. The magnetic
or magnetizable material can be a superparamagnetic material. The
fatty acid can comprise any number of carbons, and can be, for
example oleic acid or a salt thereof, for example, a calcium salt
of oleic acid. The protein can be an enzyme, and more preferably
can be an antioxidant enzyme. The antioxidant enzyme can be
catalase, superoxide dismutase, or glutathione peroxidase. The
stabilizer can be biotinylated.
[0016] The therapeutic particles can further comprise one or more
antibodies. The antibodies can facilitate delivery of the particles
to a particular targeted cell or tissue, in vitro or, preferably,
in vivo. The antibody can be directly incorporated into the
particle, or can be coated on the surface of the particle. The
antibody can be joined to avidin or streptavidin, and incorporated
into or onto the particle via one or more biotinylated components
of the particle, for example, biotinylated stabilizer. The antibody
can specifically bind to an antigen on the surface of an
endothelial cell.
[0017] The invention also provides methods for protecting cells
from oxidative damage, for example, oxidative damage caused by
exposure of the cell to a reactive oxidative species. In general,
the methods comprise contacting the cell with a particle comprising
a magnetic or magnetizable material and at least one antioxidant
enzyme, and generating a uniform magnetic field capable of
magnetizing the magnetic or magnetizable material proximal to the
cell for a period of time sufficient to permit the cell to
internalize the particle. The antioxidant enzyme can be catalase,
superoxide dismutase, or glutathione peroxidase. The particle can
further comprises an antibody that specifically binds to an antigen
on the surface of the cell. The methods can be carried out in vitro
or in vivo. The cell can be any cell, such as an epithelial cell or
an endothelial cell. Some preferred cells are vascular endothelium
cells.
BRIEF DESCRIPTION OF THE DRAWINGS
[0018] The patent or application file contains at least one drawing
executed in color. Copies of this patent or patent application
publication with color drawings will be provided by the Office upon
request and payment of the necessary fee.
[0019] FIG. 1A shows the relationship between the size of
nanoparticles (NP) and the concentration of stabilizer. FIG. 1B
shows the relationship between the yield of nanoparticles (NP) and
the concentration of stabilizer.
[0020] FIG. 2 shows the effect of taxol-loaded magnetic
nanoparticles on the proliferation of cultured rat aortic smooth
muscle cells as a function of the nanoparticle amount.
[0021] FIG. 3A shows transgene expression in cultured rat aortic
smooth muscle cells as a function of the poly-L-arginine
formulation amount and nanoparticle dose. FIG. 3B shows transgene
(Green Fluorescent Protein, GFP) expression in bovine aortic
endothelial cells as a function of the poly-L-arginine formulation
amount and nanoparticle dose. FIG. 3C shows transgene expression in
cultured endothelial cells as a function of magnetic exposure. FIG.
3D shows the kinetics of transgene expression in cultured
endothelial cells treated with poly-L-arginine modified
nanoparticles at a dose equivalent to 285.times.10.sup.6 viral
particles per well with or without a magnetic field.
[0022] FIG. 4 shows an exemplary magnetically assisted therapeutic
system according to an embodiment of the invention.
[0023] FIG. 5 shows a flowchart illustrating an exemplary method
for administering a therapeutic agent to an implanted device and
for retrieving magnetic carrier nanoparticles that do not localize
on the implanted device, according to an embodiment of the
invention.
[0024] FIG. 6 summarizes an exemplary embodiment of the
magnetically assisted therapeutic system, in which albumin modified
magnetic carrier nanoparticles with a red fluorescent label were
injected into a rat having an intravascularly implanted steel
stent. FIG. 6B summarizes results of the therapeutic agent
delivery, for sequestering in the implanted device.
[0025] FIG. 7 summarizes schematically the retrieval system shown
in FIG. 5 that is used to model the retrieval of magnetic carrier
nanoparticles or cells from the cardiovascular circulation
cycle.
[0026] FIG. 8 summarizes exponential depletion kinetics of carrier
nanoparticles under the influence of a magnetic field gradient.
[0027] FIG. 9 summarizes exponential depletion kinetics of carrier
cells under the influence of a magnetic field gradient.
[0028] FIG. 10 summarizes how different magnetic sequestering
configurations, for performing the exemplary method shown in FIG.
5, affect depletion kinetics.
[0029] FIGS. 11A and 11B summarize results of transmission electron
microscopy and magnetic moment versus magnetic field (magnetization
curve) for Albumin-stabilized superparamagnetic nanoparticles
(MNP).
[0030] FIG. 12A-12B summarize in vitro MNP cell loading studies
with respect to the kinetics of MNP uptake and viability of cells
loaded with MNP.
[0031] FIG. 13A shows reporter gene transfer mediated by
polyethylenimine-coated MNP combined with DNA encoding green
fluorescent protein (GFP) presented as GFP fluorescence at
.lamda.em/.lamda.ex of 485 nm/535 nm as a function of a
nanoparticle amount in A10 cells, wherein iron oxide-loaded
nanoparticles were prepared using 0 ml THF (large nanoparticles,
LNP), 3 ml THF (medium nanoparticles, MNP), or 4.5 ml THF (small
nanoparticles, SNP) in the organic phase, versus large
nanoparticles without iron oxide (LNP Non Mag, used herein as a
control). FIG. 13B shows the relative fluorescence measured at 485
nm/535 nm as a function of a nanoparticle amount in BAEC cells.
FIG. 13C shows internalization of fluorescent (far red) labeled
nanoparticles expressed as the relative fluorescence measured at
650 nm/670 nm as a function of a nanoparticle amount in A10 cells.
FIG. 13D shows the relative fluorescence measured at 650 nm/670 nm
as a function of a nanoparticle amount in BAEC. FIG. 13E shows cell
survival as a function of a nanoparticle amount in A10 cells. FIG.
13F shows cell survival as a function of a nanoparticle amount in
BAEC cells.
[0032] FIG. 14 shows suppression of eGFP expression in
lentivirus-transduced smooth muscle cells (A10) by siRNA delivered
with magnetic nanoparticles in the presence of a magnetic field
(500 Oe).
[0033] FIG. 15 shows the characterization of MNP and MNP-cell
loading. FIG. 15A shows magnetization curves of 304 (left sided Y
axis) and 316L (right sided Y axis) grade stainless steel stents.
The 304 stainless steel stent exhibits a near superparamagnetic
behavior showing slight hysteresis and a remnant magnetization on
the order of 7% of the saturation magnetization value. By
comparison, the 316L stent shows far less magnetic responsiveness.
FIG. 15B shows micrographs of BAEC's in culture (magnification of
.times.100) with bright field and red fluorescent images
qualitatively showing the relative amount of MNP internalized
within cells at different time points at the applied MNP dose of 9
.mu.g/well. Green fluorescent micrographs show cell viability as
assessed by Calcein Green staining.
[0034] FIG. 16 shows magnetic targeting of MNP-preloaded BAEC under
flow conditions in vitro and in vivo. FIG. 16A shows in vitro
capture kinetics of magnetically responsive BAEC onto a 304 grade
stainless steel stent in the presence of a uniform field of 1000
Gauss and a nonpulsatile flow with a rate of 30 ml/min. The initial
capture rate was estimated to be 1% of cells/min. The data were
obtained by measuring the fluorescence of internalized MNP. FIG.
16B and FIG. 16C show magnetically responsive BAEC captured in
vitro onto a 304 stainless steel stent as evidenced by the red
fluorescence of internalized MNP, or by Calcein Green staining of
live cells, respectively. FIG. 16D shows MNP loaded BAEC captured
in vivo onto a deployed 304 stainless steel stent in rat carotid
artery. BAEC preloaded with fluorescent MNP were transthoracically
injected into the left ventricular cavity. Animals were exposed to
a magnetic field of 1000 Gauss for 5 minutes including the period
of injection. The animals were sacrificed 5 minutes after delivery,
and the explanted stents were immediately examined by fluorescence
microscopy. FIG. 16E shows control rats subjected to an identical
procedure, where no magnetic field was employed. Micrographs (b-e)
were obtained at the magnification of .times.40. FIG. 16F shows in
vivo local magnetic cell delivery in a rat carotid stenting model
under stop-flow conditions. A catheter was introduced via the
external carotid into the common carotid artery and was positioned
distal to a deployed stent. The cell suspension was delivered into
isolated arterial segments for 15 sec. FIG. 16G shows in vivo cell
delivery under uninterrupted blood flow conditions. A catheter was
introduced via the external carotid into the common carotid and
advanced beyond the stent to the aortic arch. The cells were
injected at this site at the rate of 1 ml/min during one minute.
For both delivery protocols (f and g), in the magnetic group (Mag+)
the injection was carried out with animals placed in a magnetic
field of 1000 Gauss, and the field was maintained for a total of 5
minutes following delivery. In control rats (Mag- group) no
magnetic field was applied. In both settings BAEC were first
transduced in culture with luciferase adenovirus and then loaded
with MNP. The animals were imaged 48 hours post delivery by local
perivascular administration of luciferin admixed in a Pluronic gel.
The signal emitted from the stented arterial segment due to the
luciferase transgene expression was significantly higher in the
animals that received cells in the presence of a magnetic field
(Mag+ group).
[0035] FIG. 17 shows that a MRI imager can magnetize a 316L steel
stent for cell targeting. In the presence of a magnetic field
(Mag+), BAECs preloaded with red fluorescent polylactic acid (PLA)
MNP are shown to localize to the magnetized steel stent. Controls
(Mag-) did not show a significant localization to the stent.
[0036] FIG. 18 shows MNP physicochemical properties.
[0037] FIG. 19 shows MNPs loaded with SOD. FIG. 19A shows % SOD
activity retained relative to mass added. FIG. 19B shows % Mass of
SOD loaded relative to mass added. FIG. 19C shows the calculated
number of molecules per particle based on mass loading.
[0038] FIG. 20 shows catalase loading versus mass addition and
catalytic activity.
[0039] FIG. 20A shows catalase loading versus addition measured by
radiotracing of .sup.125I-catalase. FIG. 20B shows the activity of
loaded catalase as measured by degradation of H2O2 absorbance at
242 nm over time.
[0040] FIG. 21 shows the protection of catalase mass and activity
from proteolysis. FIG. 21A shows catalase mass added to MNP versus
mass protected from proteolysis from 0.2 wt % Pronase at 37.degree.
C. shaken for 1 hr. FIG. 21B shows (-.cndot.-) activity of catalase
loaded into MNP versus time versus time with exposure to 0.2 wt %
Pronase at 37.degree. C. and (-.smallcircle.-) activity of free
catalase versus time versus time with exposure to 0.2 wt % Pronase
at 37.degree. C.
[0041] FIG. 22 shows the stability of MNP in plasma at 37.degree.
C. over time. Release of catalase measured by radiotracing of
.sup.125I-catalase. MNP incubated with aqueous glucose solution
(5%) or plasma at 37.degree. C. over time. Release of catalase
determined by centrifuging free catalase from particles and
measuring activity in supernantant versus retained MNP on
microcentrifuge concentrator filter. (-.cndot.-) Released catalase
from MNPs diluted in glucose solution. (-.smallcircle.-) Released
catalase from MNPs diluted in whole heparinized mouse plasma.
[0042] FIG. 23 shows magnetic delivery of MNPs to cultured
endothelial cells. FIG. 23 A shows phase contrast micrograph of 10
min magnetic delivery of MNPs. FIG. 23B shows fluorescent
micrograph of 10 min magnetic delivery of MNP containing Dylight
488-labeled catalase. FIG. 23C shows 5 min MNP magnetic delivery.
FIGS. 23D & 23E show MNP delivery for 10 min without magnetic
field. FIG. 23F shows the control--without MNP.
[0043] FIGS. 24A and 24B show the protection of HUVECs from
oxidative stress through magnetic delivery of catalase loaded
MNPs.
[0044] FIG. 25 illustrates particle formation and synthesis.
[0045] FIG. 26 shows biotinylated MNP affinity.
[0046] FIG. 27 shows protection of HUVECs from oxidative stress
through magnetic delivery of catalase loaded MNPs and protection of
HUVECs from oxidative stress through antibody-targeted
delivery.
[0047] FIG. 28 shows biodistribution of Ab62-modified MNP vs.
control IgG-modified MNP after tail vein injection in mice. Tail
vein injected anti-PECAM labeled MNP specifically target the lung
endothelium.
DETAILED DESCRIPTION OF THE INVENTION
[0048] Various terms relating to the methods and other aspects of
the present invention are used throughout the specification and
claims. Such terms are to be given their ordinary meaning in the
art unless otherwise indicated. Other specifically defined terms
are to be construed in a manner consistent with the definition
provided herein.
[0049] As used in this specification and the appended claims, the
singular forms "a," "an," and "the" include plural referents unless
the content clearly dictates otherwise. Thus, for example,
reference to "a particle" includes a combination of two or more
particles, and the like.
[0050] The term "about" as used herein when referring to a
measurable value such as an amount, a temporal duration, and the
like, is meant to encompass variations of .+-.20% or .+-.10.degree.
A), more preferably .+-.5%, even more preferably .+-.1%, and still
more preferably .+-.0.1% from the specified value.
[0051] "Polynucleotide," also referred to as "nucleic acid" or
"nucleic acid molecule," refers to any polyribonucleotide or
polydeoxyribonucleotide, which may be unmodified RNA or DNA or
modified RNA or DNA. Polynucleotides include, without limitation
single- and double-stranded DNA, DNA that is a mixture of single-
and double-stranded regions, single- and double-stranded RNA, and
RNA that is mixture of single- and double-stranded regions, hybrid
molecules comprising DNA and RNA that may be single-stranded or,
more typically, double-stranded or a mixture of single- and
double-stranded regions. In addition, polynucleotide refers to
triple-stranded regions comprising RNA or DNA or both RNA and DNA.
The term polynucleotide also includes DNAs or RNAs containing one
or more modified bases and DNAs or RNAs with backbones modified for
stability or for other reasons. Modified bases include, for
example, tritylated bases and unusual bases such as inosine. A
variety of modifications can be made to DNA and RNA; thus,
polynucleotide embraces chemically, enzymatically or metabolically
modified forms of polynucleotides as typically found in nature, as
well as the chemical forms of DNA and RNA characteristic of viruses
and cells. Polynucleotide also embraces relatively short
polynucleotides, often referred to as oligonucleotides.
[0052] "Polypeptide" refers to any peptide or protein comprising
two or more amino acids joined to each other by peptide bonds or
modified peptide bonds, i.e., peptide isosteres. Polypeptide refers
to both short chains, commonly referred to as peptides,
oligopeptides or oligomers, and to longer chains, generally
referred to as proteins. Polypeptides may contain amino acids other
than the 20 gene-encoded amino acids. Polypeptides include amino
acid sequences modified either by natural processes, such as
post-translational processing, or by chemical modification
techniques which are well known in the art. Such modifications are
well described in basic texts and in more detailed monographs, as
well as in a voluminous research literature. Modifications can
occur anywhere in a polypeptide, including the peptide backbone,
the amino acid side-chains and the amino or carboxyl termini. It
will be appreciated that the same type of modification may be
present in the same or varying degrees at several sites in a given
polypeptide. Also, a given polypeptide may contain many types of
modifications.
[0053] Except when noted, "subject" or "patient" are used
interchangeably and refer to any animal, but preferably refer to
mammals such as humans and non-human primates, as well as
companion, farm, or experimental animals such as rabbits, dogs,
cats, rats, mice, horses, cows, pigs, and the like. Humans are most
preferred.
[0054] "Effective amount" or "therapeutically effective amount" are
used interchangeably herein, and refer to an amount of a
therapeutic agent, as described herein, effective to achieve a
particular biological result such as, but not limited to,
biological results disclosed, described, or exemplified herein, as
determined by any means suitable in the art.
[0055] "Pharmaceutically acceptable" refers to those properties
and/or substances which are acceptable to the patient from a
pharmacological/toxicological point of view and to the
manufacturing pharmaceutical chemist from a physical/chemical point
of view regarding composition, formulation, stability, patient
acceptance and bioavailability. "Pharmaceutically acceptable
carrier" refers to a medium that does not interfere with the
effectiveness of the biological activity of the therapeutic
agent(s) and is not toxic to the host to which it is
administered.
[0056] It has been discovered in accordance with the present
invention that therapeutic agents can be targeted to specific
locations in the body through use of uniform magnetic fields to
induce magnetization of magnetizable objects and to generate a
magnetic field gradient. It has further been discovered that
magnetic targeting can be utilized for any type of therapeutic
agent, including pharmaceutical or chemical compounds,
biomolecules, and cells. Accordingly, the invention features
systems and methods for magnetically targeting therapeutic agents
to one or more desired locations in the body.
[0057] In one aspect, the systems comprise therapeutic agents
provided as part of a therapeutic formulation. The therapeutic
formulation can comprise an effective amount of a therapeutic agent
and a particle, which particle can comprise a magnetic or
magnetizable material. Preferably, the particle is a nanoparticle.
The associated particle and therapeutic agent are synonymously
referred to herein as a therapeutic particle. Magnetic
nanoparticles include particles that are permanently magnetic and
those that are magnetizable upon exposure to an external magnetic
field, but lose their magnetization when the field is removed.
Materials that are magnetic or magnetizable upon exposure to a
magnetic field that lose their magnetic properties when the field
is removed are referred to herein as superparamagnetic material.
Superparamagnetic particles are preferred to prevent irreversible
aggregation of the particles. Examples of suitable
superparamagnetic materials include, but are not limited to, iron,
mixed iron oxide (magnetite), or gamma ferric oxide (maghemite) as
well as substituted magnetites that include additional elements
such as zinc. Preferably, the superparamagnetic material is in the
form of one or more nanocrystals, for example, single-domain
crystalline systems with at least one dimension .ltoreq.100 nm. A
nanocrystal is any nanomaterial with at least one dimension
.ltoreq.100 nm and that is singlecrystalline or monocrystalline,
formed of a single crustal-unit, and so all elements have identical
crystallographic orientation of c- and a-axes and overgrow as one
unit. Any particle that exhibits regions of cyrstalinity can be
termed nanoparticle or nanocluster based on dimensions.
[0058] Ferromagnetic crystals can be comprised of magnetized
domains the size of a micron. Superparamagnetism can occur when the
size of the crystals is smaller than the ferromagnetic domain
(.about.30 nm). Superparamagnetic properties can depend on
temperature. Temperature can, under some conditions, destabilize
the magnetism. Without intending to be limited to any particular
theory or mechanism of action, it is believed that thermal energy
may prevent the alignment of the magnetic moments present in
superparamagnetic materials. After the removal of an applied
magnetic field, the magnetic moments of superparamagnetic materials
still exist, but are in rapid motion, causing a randomly oriented
or disordered magnetic moment and, thus, no net magnetic field. At
the temperatures of biological systems and in the applied magnetic
fields of MR imagers, superparamagnetic materials are less magnetic
than their ferromagnetic counterparts. For example, it has been
noted that magnetism of small superparamagnetic iron oxides
decreases at elevated temperatures. (Berkowitz et al. (1968) J.
Appl. Phys. 39:1261).
[0059] The superparamagnetic nanocrystals can range in size from
about 1 nm to about 20 nm, depending on, among other things, the
preparation method and medium composition. Preferably, the
nanocrystals are smaller than 10-20 nm to ensure superparamagnetic
properties of the material. More preferably, the nanocrystals are
from about 5 nm to about 20 nm.
[0060] In some aspects, the particle is a composite nanocrystal.
The composite nanocrystal can comprise more than one individual
magnetic or magnetizable nanocrystals and one or more
water-insoluble biocompatible materials to hold the crystals
together. The biocompatible materials can be a polymer, which can
be biodegradable or non-biodegradable. Non-limiting examples of
such polymers include poly(urethane), poly(ester), poly(lactic
acid), poly(glycolic acid), poly(lactide-co-glycolide),
poly(.epsilon.-caprolactone), poly(ethyleneimine), poly(styrene),
poly(amide), rubber, silicone rubber, poly(acrylonitrile),
poly(acrylate), poly(methacrylate), poly(.alpha.-hydroxy acid),
poly(dioxanone), poly(orthoester), poly(ether-ester),
poly(lactone), poly(alkylcyanoacrylate), poly(anhydride),
poly(ethylenevinyl acetate), poly(hydroxybutyrate),
poly(tetrafluoroethylene), poly(ethylene terephthalate,
polyoxyethylene, polyoxyethlyene-polyoxypropylene block copolymers,
mixtures thereof and copolymers of corresponding monomers.
[0061] Polymeric nanoparticles with incorporated superparamagnetic
nanocrystals can be prepared according to any means suitable in the
art. For example, the nanoparticles can be prepared by dispersing
the superparamagnetic nanocrystals in an organic solvent, in which
the polymer and/or the therapeutic agent is dissolved, emulsifying
the organic phase in water in the presence of a suitable
stabilizer, and finally eliminating the solvent to obtain
solidified nanoparticles. Conditions of nanoparticle preparation
should not be damaging for the therapeutic agent to be attached.
The temperature for nanoparticle preparation preferably ranges from
about 25.degree. C. to about 37.degree. C., although higher or
lower temperatures can be used. Non-limiting examples of ways to
prepare superparamagnetic nanoparticles for biological applications
are described in U.S. Pat. Nos. 7,175,912 and 7,175,909, and U.S.
Publication No. 20050271745. Magnetic nanoparticles, information
for the development of magnetic nanoparticles, and reagents for the
preparation of magnetic nanoparticles (MNP) are commercially
available.
[0062] The particles can be composed of the salts/complexes of
anionic lipids, for example, fatty acids or lipid phosphates with
polyvalent biocompatible cations. The particles can be formed under
mild conditions through combination of the respective aqueous
solutions in the presence of colloid stabilizers, thus avoiding use
of organic solvents and without need for external mechanical energy
input.
[0063] In some preferred aspects, the particles are bioresorbable
nanoparticles, including those prepared without the use of high
energy dispersion or organic solvents. Bioresorbable nanoparticles
can be comprised of at least one anionic lipid salt, at least one
therapeutic agents, and at least one magnetic or magnetizable
material.
[0064] To prepare bioresorbable nanoparticles, a first aqueous
solution is provided. The first aqueous solution comprises i) a
water soluble salt of a mono-carboxylic fatty acid, or salt
thereof, or a lipid phosphate/phosphonate, ii) a stabilizer, and
iii) a therapeutic agent. Exemplary soluble salts include, but are
not limited to, the lithium, sodium, ammonium, and potassium salts.
An aqueous solution of the fatty acid salt can be prepared, for
example, by adding the fatty acid and base, such as sodium
hydroxide, to water and dissolving the fatty acid.
[0065] Fatty acids that can be used include straight and branched
chain, saturated and unsaturated mono-carboxylic fatty acids having
eight or more carbon atoms, particularly eight to thirty carbon
atoms. Typical mono-carboxylic fatty acids include caprylic acid
(octanoic acid), 2-ethyl octanoic acid, capric acid (decanoic
acid), 2-ethyl-decanoic acid, 11-undecenoic acid, undecanoic acid,
2-ethyl-dodecanoic acid, cis-5-dodecenoic acid, lauroleic acid
(cis-9-dodecanoic acid), traumatic acid (2-dodecenoic acid), lauric
acid (dodecanoic acid), brassylic acid (tridecanoic acid),
2-ethyl-tetradecanoic acid, myristoleic acid (cis-9-tetradecanoic
acid), tsuzuic acid (cis-4-tetradecenoic acid), myristic acid
(tetradecanoic acid), pentadecanoic acid, 2-ethyl-hexadecanoic
acid, palmitoleic acid (cis-9-hexadecanoic acid), palmitic acid
(hexadecanoic acid), heptadecanoic acid, margaric acid
(heptadecanoic acid), petroselic acid (cis-6-octadecenoic acid),
2-ethyl-octadecanoic acid, oleic acid (cis-9-octadecenoic acid),
elaidic (trans-9-octadecenoic acid), asclepinic acid
(cis-11-octadecenoic acid), vaccenic acid (trans-11-octadecenoic
acid), taxoleic acid (cis, cis-5,9-octadecadienoic), linoleic acid
(cis, cis-9,12-octadecadienoic acid), linolenic acid (cis, cis,
cis-9,12,15-octadecatrienoic acid), stearic acid (octadecanoic
acid), tuberculostearic acid (10-methyl octadecanoic acid),
nonadecanoic acid, 2-ethyl-eicosanoic acid, arachidonic acid
(5,8,11,14-eicosatetraenoic acid), cis-8,11,14-eicosatrienoic acid,
gadoleic acid (cis-9-eicosenoic acid), gondoic acid
(cis-11-eicosenoic acid), arachidic acid (eicosanoic acid),
2-ocyldodecanoic acid, erucic acid (cis-13-docosenoic acid),
behenic acid (docosanoic acid), tricosanoic acid, selacholeic acid
(cis-15-tetracosanoic acid), lignoceric acid (tetracosanoic acid),
ximenic acid (cis-17-hexacosenoic acid), and hexacosanoic acid. A
particularly preferred fatty acid is oleic acid. Salts of the fatty
acids, including for example, alkaline metal and alkaline earth
metal salts, and ammonium salts, can also be used.
[0066] As an alternative to fatty acids, lipid phosphates, such as
the water soluble mono-phosphate salts of alcohols having eight or
more carbon atoms, more preferably eight to thirty carbon atoms,
can also be used. Such phosphates include .alpha.-tocopherol
phosphate disodium salt, oleyl phosphate disodium salt, and the
disodium salts of the phosphate esters of straight and branched
chain, saturated and unsaturated mono-alcohols having eight or more
carbon atoms, such as the disodium salts of the phosphate esters of
n-decanol, n-dodecanol, n-tetradecanol, n-hexadecanol, and
n-octadecanol.
[0067] Hydroxy acids such as 11-hydroxy-undecanoic acid, ricinoleic
acid (12-hydroxy-cis-9-octadecenoic acid), lesquerolic acid
(14-hydroxy-cis-11-eicosenoic acid: 20:1-OH), densipolic acid
(12-hydroxy-cis, cis-9,15-octadecadienoic acid) auricolic acid
(14-hydroxy-cis, cis-11,17-eicosadienoic acid),
9,10-dihydroxyoctadecanoic acid, 9,14-dihydroxyoctadecanoic acid,
and phellonic acid (22-hydroxydocosanoic acid) and salts thereof
can also be used.
[0068] Lipid phosphates, such as the water soluble mono-phosphate
salts of alcohols having eight or more carbon atoms, more
preferably eight to thirty carbon atoms, can also be used. Such
phosphates include .alpha.-tocopherol phosphate disodium salt,
oleyl phosphate disodium salt, and the disodium salts of the
phosphate esters of straight and branched chain, saturated and
unsaturated mono-alcohols having eight or more carbon atoms, such
as the disodium salts of the phosphate esters of n-decanol,
n-dodecanol, n-tetradecanol, n-hexadecanol, and n-octadecanol.
[0069] A colloidal stabilizer, or mixture of colloid stabilizers,
can be added to the aqueous solution of the fatty acid salt or to
the aqueous solution containing the polycation. Colloidal
stabilizers are materials believed to be adsorbed onto the
nanoparticles, thereby providing charge or steric protection of the
particles from aggregation. Suitable stabilizers include secondary
colloids, such as gelatin, agar-agar, starch, cellulose derivatives
such as carboxymethyl cellulose and hydroxypropyl cellulose, and
proteins, such as albumin. Non-ionic surfactants, such as
polyethylene oxide, ethylene oxide/propylene oxide block
co-polymers, for example, PLURONIC.RTM. surfactants, and
ethoxylated fatty acid esters of esters of sorbitol, such as
polyoxyethylene (20) sorbitan monolautate (TWEEN.RTM. 20),
polyoxyethylene (20) sorbitan monopalmitate (TWEEN.RTM. 40),
polyoxyethylene (20) sorbitan monosterate (TWEEN.RTM. 60),
polyoxyethylene (20) sorbitan monooleate (TWEEN.RTM. 80), or
polyoxyethylene (20) sorbitan trioleate (TWEEN.RTM. 85) can also be
used. A preferred stabilizer is albumin. PLURONIC is a registered
trademark of BASF Corporation and TWEEN is a registered trademark
of Croda International PLC.
[0070] A second aqueous solution comprising a water-soluble salt of
a polyvalent biocompatible metal or organic cation can be added to
the first aqueous solution. A cation is biocompatible if it is
non-toxic to the recipient in the quantities used, and also
presents no significant deleterious or untoward effects on the
recipient's body. Useful biocompatible polyvalent cations include,
without limitation, Al.sup.+3, Ca.sup.+2, Mg.sup.+2, Zn.sup.+2,
Ba.sup.+2, Sr.sup.+2, Fe.sup.+2, and Cu.sup.+2, polyarginine,
protamine. Preferred biocompatible polyvalent cations include
Ca.sup.+2 and ZN.sup.+2.
[0071] The size of the bioresorbable particles can be readily
controlled and adapted for specific applications by adjusting the
amount of the stabilizer, lipid salt, and polyvalent biocompatible
cation. Although the particles are generally lipophilic, showing
high affinity for hydrophobic therapeutic agents, ionic
water-soluble therapeutic agents can also be encapsulated as their
water-insoluble salts/complexes in the process of particle
formation. The nature and amount of the lipid salt and polyvalent
biocompatible cation can be varied in order to adjust the relative
lipophilicity of the resulting particles.
[0072] A cationic peptide, cationic protein, or a mixture of
cationic peptides and/or cationic proteins can also be co-added to
the second aqueous solution containing a metal polycation.
Preferred cationic peptides contain at least about 50%, preferably
at least about 70%, and more preferably at least about 85% of basic
amino acid residues, such as arginine, lysine, and guanidine, and
contain more then five amino acid residues, preferably about 10 to
about 1000 residues. More preferred cationic peptides include
arginine-rich polypeptides, such as poly-L-arginine. More preferred
peptides are arginine-rich proteins, such as protamine.
Guanidinium-rich proteins can also be used. Synthetic organic
polycations (polypeptide-like substances), such as
polyethyleneimine, can also be used.
[0073] Bioresorbable nanoparticles can be rendered magnetic through
inclusion of magnetically responsive nanocrystals in their
structure, for example, by combining a fine suspension of such
crystals (a ferrofluid) with the anionic lipid solution prior to
the particle formation. Ferrofluids are composed of nanosacle
ferromagnetic particles suspended in a carrier fluid, such as
water. Preparation of such nanoparticles is a two-step process
consisting of 1) making the fine suspension of magnetic
nanocrystals (ferrofluid) in the presence of an anionic lipid, and
2) forming nanoparticles by controlled precipitation of the anionic
lipid with a polyvalent cation in the presence of a stabilizer and
a therapeutic agent. In one aspect, the magnetic nanoparticles are
prepared by controlled aggregation of an oleate-stabilized
ferrofluid with Ca.sup.+2.
[0074] To prepare a ferrofluid, an aqueous solution containing a
water soluble ferric (Fe.sup.+3) salt, such as ferric chloride
hexahydrate, and a water soluble ferrous salt (Fe.sup.+2), such as
ferrous chloride tetrahydrate, is precipitated with base, such as
an aqueous sodium hydroxide solution to form a magnetite
precipitate containing magnetic nanocrystals. A water soluble salt
of a fatty acid, such as an aqueous solution of sodium oleate, is
added, and the magnetic nanocrystals resuspended by heating, for
example, in an inert atmosphere, such as under argon. A stabilizer
such as albumin can be added, along with the therapeutic agent,
either to the first aqueous solution, which comprises the magnetic
nanocrystals, stabilizer, water soluble salt of a mono-carboxylic
fatty acid, and therapeutic agent, or to the second aqueous
solution, which comprises the polyvalent biocompatible cation. The
second solution is then added to form the magnetic
nanoparticles.
[0075] In some aspects, the therapeutic agent can be attached or
tethered to the surface of a pre-formed nanoparticle. The
attachment can be according to any means suitable for the
therapeutic application to which the agent will be used, or
according to the chemical properties of the agent or the
nanoparticle. For example, attachment can be by adsorption,
electrostatic interactions, charge complexation, or covalent
binding, including the use of biomolecule tethers. Non-limiting
examples of procedures for associating therapeutic agents with
nanoparticles are described in U.S. Pat. Nos. 7,081,489, 6,048,515,
6,576,221, and 6,767,635. The attachment can be by way of a linking
molecule. Some non-limiting examples of linking molecule pairs
include avidin or streptavidin and biotin, thiol and Succinimidyl
3-(2-pyridyldithio)-propionate (SPDP) or Succinimidyl
4-[N-maleimidomethyl]cyclohexane-1-carboxylate (SMCC), or suitable
variants or isoforms thereof, and folate and the folate
receptor
[0076] The magnetic nanoparticles associated with the therapeutic
agent can range in size from about 50 to about 500 nm. The size can
vary according to any appropriate variable. Preferably, the
nanoparticles range in size from about 50 nm to about 200 nm, and
more preferably from about 100 nm to about 200 nm.
[0077] The particle can be derivatized, and the surface of the
particle can be modified to facilitate derivatization. For example,
the particles can be coated with a thiol-reactive and
photoactivatable polymer. Irradiation can facilitate the covalent
binding of the polymer to the surface, and its thiol-reactive
groups can subsequently be used to attach agents providing stealth
properties in the blood circulation and/or specific binding to a
target tissue. Photochemical activation of surfaces for attaching
biomaterial is described in US Publ. No. 20060147413.
[0078] Extended circulation time of particles associated with a
therapeutic agent can be achieved by preventing opsonization and
clearance by the subject's immune system by coating the particle
with a biocompatible hydrophilic polymer such as polyethyleneglycol
or dextran, or by coating the particle with albumin to inhibit the
binding of opsonins to the particle surface.
[0079] Preparation of Modified Particles can Proceed According to
any Means Suitable in the art. For example, a magnetically
responsive agent, iron oxide, can be produced. Fine dispersion of
iron oxide in a suitable organic solvent is typically obtained as
follows: an aqueous solution containing ferric and ferrous
chlorides is mixed with an aqueous solution of sodium hydroxide.
The precipitate is coated with oleic acid by short incubation at
90.degree. C. in ethanol. The precipitate is washed once with
ethanol to remove free acid and dispersed in chloroform.
[0080] The resulting organic dispersion of iron oxide in chloroform
is used to dissolve a biodegradable polymer, polylactic acid (PLA)
or its polyethyleneglycol conjugate (PLA-PEG), thus forming an
organic phase. The organic phase is emulsified in an aqueous
albumin solution (1%) by sonication on an ice bath followed by
evaporation of the organic solvent. The particles are separated
from the unbound albumin by repeated magnetic
sedimentation/resuspension cycles.
[0081] In an alternative aspect, a post-formation surface
modification can be used. For example, particles can be formed
using a photoreactive polymer (e.g., PBPC/PBMC,
polyallylamine-benzophenone-pyridyldithio/maleimido-carboxylate
polymer) as a stabilizer in the aqueous phase. Subsequent brief
ultraviolet irradiation achieves covalent binding of the polymer to
the magnetic nanoparticle. The resulting particles are reacted in
suspension with a thiolated polyethyleneglycol, which allows better
control over the particle size and the extent of surface
modification.
[0082] Therapeutic agents include any molecules that can be
associated with a particle and used in the systems and methods of
the present invention. Agents can be purified molecules,
substantially purified molecules, molecules that are one or more
components of a mixture of compounds, or a mixture of a compound
with any other material. Agents can be organic or inorganic
chemicals, radioisotopes, pharmaceutical compounds, pharmaceutical
salts, pro-drugs, or biomolecules, and all fragments, analogs,
homologs, conjugates, and derivatives thereof. Biomolecules
include, without limitation, proteins, polypeptides, nucleic acids,
lipids, polysaccharides, monosaccharides, and all fragments,
analogs, homologs, conjugates, and derivatives thereof. Agents can
also be an isolated product of unknown structure, a mixture of
several known products, or an undefined composition comprising one
or more compounds. Examples of undefined compositions include cell
and tissue extracts, growth medium in which prokaryotic,
eukaryotic, and archaebacterial cells have been cultured,
fermentation broths, protein expression libraries, and the like.
Agents can also be one or more cells, including eukaryotic or
prokaryotic cells, or can be one or more viruses. Therapeutic
agents can be provided in or otherwise associated with a carrier
such as a pharmaceutically acceptable carrier.
[0083] Therapeutic agent also includes viral vector systems, which
are used in gene therapy. A number of viral vector systems under
development, such as adenovirus, adeno-associated virus, retrovirus
and Herpes simplex virus. One of the most successful ways of
introducing the gene of interest into the appropriate cell line
uses recombinant adenovirus. Adenoviruses are non-enveloped
particles having a diameter of about 70 nm, and contain a linear
double stranded DNA of approximately 36,000 base pairs. They are
easily prepared with high titers and can infect a wide range of
cells, including non-dividing cells. Recombinant adenovirus can
also be used in vaccination by expressing a gene product that
triggers an immune response.
[0084] Adeno-associated viruses have a particle diameter of 20 nm.
Retroviruses are spherical, enveloped particles having a particle
diameter of between about 80 nm to about 100 nm in diameter.
Retroviruses have been widely used as vectors for DNA delivery.
Herpes simplex viruses have a particle diameter of about 100 nm,
and contain enveloped, double-stranded DNA virus of approximately
150,000 base pairs. These viruses have a large loading capacity for
foreign genes and are able to infect a wide range of cells. In
addition, the virus genome remains episomal after infection, thus
eliminating the possibility of opportunistic malignant insertional
mutagenesis of the host genome. Herpes viruses have been exploited
for specific gene transfer trials into the central nervous
system.
[0085] Multiple agents can be included in a particle. Those of
skill in the art can determine the particular combination of
agents, based, for example, on the condition being treated, or on
the needs of the particular subject. For example, additional agents
that modulate the activity of a primary agent, reduce pain, support
growth of therapeutic cells, are antithrombogenic, anti-apoptotic,
anti-inflammatory, immunosuppressants, or antioxidants, or other
agents ordinarily used in the art to treat the disease of interest
can be used.
[0086] The therapeutic agents can also be formulated in sustained
release vehicles or depot preparations. For example, the agents can
be formulated with suitable polymeric or hydrophobic materials (for
example, as an emulsion in an acceptable oil) or ion exchange
resins, or as sparingly soluble derivatives, for example, as a
sparingly soluble salt. Liposomes and emulsions are well-known
examples suitable for use as carriers for hydrophobic drugs.
[0087] In some preferred aspects, the therapeutic agents are
enzymes. For example, antioxidant enzymes can be used. Antioxidant
enzymes include, without limitation, catalase, superoxide
dismutase, and glutathione peroxidase. Other examples of proteins
include antibodies. Any antibody suitable for the purpose to which
the particle is being used can be included. The antibodies can be
the therapeutic agent, or can be used to help guide the particle to
targeted tissue.
[0088] In some preferred aspects, the therapeutic agents are
regulatory nucleic acids. For example, regulatory nucleic acids can
be used to facilitate post-transcriptional gene silencing (RNA
silencing). RNA silencing involves the processing of
double-stranded RNA (dsRNA) into small 21-28 nucleotide fragments
by an RNase H-based enzyme. The cleavage products are siRNA (small
interfering RNA) or miRNA (micro-RNA), which regulate gene
expression in a sequence-specific manner. Regulatory nucleic acids
can be part of a plasmid or other suitable vector, for example,
administered as DNA that is transcribed and processed to regulatory
RNA.
[0089] siRNAs may thus comprise RNA molecules having a
double-stranded region approximately 19 nucleotides in length with
1-2 nucleotide 3' overhangs on each strand, resulting in a total
length of between approximately 21 and 23 nucleotides. As used
herein, siRNAs also include various RNA structures that may be
processed in vivo to generate such molecules. Such structures
include RNA strands containing two complementary elements that
hybridize to one another to form a stem, a loop, and optionally an
overhang, preferably a 3' overhang. Preferably, the stem is
approximately 19 by long, the loop is about 1-20, more preferably
about 4-10, and most preferably about 6-8 nt long and/or the
overhang is about 1-20, and more preferably about 2-15 nt long. In
certain embodiments of the invention the stem is minimally 19
nucleotides in length and may be up to approximately 29 nucleotides
in length. Loops of 4 nucleotides or greater are less likely
subject to steric constraints than are shorter loops and therefore
may be preferred. The overhang may include a 5' phosphate and a 3'
hydroxyl. The overhang may, but need not comprise a plurality of U
residues, e.g., between 1 and 5 U residues.
[0090] miRNAs are typically between approximately 20 and 26
nucleotides in length, e.g., 22 nt in length. It is believed that
they are derived from larger precursors known as small temporal
RNAs (stRNAs) or mRNA precursors, which are typically approximately
70 nt long with an approximately 4-15 nt loop.
[0091] Viral vectors or DNA vectors encoding short hairpin RNA
(shRNA) which are processed in the cell cytoplasm to short
interfering RNA (siRNA) can also be used. A plasmid containing a
DNA sequence encoding for a particular desired siRNA sequence can
be delivered to a target cell, and subsequently internalized, for
example, by virally-mediated infection. Once in the cell, the DNA
sequence is continuously transcribed into RNA molecules that loop
back on themselves and form hairpin structures through
intramolecular base pairing. These hairpin structures, once
processed by the cell, are equivalent to transfected siRNA
molecules and are used by the cell to mediate RNAi of the desired
protein. The use of shRNA has an advantage over siRNA as the former
can lead to stable, long-term inhibition of protein expression. In
cases where longer periods of protein inhibition are necessary,
shRNA as the therapeutic agent is preferable.
[0092] In some preferred aspects, the therapeutic agent is one or
more cells. For example, the cell can be a stem cell such as a
postpartum derived cell or bone marrow derived cell or can be a
progenitor cell, Blood Outgrowth Endothelial Cell (BOED), adult and
cord blood stem cells (CBSC), Induced Pluripotent Stem Cells, e.g.,
skin cells that are programmed to transform into pluripotent stem
cells with further potential to differentiate them into cell with
at least one endothelial phenotype. In some exemplary aspects, the
cell is a vascular cell such as a vascular endothelial cell.
Endothelial cells can be autologous, heterologous, or derived from
either blood, bone marrow, or tissue biopsy. Tissue biopsied
endothelial cells can be derived from arteries, veins, adipose
tissue, or any other tissue with the potential to contain
endothelial cells or their progenitors.
[0093] In some aspects, the systems comprise an implantable device.
Any implantable device known or used in the art can be utilized in
the inventive systems. Non-limiting examples of suitable
implantable device include stents, heart valves, wire sutures,
temporary joint replacements and urinary dilators, orthopedic
implants such as joint prostheses, screws, staples, nails, nuts,
bolts, plates, rods, pins, wires, inserters, osteoports, halo
systems and other orthopedic devices used for stabilization or
fixation of spinal and long bone fractures or disarticulations.
Other devices include non-orthopedic devices, temporary placements
and permanent implants, such as traceostomy devices, drainage
ducts, jejunostomy and gastrostomy tubes, intraurethral and other
genitourinary implants, stylets, dilators, vascular clips and
filters, pacemakers, wire guides and access ports of subcutaneously
implanted vascular catheters, electronic chips,
transmitting/receiving micro-electronic implants, implantable drug
delivery micro-devices, implantable biosensors, implantable
micro-video devices, and implantable microbattery devices. A highly
preferred implantable device is a stent. The stent can be a
drug-eluting stent.
[0094] Preferably, the implantable device comprises a magnetic or
magnetizable material. More preferably, such magnetic or
magnetizable materials are biocompatible. The device can be
modified to be biocompatible. For example, surface modifications of
metal supports to improve biocompatibility are described in US
Publ. No. 2003/0044408.
[0095] Stainless steel, for example, Grade 304 Stainless Steel is
one preferred non-limiting example of a material that can be used
in the implantable device. Other examples includes the 200-series
austenitic chromium-nickel-manganese alloys and 300-series
austenitic chromium-nickel alloys.
[0096] The device can be implanted anywhere in the body of the
subject. In some preferred aspects, the device is implanted in the
vascular system of the subject, for example, in a blood vessel such
as a vein, artery, or capillary. Where stents are used, the stents
can be implanted in any duct such as a hepatic duct, bile duct,
parts of the digestive system such as the esophagus, stomach,
intestines, or colon, parts of the respiratory system such as the
trachea or bronchi, or parts of the excretory system such as the
ureter, urethra, or renal excretory duct. Other implants include
ocular implants and radioactive seeds.
[0097] In some aspects, the systems can comprise a retrieval
system. In general, the retrieval system can be used to capture and
contain therapeutic particles that do not reach the target site, or
to capture and contain particles after the therapeutic agent has
been delivered to the target site, synonymously referred to herein
as spent particles. Unused or spent particles may enter or remain
in the blood of the subject, and may produce untoward effects in
the subject. To minimize risks to the subject, it is preferable to
remove such unused and/or spent particles. The retrieval system
preferably captures and contains most, and more preferably
substantially all unused and/or spent particles such that the body
or particular fluid, organ, appendage, and the like within the body
is substantially free of spent or unused particles.
[0098] In some preferred aspects, the retrieval system comprises a
magnetic or magnetizable material. The material can be provided in
any form suitable in the art. For example, the material can be a
rod, plate, bead, tube, wire, panel, filter, screen, mesh, and the
like. The particular form (geometry) is not critical, and can vary
according to any number of variables.
[0099] The retrieval system is preferably biocompatible. Suitable
materials that can be used to comprise the retrieval system
include, but are not limited to stainless steel such as 316L
stainless steel. 400-series stainless steel, including 430-grade
can also be used in some instances, such as those for short term
use where potential long-term corrosive properties of retrieval
system materials is not of concern.
[0100] Preferably, the retrieval system is configured such that it
is capable of being reversibly connected to the subject. The
retrieval system can be reversibly connected to a subject at any
location on the body suitable according to the therapeutic use to
which the overall system is being used. For example, the retrieval
system can be reversibly connected to the body surface, or to a
particular interior organ, bone, or system. Preferably, the
retrieval system is reversibly connected to at least one blood
vessel, and more preferably to the lumen of the blood vessel to
allow blood to directly flow into the retrieval system. The
circulatory system is a high-flow, well-accessed system, and is
thus highly preferred for connection to a retrieval system.
[0101] In some aspects, the retrieval system is indirectly
connected to the subject. For example, a biological fluid of the
subject can be removed and contacted with the retrieval system.
Biological fluids can include, but are not limited to blood,
cerebrospinal fluid, ascites fluid, bile, amniotic fluid, milk,
saliva, gingival crevicular fluid, urine, mucosal fluid, renal
fluid, and the like. After the particles are sequestered from the
biological fluid, the biological fluid can be returned to the
subject. Blood is a particularly preferred biological fluid. Thus,
for example, the subject's blood may be removed from the body,
contacted with the retrieval system, and returned to the body by
transfusion. The blood can be separated into its components or can
remain as whole blood.
[0102] Particles directed to the retrieval system can be disposed
of according to any means suitable in the art. After the particles
are directed to the retrieval system, the retrieval system can be
removed from the subject.
[0103] The particles comprising at least one therapeutic agent and
at least one magnetic or magnetizable material are targeted to one
or more desired locations in the body, for example, to one or more
implanted devices in the body, through a magnetic field. Thus, the
inventive systems can comprise a magnetic field generator. The
magnetic field generator can include an external magnet, including
a magnetic resonance imaging device. In some aspects, the magnetic
field generator is configured to generate at least one directable
magnetic field gradient. The magnetic field gradient can direct the
particle to the implantable device. The magnetic field gradient can
direct particles not delivered to the device to the retrieval
system, or can direct spent particles, that is, particles that have
successfully delivered and are depleted of the therapeutic agent to
the retrieval system. A single magnetic field gradient can be used
to direct the particles to the implantable device, and then
reconfigured to direct extant unused or spent particles to the
retrieval system. Alternatively, multiple gradients can be produced
and used, with at least one gradient directing particles to the
implanted device, and at least one additional gradient directing
particles to the retrieval system. The gradient can be generated
proximal to the implanted device, and can be generated proximal to
the retrieval system.
[0104] Referring to FIGS. 4 and 5, an exemplary magnetically
assisted therapeutic system 100 is illustrated. The therapeutic
system 100 comprises a device 104 that has been implanted in a
mammalian subject (not shown), a magnetic field generator 106,
configured to generate a magnetic field gradient external to the
subject that is directed proximally to the implanted device 104,
and a therapeutic particle 102 that has been administered to the
subject. Device 104 can be a vascular device that has been
implanted in the vascular system of the mammalian subject.
[0105] Also featured in accordance with the present invention are
methods for magnetically targeting a therapeutic particle to one or
more desired locations in or on a subject. In some preferred
aspects, the methods are applicable to magnetically target a
therapeutic particle to a device implanted in a subject.
[0106] The methods can comprise administering to a subject having
an implanted device comprising at least one biocompatible magnetic
or magnetizable material a therapeutic particle comprising at least
one therapeutic agent and at least one magnetic or magnetizable
material, generating a magnetic field gradient proximal to the
implanted device, wherein the gradient targets the particle to the
implantable device, and removing particles not delivered to the
implantable device, or removing spent particles.
[0107] The therapeutic agent can be any molecule as described or
exemplified herein, including without limitation, a pharmaceutical,
biomolecule, or cell. The implanted device can be any device used,
known, or otherwise suitable in the art such as those described or
exemplified herein.
[0108] In some preferred aspects, the methods are applicable to
magnetically target a therapeutic particle to a particular cell or
tissue. These methods can be carried out in vitro, and preferably
can be carried out in vivo. Thus, for example, therapeutic
particles can be magnetically targeted to a particular location in
the body of a subject. The location need not have an implanted
device. A magnetic field can be used to guide the particle to the
desired location, and can be used to facilitate internalization of
the therapeutic particle by particular cells at the desired
location.
[0109] In some detailed aspects, these methods can be used to
protect cells from oxidative damage. Thus, for example, methods for
protecting a cell from oxidative damage comprise contacting the
cell with a particle comprising a magnetic or magnetizable material
and at least one antioxidant enzyme, and generating a uniform
magnetic field capable of magnetizing the magnetic or magnetizable
material proximal to the cell for a period of time sufficient to
permit the cell to internalize the particle. The cell can be in
vitro or in vivo. The cell can be an endothelial cell, for example,
a vascular endothelium cell. The antioxidant enzyme can be
catalase, superoxide dismutase, or glutathione peroxidase. The
particle can further comprise an antibody that specifically binds
to an antigen on the surface of the cell. Thus, the antibody can be
used to facilitate targeting to the proper target cell.
[0110] Administration of the therapeutic particles to a subject can
be by infusion or injection (intravenously, intramuscularly,
intracutaneously, subcutaneously, intrathecal, intraduodenally,
intraperitoneally, and the like). The particles can also be
administered intranasally, vaginally, rectally, buccally, orally,
or transdermally. Preferably, the compositions are administered
intravenously. Administration can be at the direction of a
physician. The particles can be administered proximally or distally
to the implanted device.
[0111] For buccal administration, the compositions may take the
form of tablets, troche or lozenge formulated in conventional
manner. Compositions for oral or buccal administration, may be
formulated to give controlled release of the particles. Such
formulations may include one or more sustained-release agents known
in the art, such as glyceryl mono-stearate, glyceryl distearate and
wax.
[0112] Particles may be applied topically. Such administrations
include applying the particles externally to the epidermis, the
mouth cavity, eye, ear and nose. Particles for use in topical
administration include, e.g., liquid or gel preparations suitable
for penetration through the skin such as creams, liniments,
lotions, ointments or pastes, and drops suitable for delivery to
the eye, ear or nose.
[0113] Various alternative pharmaceutical delivery systems may be
employed. Non-limiting examples of such systems include liposomes
and emulsions. Certain organic solvents such as dimethylsulfoxide
also may be employed. Additionally, the particles may be delivered
using a sustained-release system, such as semipermeable matrices of
solid polymers containing the therapeutic agent. The various
sustained-release materials available are well known by those
skilled in the art. Sustained-release capsules may, depending on
their chemical nature, release the particles over a range of
several days to several weeks to several months.
[0114] The particles may also be co-administered with other well
known therapeutic agents that are selected for their particular
usefulness against the condition that is being treated. For
example, such therapeutic agents can be pain relievers, blood
thinners/anticoagulants, clot busters, stomach antacids, or
compounds which lessen untoward effects of the particles.
[0115] The administration of these additional compounds may be
simultaneous with the administration of the particles, or may be
administered in tandem, either before or after the administration
of the particles, as necessary. Any suitable protocol may be
devised whereby the various compounds to be included in the
combination treatment are administered within minutes, hours, days,
or weeks of each other. Repeated administration in a cyclic
protocol is also contemplated to be within the scope of the present
invention.
[0116] Following administration of the particles, capture of the
therapeutic particles by the implanted device is effectuated for a
period of time. The duration of the magnetic particle delivery may
be dependent on any number of variables, including without
limitation, the species, breed, size, height, weight, age, overall
health of the subject, the type of therapeutic agent, the
composition of the particle, the mode or manner or administration,
or the type or severity of the condition being treated. The
appropriate effective amount of particles to use can be routinely
determined by those of skill in the art using routine optimization
techniques and the skilled and informed judgment of the
practitioner and other factors evident to those skilled in the art.
Preferably, a therapeutically effective dose of the particles
described herein will provide therapeutic benefit without causing
substantial toxicity to the subject.
[0117] The particle therapeutic regimen can be initiated with
smaller dosages of particles, followed by an increase in dosage
over the course of the treatment until the optimum effect under the
circumstances is reached. If needed, the total daily dosage may be
divided and administered in portions throughout the day.
[0118] For effective treatment of a particular condition, one
skilled in the art may recommend a dosage schedule and dosage
amount adequate for the subject being treated. It may be preferred
that dosing occur one to four or more times daily for as long as
needed. The dosage schedule may also vary depending on the active
agent concentration, which may depend on the needs of the
subject.
[0119] The inventive methods can be used to treat any condition
that is amenable to targeting therapeutics. The methods are
particularly well suited to treat vascular conditions, including
follow up care for a metallic stent angioplasty.
[0120] The following examples are provided to describe the
invention in greater detail. They are intended to illustrate, not
to limit, the invention.
Example 1
Preparation of Non-Magnetic and Magnetic, Stabilized Nanoparticles
Comprised of Anionic Lipid Salt
[0121] To prepare non-magnetic calcium oleate-based nanoparticles,
sodium oleate was formed by dissolving oleic acid (100 mg) in 5 ml
aqueous solution containing 14.8 mg sodium hydroxide with gentle
heating to 40.degree. C. Albumin solution (10%, 0.4 ml) was added
to the aqueous sodium oleate. Calcium chloride aqueous solution
(111 mg in 5 ml) was added dropwise resulting in formation of
nanoparticles exhibiting a characteristic bluish opalescence due to
the Tyndall effect. The nanoparticle size was 230.+-.20 nm as
determined by photon correlation spectroscopy.
[0122] Magnetic calcium oleate-based nanoparticles were prepared by
a two-step procedure as follows. To prepare a stable aqueous
suspension of mixed iron oxide (magnetite), ferric chloride
hexahydrate and ferrous chloride tetrahydrate (100 mg and 50 mg,
respectively) are dissolved in 4 ml deionized water and
precipitated by 1.6 ml of aqueous sodium hydroxide (1 M). Sodium
oleate (150 mg in 5 ml deionized water) is then added to the
resulting precipitate. The magnetite precipitate is resuspended in
the form of nanocrystals by heating under argon to 90.degree. C.
and ultrasonication (5 min each step) repeated twice to form a
ferrofluid. Bovine serum albumin (200 .mu.l, 10% w/v) is added as a
stabilizer to 1 ml of the obtained sodium oleate solution
containing oleate-stabilized colloidal magnetite, and nanoparticles
are formed by dropwise adding calcium chloride (33.3 mM, 1.5 ml)
upon gentle stirring. The particles are washed by sedimentation on
a magnet and subsequently resuspended in water. The particles can
also be stored lyophilized after freeze drying in 10% w/v trehalose
solution as a cryoprotectant.
[0123] FIG. 1A shows that the size of the resultant nanoparticles
can be adjusted by varying the concentration of the stabilizer.
FIG. 1B shows that the yield of the resultant nanoparticles can be
adjusted by varying the concentration of the stabilizer.
Example 2
Incorporation of a Neutral Lipophilic Agent into Magnetic
Nanoparticles
[0124] This example shows the incorporation of a neutral lipophilic
agent, such as taxol, into magnetic nanoparticles, by adding its
concentrated solution in a small volume of a biocompatible
water-miscible solvent, to the ferrofluid containing the anionic
lipid and the stabilizer.
[0125] Taxol-loaded nanoparticles were prepared as in Example 1.
Taxol, 1.0 mg in 10 .mu.l dimethylformamide, was added to the
ferrofluid containing the anionic lipid and the stabilizer and the
nanoparticles isolated as in Example 1.
[0126] The effect of taxol-loaded magnetic nanoparticles in
comparison to an equivalent dose of nanoparticles containing no
drug on proliferation of cultured rat aortic smooth muscle cells
following 15 min incubation under magnetic field (500 G) was
determined using Alamar Blue assay (.lamda..sub.excitation=540 nm,
.lamda..sub.emission=575 nm). The cells were seeded on a 96-well
plate at 10% confluency, and the cell proliferation was measured
after three days as a function of the drug formulation amount.
[0127] FIG. 2 shows the effect of taxol-loaded magnetic
nanoparticles on the proliferation of cultured rat aortic smooth
muscle cells as a function of the nanoparticle amount. As can be
seen from this Figure, although the control nanoparticles have a
weak stimulatory effect on the growth of smooth muscle cells, the
proliferation of cells treated with taxol nanoparticles was
inhibited in a dose dependent manner and decreased by .about.30% at
the highest dose applied compared to untreated cells.
Example 3
Preparation of all-Trans Retinoic Acid-Loaded Magnetic
Nanoparticles
[0128] The formulation method described above is suitable for
preparing nanoparticles with ionic compounds through their
inclusion as their water-insoluble complexes. All-trans retinoic
acid (atRA) sodium salt, an anticancer agent, is an anionic lipid
that readily complexes with calcium, and provides an example of an
ionic substance that can be incorporated into nanoparticles.
[0129] A formulation containing atRA was prepared as described in
Example 2 with the following modifications. Magnetite aqueous
dispersion was prepared in 4 ml water containing 100 mg sodium
oleate. All-trans retinoic acid (50 mg) was dissolved in 1 ml
aqueous of sodium hydroxide (6.7 mg) and added to the magnetite
dispersion prior to the dropwise addition of calcium chloride in
the presence of albumin.
Example 4
Preparation of Adenovirus Containing Magnetic Nanoparticles
[0130] Magnetic nanoparticles encapsulating adenovirus can be
produced by adding adenovirus prior to the nanoparticle formation
step either in the sodium oleate solution containing ferrofluid, or
in the Ca.sup.2+ or Zn.sup.2+ solution. In the following examples
50 .mu.l of adenovirus (5.times.10.sup.12 particles per ml)
encoding for green fluorescent protein (GFP) were added to the
ferrofluid to accomplish adenovirus entrapment in the
particles.
[0131] Adenovirus-impregnated nanoparticles were applied to
confluent smooth muscle cells seeded on 96-well plates at doses
equivalent to 60-285 million viral particles per well for 30 min
with or without a magnetic field. The gene expression was assayed
by measuring GFP fluorescence (.lamda..sub.excitation=485 nm,
.lamda..sub.emission=535 nm) in cells 3 days post treatment.
Example 5
Formation of Magnetic Nanoparticles in the Presence of a Cationic
Peptide
[0132] A further improvement in the transduction efficiency can be
achieved by co-addition of one or more cationic peptides or
proteins, in particular arginine-rich polypeptides and proteins,
such as poly-L-arginine or protamine, to the calcium chloride or
zinc chloride solution. Nanoparticle modification with these
peptides and proteins facilitates the cellular uptake and therefore
results in a more efficient internalization of the encapsulated
adenovirus with a resultant increase in transgene expression.
Incorporating poly-L-arginine hydrochloride (molecular weight
.about.70,000 Da) in the nanoparticles results in a dose dependent
increase in adenoviral gene transfer both in cultured rat aortic
smooth muscle cells and bovine aortic endothelial cells.
[0133] The cells were seeded at confluence on 96-well plates and
treated for 15 min in the presence of a magnetic field with
increasing doses of adenovirus-impregnated nanoparticles (290.+-.20
nm) prepared with addition of 0-2.25 mg poly-L-arginine
hydrochloride. The expression of GFP was measured fluorimetrically
on day three.
[0134] FIG. 3 shows transgene expression in cultured rat aortic
smooth muscle cells and bovine aortic endothelial cells (FIG. 3A
and FIG. 3B, respectively) as a function of the poly-L-arginine
formulation amount and nanoparticle dose. Transgene expression in
cultured endothelial cells with and without magnetic exposure is
shown in FIG. 3C. The kinetics of transgene expression in cultured
endothelial cells treated with poly-L-arginine modified
nanoparticles at a dose equivalent to 285.times.10.sup.6 viral
particles per well with or without a magnetic field is shown in
FIG. 3D. In the absence of a magnetic field substantially lower
gene transfer rates were observed as shown here for cultured
endothelial cells (FIG. 3C).
Example 6
Magnetic Gradient Targeting of Nanoparticles
[0135] Albumin modified magnetic nanoparticles with a red
fluorescent label were injected into the tail vein of a rat with an
already deployed 6 mm-long Grade 304 Stainless Steel stent (FIG.
6A). Grade 304 Stainless Steel ("304 steel") has a history of use
in implantable devices. Although there are no commercially
available stents made out of 304 steel, a stent design was created
and contracted to a medical device company to fabricate a set of
these stents for use in the experiments. Thus, all of the studies
reported here did not use any of the currently commercially used
stents.
[0136] The 304 stent in these rat studies was investigated both
with and without a magnetic field across the stent. In addition,
magnetic nanoparticles without a stent were also injected into
animals, with investigations to see if there was any localization
that took place without stent deployment.
[0137] Methods: Paclitaxel was dispersed within the polylactic acid
(PLA) matrix of magnetite-loaded nanoparticles (MNP).
Adenovirus-tethered MNP were prepared using photochemical surface
activation with the subsequent attachment of a recombinant
adenovirus binding protein, D1, followed by formation of
nanoparticle-adenovirus complexes. Plasmid vectors were
charge-associated with PEI-functionalized MNP. Magnetic trapping of
MNP on the steel meshes and stents under different field strength
and flow conditions was studied in a closed circuit flow system.
Transfection/transduction using gene vectors associated with
magnetic nanoparticles was studied in smooth muscle (SMC) and
endothelial cells. Magnetic force-driven localization of reporter
gene-associated MNP and MNP-loaded cells on pre-deployed stents and
resulting transgene expression were studied a rat carotid stent
model.
[0138] Protocol (FIG. 6A): Four hundred .mu.l of magnetically
responsive fluorescent labeled, polylactic acid based
magnetite-loaded nanoparticles were intravenously-injected (through
the tail vein) upon induction of anesthesia in 480-510 g rats
(Sprague-Dawley rats (n=6)). The magnetite-loaded nanoparticles
were 350 nm, consisting of 7.2 mg per injection. This injection was
carried out to saturate the reticulo-endothelial system of the
animal to prevent excessive capturing of the second main dose of
nanoparticles in liver and spleen.
[0139] Within 30 minutes of the first injection, a 304 steel stent
was deployed in the left common carotid artery. Immediately after
that, another 400 .mu.l dose of the nanoparticles was injected
intravenously, either with or without 300 G magnetic field created
by 2 electromagnets placed adjacent to the neck of the animal. The
field was maintained for 5 min after injection, after which the
arteries were harvested. The stents were removed and nanoparticles
deposition on stents and luminal aspects of arteries was examined
by fluorescence microscopy. After acquisition of respective images
BODIPY-labeled (red fluorescent) PLA was extracted in acetonitrile
and its concentration was determined fluorimetrically against a
calibration curve. For fluorescence control/background purposes in
one additional rat no nanoparticles were injected and the stented
arteries were removed and similarly processed to obtain background
fluorescence values.
[0140] Results: In a closed circuit flow system MNP and cells
loaded with MNP were trapped on magnetic meshes with exponential
kinetics. Rat aortic SMC (A10) cultured on 316L stainless steel
grids showed 100-fold increased gene transduction when exposed to
the MNP-Ad.sub.GFP compared to controls. Paclitaxel MNP
demonstrated inhibition of A10 cells growth in culture. Systemic
intravenous injection in rats of MNP resulted in 7-fold higher
localization of MNP on intra-arterial stents compared to controls
when carried out in the presence of external magnetic field
(300-G).
[0141] The results of these studies are shown in FIG. 6B
(fluorimetry, 540/575 nm), as well as with fluorescent microscopy
(not shown), demonstrating intense localization of magnetic
nanoparticles to the deployed 304 stent, and also localization of
magnetic nanoparticles to the arterial wall directly proximal to
the stent. In addition, using a specific fluorescent assay, the
significant localization of magnetic nanoparticles following
intravenous injection using this methodology was quantified.
[0142] Conclusion: Magnetically targeted drug/gene delivery using
high field gradients to stented arteries offers great promise
because of the potential for not only initial dosing, but repeated
administration utilizing magnetic field-mediated localization of
vectors to the stented arterial wall. These results clearly
demonstrate a significantly higher nanoparticles deposition on
stents and adjacent arterial tissue in the group where systemic
intravenous delivery was carried out in conjunction with an
electromagnetic field compared to "no field" controls. Non-stented
arteries demonstrated no nanoparticle localization with or without
a magnetic field.
Example 7
Magnetic Trapping and Removal of Residual Nanoparticles and
Cells
[0143] This Example illustrates removal of residual nanoparticles
and cells with an external magnetically responsive steel filter
("magnetic trap"). FIG. 7 illustrates a flow system 400 that
schematically summarizes the retrieval system 108 (FIG. 4) that is
used to model the retrieval of magnetic nanoparticles or cells from
the circulation. As shown in FIG. 7, flow system 400 includes a
magnetic trap 402 (an Eppendorf with 430 stainless steel mesh for
capturing of the residual nanoparticles), electromagnets 404 for
generating a magnetic field, a peristaltic pump 406, a stirrer 408,
and faucets 410 for directing flow to cycle A or cycle B. A
suitable peristaltic pump 406, stirrer 408, and faucets 410, as
commonly for an apheresis apparatus, will be understood by the
skilled person from the description herein.
[0144] The following experimental protocol was used to determine
the kinetics of magnetic nanoparticles and cell capture,
respectively, using the "Magnetic Trap" apparatus.
[0145] PLA-PEG based magnetic nanoparticles were diluted in 50 ml
of 5% glucose solution and filtered (5 .mu.m cut-off) to ensure
uniform particle size. Alternatively, bovine aortic endothelial
cells (BAEC) were grown to confluence and incubated with
fluorescently labeled magnetic nanoparticles on a cell culture
magnet (Dexter Magnet Technologies, Elk Grove Village, Ill.)
producing a strong magnetic field (500 Gauss) for 24 hours,
followed by cell washing and resuspension in fresh cell culture
medium. Untreated cells were used as a control.
[0146] The flow system 400 was purged with 5% glucose or cell
culture medium, respectively, (washing step) followed by one cycle
of nanoparticle/cell suspension in the loop A to equilibrate the
system (priming step). Next, nanoparticle/cell suspension was
redirected to the loop B including the trapping device 402 equipped
with one or three 430 stainless steel mesh pieces (total weight of
0.30.+-.0.01 and 0.83.+-.0.05 g, respectively) and an external
magnetic field of 800 Gauss generated by two solenoid
electromagnets 404. A t.sub.0 sample was withdrawn and further used
as a reference (100% of NP/cells). Additional samples were
collected at predetermined time points during 2.5 hours and 35 min
in the nanoparticles and cell retrieval experiments, respectively.
The effect of the magnetic field exposure was investigated in
comparison to "no field" conditions employed during the first 25
and at 3 minutes into the experiment for the nanoparticles and
cells, respectively, after which the field was applied. A NP/cell
fraction remaining in the circulation at a given time point was
determined fluorimetrically (.lamda..sub.ex=540 nm,
.lamda..sub.em=575 nm) in relation to the reference sample. The
mesh samples were visualized under the fluorescent microscope using
red fluorescence filter set (540/575 nm) immediately and 24 hours
after completing the experiment. Collected cells were incubated
overnight at 37.degree. C. and their morphology was examined
microscopically.
[0147] FIG. 8 and FIG. 9 depict exponential depletion kinetics of
nanoparticles and BAEC cells, respectively, over time under the
influence of a magnetic field. A significantly less pronounced
decrease in both nanoparticles and BAEC cells is also observed in
"no field" conditions. Under the magnetic field exposure, the
depletion kinetics of both nanoparticles and cells was very fast
with t.sub.90% (i.e., time required to eliminate 90% of the
circulating nanoparticles or cells) equaling 75 min and 16 min for
nanoparticles and cells, respectively. The five-fold lower
t.sub.90% for cell capture is apparently due to their higher
magnetic responsiveness due to the cells containing a large number
of nanoparticles/cell compared to that of the smaller sized NP.
[0148] Referring to FIG. 10, different magnetic trap configurations
and corresponding depletion kinetics are shown. Increasing the
amount and surface area of the 430 stainless steel in the "Magnetic
Trap" from 0.3 to 0.83 g, caused a significant decrease in the
circulation t.sub.1/2 of the nanoparticles (27 vs. 50 min). Thus,
optimization of the "Magnetic Trap" design could potentially allow
for nanoparticles and cell retrieval kinetics sufficiently fast for
its clinical use. Spreading of cells was also demonstrated where
the cells were removed from the circulation for measurement of cell
depletion. Cells were grown overnight on the cell culture plate at
the 37.degree. C. and in the atmosphere of 5% of CO.sub.2.
Micrographs of the mesh taken post experiment demonstrated
nanoparticles deposited on the "Magnetic Trap."
[0149] Magnetically responsive cells captured at the end of the
experiment and spreading of the cells 24 hours later were also
demonstrated. Cells sampled from the circulation during the cell
capture experiment demonstrate normal morphology characteristic of
BAEC. The growth conditions are 10% FBS supplemented DMEM at
37.degree. C. and 5% CO.sub.2. The meshes used in the magnetic trap
in this experiment were visualized under the fluorescent microscope
immediately and 24 hours post experiment in order to evaluate the
morphology of the captured cells. A high number of cells are shown
to be initially captured by the edges of the mesh, of which those
located most adjacent to the mesh surface form a layer of uniformly
spread cells after 24 hours over the expanse of the entire surface
of the mesh framework thus showing the viability of the
magnetically targeted cells. Capture of magnetic carrier
nanoparticles at the end of experiment was demonstrated on the
surface of the 430 stainless steel mesh under the field of 800
Gauss ("The Magnetic Trap"), as compared with a control mesh at the
beginning of the experiment before application of magnetic
field.
Example 8
TEM and Magnetization Curve of Albumin-Stabilized Magnetic
Nanoparticles
[0150] Referring now to FIGS. 11A and 11B, results from
transmission electron microscopy and a magnetization curve
(magnetic moment versus magnetic field) are shown, respectively for
Albumin-stabilized magnetic nanoparticles (MNP), described above
with respect to Example 6. Note the small size and the large number
of individual oleic acid coated magnetite grains distributed in the
MNP polymeric matrix (FIG. 11A). MNP exhibits a superparamagnetic
behavior, showing no significant hysteresis, and a remnant
magnetization on the order of 0.5% of the respective saturation
magnetization value (FIG. 11B).
Example 9
MNP Cell Loading
[0151] Referring now to FIGS. 12A-12B, in vitro MNP cell loading
studies are illustrated. In particular, FIG. 12A illustrates
kinetics of the MNP uptake by bovine aortic endothelial cells
(BAEC) as a function of MNP dose and incubation time; FIG. 12B
illustrates cell viability as a function of MNP dose and incubation
time; and FIG. 12C illustrates a magnetization curve of cells
loaded with MNP demonstrating superparamagnetic behavior as was
observed with MNPs per se. The nanoparticles uptake was determined
by fluorescence of internalized MNPs. Cell survival was determined
by Alamar Blue assay.
[0152] BAEC (bovine aortic endothelial cells) were incubated with
various doses of MNP on a magnet. As shown in FIG. 12A, the MNP
uptake was determined at different time points by fluorescence of
internalized nanoparticles. The amount of internalized MNP was near
linearly dependent on the nanoparticle dose. Approximately 30% of
internalization was observed after 8 hours and the uptake was
practically complete after 24 hours, whereas no significant uptake
was achieved in the absence of a magnetic field at 24 hr. As shown
in FIG. 12B, cell viability at different experimental conditions
(incubation time and MNP dose) was not adversely affected by MNP
loading. Greater than 85% of cell survival was observed at all
studied MNP doses and incubation times relatively to untreated
cells. As shown in FIG. 12C, the magnetization curve of cells
loaded with MNPs demonstrating super-paramagnetic behavior showing
no significant hysteresis and a remnant magnetization on the order
of 0.5% of the respective saturation magnetization value.
Example 10
Gene Transfer Efficiency and Cell Toxicity
[0153] Particles were studied for transfection of cells in culture.
Three kinds of magnetically responsive particles were prepared and
complexed with DNA at different PEI:DNA ratios. In all experiments,
nanoparticles were complexed with 0.25 .mu.g GFP-encoding DNA
plasmid per well in 5% glucose for 30 min, then mixed 1:4 with cell
culture medium supplemented with 10% fetal bovine serum (FBS) and
applied to cells for 10 min with magnetic field. Their transfection
efficiency, as well as nanoparticles uptake and toxicity, was
studied in cultured rat aortic smooth muscle and bovine aortic
endothelial cells (A10 and BAEC, respectively) using non-magnetic
particles as a control. Gene expression, NP uptake and cell
survival were determined by measuring fluorescence at 485/535 nm,
620/670 nm and with the Alamar Blue assay (540/575 nm),
respectively, at 2 day time point. The results are presented in
FIG. 13A-F. Magnetically responsive formulations resulted in high
levels of gene product as opposed to non-magnetic nanoparticles
(FIGS. 13A-F) in correlation with their cellular uptake (FIGS. 13C
and D). All formulations exhibited low toxicity in cell culture in
the examined amount range (FIGS. 13 E and F).
[0154] In another experiment, bovine aortic endothelial cells
(BAEC) were seeded on day -1 (2.times.10.sup.4/well, on four
24-well plate). The cells were washed 2 times (2.times.1 hr) with
the 10% FBS-supplemented Dulbecco's Modified Eagle's Medium (DMEM)
on day 0 prior to transfection. Plasmid DNA was incubated for 30
minutes with magnetic nanoparticles (the complexants) at various
ratios in 5% w/v glucose solution, serially diluted 1.25-fold with
FBS-containing DMEM to provide a final serum concentration of 10%
or 80% and applied to cells at 0.25 .mu.g DNA/well. The cells were
incubated at 37.degree. C., while one plate was placed at a time on
the magnet (15 min), and another kept at a distance from it. The
medium was then replaced with fresh pre-warmed DMEM supplemented
with 10% FBS. The cells were observed for transfection after 24
hr.
[0155] The nanoparticles and PEI showed comparable transfection of
BAEC cells in culture with DNA encoding for green fluorescent
protein when applied without use of external magnetic field,
whereas the transfection efficacy of the magnetic nanoparticles
applied in the presence of a permanent magnet was substantially
increased as compared to both control formulations and the magnetic
nanoparticles applied in the absence of the magnet.
[0156] Similar effect of the magnetic field on the transfection
efficacy was also observed in A10 cells in culture.
[0157] Notably, the magnetic NP were able to effectively transfect
cells in presence of 10% and 80% serum apparently due to their
protective effect against DNA enzymatic degradation, whereas
practically no transfection was found when DNA:PEI complex was
added to the cells in the presence of serum for the same time
period.
Example 11
Magnetic Targeting of siRNA-Containing Nanoparticles
[0158] Magnetic nanoparticles were formulated using following
protocol: 5.5 ml of an aqueous solution containing 300 mg
FeCl.sub.3 hexahydrate and 150 mg FeCl.sub.2 tetrahydrate was
rapidly mixed with 4.75 ml aqueous solution of NaOH (1.0 M). The
obtained precipitate was separated on a magnet. Oleic acid (150 mg)
was added dropwise, the precipitate was suspended in 2 ml ethanol,
and the mixture was degassed in argon. The contents were heated to
90.degree. C. in a water bath for 5 min with several stirrings. 4
ml water was added dropwise upon gentle stirring, the oleic
acid-coated iron oxide was precipitated on a magnet, and the liquid
phase was carefully aspirated. The precipitate was washed with 4 ml
ethanol to remove excess oleic acid; ethanol was aspirated
following sedimentation on a magnet. The precipitate was
resuspended in 5 ml chloroform.
[0159] An organic phase consisting of 200 mg polylactic acid (PLA)
(D,L-PLA 70-120 K Sigma), 100 mg polyethyleneimine (PEI) (branched
PEI, Aldrich 25 K) or 200 mg of linear PEI 200K (pH 7) and 100 mg
oleic acid dissolved in the chloroformic suspension of magnetite
was added to 15 ml deionized water pre-cooled in an ice bath, and
the mixture was emulsified by sonication. The organic solvent was
removed by rotavaporation at 25.degree. C. The particles were
filtered through 1.0 .mu.m glass fiber filter and dialyzed against
deionized water at 4.degree. C. for 24 hr with several water
replacements using 300,000 Da cut-off dialysis membrane. Trehalose
(10% w/v) was added to the obtained nanoparticle suspension, and
nanoparticles were lyophilized and stored at -20.degree. C.
[0160] The NP formulation (FIG. 14) used in the present example,
diameter 360 nm, exhibited superparamagnetic behavior showing no
significant hysteresis, and a remnant magnetization in the order of
0.5% of the respective saturation magnetization values. The
magnetic moment depended near-linearly on magnetic field up to 1000
Oe reaching 66-68% of the saturation value, while a comparatively
low increment in magnetization was observed upon further increasing
the field to 5000 Oe (FIG. 14). The specific magnetic
susceptibility of the NP was found to be about 5.03+0.04
emu/cm.sup.3.times.kOe.
[0161] The linear PEI was prepared as described in: Thomas, M et
al. (2005). Proc. Natl. Acad. Sci. USA 102:5679-84. In brief, fully
deacylated linear PEI 200K was prepared by the acid-catalyzed
hydrolysis of the commercially available 200K PEOZ
poly(2-ethyl-2-oxazoline) (Sigma-Aldrich). Typically, 3.0 g of the
PEOZ was added to 120 ml of 24% (w/v) HCl, followed by refluxing
for 96 h, the first reaction mixture contained a white precipitate
throughout the reaction. The PEOZ crystals dissolved completely in
.about.2 hr, washed once with 2-propanol. The powder was
redispersed in 2-propanol for 2 hours, isolated by filtration and
dried under reduced pressure. The resultant white powder was
confirmed by 1H-NMR to be pure PEI hydrochloride. The fully
deacylated PEI 200 exhibited a singlet at 3.57 ppm by NMR
corresponding to --CH.sub.2--CH.sub.2--NH.sub.2.sup.+ but no signal
corresponding to the N-propionyl moieties, confirming their complex
removal.
[0162] Suppression of eGFP expression in lentivirus transduced
smooth muscle cells by siRNA using magnetic NP was achieved in the
following experiment: Rat aortic smooth muscle cells (A10) were
cultivated for several passages after their transduction with GFP
encoding lentivirus. Cells were grown in DMEM medium supplemented
with 10.sup.5 fetal bovine serum (FBS). Lyophilized NP were
resuspended in 100 .mu.l of deionized water and diluted serially in
triplicates to achieve following NP amount range: 0-14 .mu.g and
2.2 .mu.g for branched and linear PEI-NP per well (96-well plate
format) respectively. siRNA was incubated for 30 min with NP at
various ratios in 5% w/v glucose solution and added to cells after
5-fold dilution with serum supplemented DMEM at 0.15, 0.25, and
0.35 .mu.g RNA/well followed by 20 min exposure to magnetic field
(500 Gauss produced by a cell culture magnet, Dexter Magnet
Technologies, Elk Grove Village, Ill.). Fluorimetric measurements
of GFP expression (.lamda.em .lamda.ex=485 nm/535 nm) and cell
viability (AlamarBlue assay [Biosource, Camarillo, Calif. USA],
(.lamda.em .lamda.ex=540 nm/575 nm) were performed in live cells 5
days post treatment.
[0163] Efficient eGFP suppression was achieved using magnetic NP
formulated with either branched or linear PEI (FIG. 14). For both
formulation types the eGFP suppression depended directly on the NP
dose, reaching maximum of 20-40% (FIG. 14). However, the eGFP
suppression achieved using linear PEI formulation exhibited
saturation with increasing NP dose, while for branched PEI-NP
formulation the eGFP suppression exhibited near-linear dose
dependence in the entire studied NP range. The suppression of eGFP
was directly siRNA dose dependent in the case of the linear PEI
formulation and inversely dependent for branched PEI-NP formulation
resulting in a maximal suppression of 38 and 40% for linear and
branched PEI formulations at a dose of 0.35 and 0.15 .mu.g of
siRNA, respectively (FIGS. 14A and C). The NP/siRNA formulations
did not significantly compromise cell survival showing more than
90% of viable cells 5 days post treatment at maximal NP dosages
(FIGS. 14 B and D).
Example 12
High Field Gradient Targeting of Magnetic Nanoparticle-Loaded
Endothelial Cells to the Surface of Steel Stents
[0164] Nanoparticle Formulation and Characterization. Magnetite
prepared from ferric and ferrous chloride (300 mg and 150 mg,
respectively) by alkaline precipitation with aqueous sodium
hydroxide was magnetically separated, resuspended in 2 ml of
ethanol and coated with oleic acid (200 mg) with heating under
argon to 90.degree. C. in a water bath for 5 min. Excess oleic acid
was phase-separated by dropwise addition of 4 ml of water and the
lipid-coated magnetite was washed twice with ethanol. Lipophilic
magnetite was dispersed in 6 ml chloroform, forming a stable
ferrofluid. The resulting organic dispersion of iron oxide was used
to dissolve PLA, thus forming an organic phase. The organic phase
was emulsified in an aqueous albumin solution (1%) by sonication in
an ice bath followed by organic solvent evaporation. The particles
were separated from the unbound albumin by repeated magnetic
sedimentation/resuspension cycles, and lyophilized with 10% (w/v)
glucose as a cryoprotectant. Lyophilized MNP were kept at
-20.degree. C. and resuspended in deionized water before use.
[0165] Particle size measurements were performed using the 90 Plus
Particle Size Analyzer (Brookhaven Instruments, Holtville, N.Y.
USA). The magnetic properties of MNP and cells loaded with MNP were
estimated from the hysteresis curves of either MNP or MNP-loaded
cells 5 .mu.l samples air-dried on a 4.times.4 mm.sup.2 cover-glass
slide using an alternating gradient magnetometer (Princeton
Instruments Corporation, Princeton, N.J., USA).
[0166] Cell Preparation. Bovine aortic endothelial cells (BAEC)
were seeded on clear-bottom 96-well plates at a density of
1.5.times.10.sup.4 cells/well using DMEM supplemented with 10%
fetal bovine serum (FBS) for the cell loading and cell viability
experiments. To synchronize cell cultures with respect to MNP
uptake, the cells were incubated at 4.degree. C. for 30 min. Then
MNP were added to cells at different doses and cell cultures were
incubated on a magnetic separator adapted for cell culture plates
using a magnetic field source of 500 Gauss (LifeSep.TM. 96F, Dexter
Magnetic Technologies, Fremont, Calif., USA). Further, at
predetermined time points cells were washed with phosphate buffered
saline and the amount of internalized MNP was measured
fluorimetrically (.lamda.em/.lamda.ex=540/575 nm). Cell viability
was determined at all time points using Calcein Green staining and
the AlamarBlue assay as described by the manufacturer (Biosource,
Camarillo, Calif. USA).
[0167] For the studies of in vitro cell capture on stents, BAEC
were seeded on clear-bottom 12-well plates. On the next day 72
.mu.g of MNP were added to each well of cells
(4.5.+-.1.0).times.10.sup.4. Cells and MNP were incubated on a
magnetic source (Life Sep.TM. 96F) for 24 h to allow nearly
complete (.about.95%) internalization of MNP. Then cells were
trypsinized and resuspended in a cell culture medium for further
capturing experiments. Cells used for in vivo delivery experiments
were first transduced with replication defective type 5 (E1, E3
deleted) adenoviruses expressing luciferase (Ad luc) under the
control of the human cytomegalovirus promoter (Gene Vector Core,
University of Pennsylvania, Philadelphia, Pa.) for 10 hours
(MOI=500) and then loaded with MNP for 24 hours.
[0168] In Vitro and In Vivo Short-Term Cell-Capture Experiments. In
an in vitro cell capture experiment, MNP-loaded BAEC (ca.
2.5.times.10.sup.6) circulated in a closed-loop system at a flow
rate of 30 ml/min (0.015 m/s fluid velocity across the stent
surface) while a homogeneous magnetic field of 1000 Gauss was
applied. A homogeneous magnetic field was produced by passing an
electrical current through serially connected solenoid coils with
iron cores (40 mm in diameter) placed at both sides of either a
stent positioned in a flow chamber of a model loop-circulatory
system or a stented animal within a distance of 40 mm between the
electromagnets' cores. An electrical current of 9.4 A was generated
by a HP 6034A (Hewlett Packard, Palo Alto, Calif.) power supply by
applying a voltage of 28V. The magnetic field strength was measured
by a Hall Probe purchased from Lake Shore Cryotronics (Westerville,
Ohio). Cell depletion was monitored by measuring MNP fluorescence
and the results presented as a percent of captured cells.
[0169] In in vivo cell capture experiments 304 grade stainless
steel stents were deployed in rat carotid arteries. For acute
studies, BAEC cells preloaded with fluorescent MNP were
transthoracically injected into the left ventricular cavity.
Animals were exposed to a magnetic field of 1000 Gauss for 5
minutes, using the system described above, including the period of
injection. Control rats underwent an identical procedure, where no
magnetic field was employed. The animals were sacrificed 5 min
after delivery, and the explanted stents were examined by
fluorescence microscopy.
[0170] Angioplasty and In Vivo Delivery Procedure: 48-Hour Studies.
The left common carotids of 450-500 g Sprague-Dawley male rats were
injured by 4 passages of a Fogarty catheter prior to deployment (16
atm) of multilink stents made of 304 grade stainless steel (Circle
Medical Devices, Los Gatos, Calif.). In the model studies of cell
delivery under stop-flow conditions, a 23 G tubing was introduced
via the external carotid into the common carotid artery and was
positioned distal to the deployed stent. Thus, for these studies
with temporary interruption of carotid blood flow, a 15 mm segment
of common carotid artery encompassing the stented site was isolated
by ligatures. The cell suspension (50 .mu.l) was delivered into the
isolated arterial segment for 15 sec, after which the excess cells
that were not retained in the artery were evacuated by syringe
retrieval. In the model studies of cell delivery under
uninterrupted flow a 26 G tubing was introduced via the external
carotid into the common carotid and advanced beyond the stent to
the aortic arch (total 3.5 cm proximal from carotid bifurcation).
The cells were injected at the rate 1 ml/min for one minute. For
both delivery protocols, in the Mag+ group the injection was
carried out with animals placed in a magnetic field of 1000 Gauss,
as described above, and the field was maintained for a total of 5
minutes following delivery. In control rats (Mag- group) no
magnetic field was applied. The animals were imaged 48 hours post
delivery by local perivascular administration of 2.5 mg of
luciferin admixed in 250 .mu.l of 25% Pluronic F127 dissolved in
PBS. This formulation undergoes phase transition between solution
and gel at temperatures higher than 30.degree. C. and thus
immediately solidifies upon contact with tissue, forming a drug
depot with well defined (24) rapid release kinetics. The imaging
was initiated 5 minutes after delivery. The integration time was 10
min. For immunohistochemical detection of luciferase,
paraformaldehyde-fixed cryoembedded arterial sections were stained
with anti-luciferase mouse monoclonal antibody (Upstate-Millipore,
Temacula, Calif., clone mAb21, 1:100) using a peroxidase/DAB
method.
[0171] Statistics. Experimental data were presented as
means.+-.standard errors (SE). The results were evaluated by
regression analysis. The Student t test was used to analyze the
significance of differences in data sets. Differences were termed
significant at p<0.05.
[0172] Results. Polylactide MNPs were prepared by a modified
emulsification-solvent evaporation methodology with the
incorporation of oleate-coated iron oxide nanocrystals
(Quintanar-Guerrero D et al. (1998) Drug Dev. Ind. Pharm.
24:1113-28) using bovine serum albumin (BSA) as a surface
stabilizing agent. Albumin-stabilized MNP displayed a narrow size
distribution with an average diameter of 290.+-.15 nm (FIG. 11A)
and exhibited superparamagnetic behavior showing no significant
hysteresis, and a remnant magnetization on the order of 0.5% of the
saturation magnetization value. The stent material used was 304
grade stainless steel, which was chosen for its combination of
suitable magnetic properties and its corrosion resistance to
aqueous environments. The 304 stents also exhibited nearly
superparamagnetic behavior showing only slight magnetic hysteresis
and displaying a remnant magnetization on the order of 7% of the
saturation magnetization value (FIG. 15A). 316L stainless steel
stents were also tested but were not included in targeting studies
due to their less responsive magnetic properties (FIG. 15A).
[0173] A subset of MNP were formulated with polylactic acid (PLA)
that was covalently modified with BODIPY 564/570 thereby resulting
in MNP that could be used in fluorescent microscopy experiments and
fluorometry based quantitation studies (Chorny M et al. (2006) Mol.
Ther. 14:382-91). This formulation was used to characterize the
kinetics of cell loading with MNP. Bovine aortic endothelial cells
(BAEC) in confluent cell cultures were incubated with various doses
of BODIPY 564/570-MNP on a cell culture magnet (see Materials and
Methods). The MNP uptake was determined at different time points by
measuring the fluorescence of internalized nanoparticles. The
amount of the internalized MNP was linearly dependent upon the MNP
dose in the tested range (FIG. 12A). Approximately 30% of
internalization was observed after 8 hours and the uptake was
essentially complete after 24 hours (FIGS. 12A and 15B). Cell
viability was not adversely affected by internalized MNP, as
assessed by the results of Calcein Green staining and Alamar Blue
assays (FIGS. 15B and 12B respectively). Cell survival of 83.+-.3%
relative to untreated cells was observed at the highest applied MNP
dose, 9 .mu.g/well (corresponding to a MNP loading of 0.3 ng/cell),
and at the maximal incubation time of 24 hours (FIG. 12B). Based on
these results, a MNP dose of 0.2 ng/cell was chosen for subsequent
experiments (92.+-.2% cell survival, a dose of 5.8 .mu.g/well per
FIG. 12B). As expected, BAEC laden with MNP demonstrated
superparamagnetic behavior, showing hysteretic properties similar
to free (non-cell associated) MNP (i.e., a remnant magnetization of
less than 1% of the saturation value) (FIG. 15A).
[0174] MNP-loaded endothelial cell targeting to 304 grade stainless
steel stents was first studied in a model flow-loop system. In the
absence of an externally applied uniform magnetic field, almost no
cell capture was observed (FIG. 16A). However when a uniform
magnetic field was applied across the stent within the flow loop
system, the stent captured a significant percentage of the
circulating cells, demonstrating an initial rate of 1% of cells
captured per minute (FIG. 16A). Saturation in cell capture was
observed within 50 min after the magnetic field was applied,
resulting in the targeting of 20% of the circulating cells (ca.
0.5.times.10.sup.6). Approximately 50% of the captured cells (ca.
0.25.times.10.sup.6) accumulated on the stent surface within the
first 6 minutes. FIG. 16B shows the stent surface at the end of the
experiment with adherent cells completely covering the stent wire
surfaces, as demonstrated by red MNP fluorescence microscopy
results and Calcein Green staining indicating viability of the
captured cells (FIG. 16C).
[0175] Acute rat carotid stenting studies were carried out by
transthoracic injection of BAEC loaded with MNP into the left
ventricular cavity in the presence of a uniform magnetic field
(1000 Gauss) across the region of the stented artery (FIGS. 16D and
E). The animals were euthanized 5 minutes after magnetic targeting,
and the stents retrieved, revealing targeting of MNP to 304 grade
stainless steel stent surfaces in the presence of a magnetic field
(FIG. 16D), again with complete uniform coverage of the stent wires
with cells containing fluorescent MNP. However, in the absence of a
magnetic field, no detectable MNP-loaded BAEC were demonstrable
(FIG. 16E). Thus, these short-term in vivo results were comparable
to the in vitro targeting studies (FIG. 16B).
[0176] Experiments using BAEC both loaded with MNP and transduced
with luciferase encoding replication defective adenoviruses (AdLuc)
were carried out next. Initial studies examined magnetic targeting
of MNP-loaded Luc modified BAEC with local delivery in a stop-flow
setting (FIG. 16F), using Luc transgene activity as an endpoint,
detected with intravital bioluminescence imaging (FIG. 16F). After
in vitro AdLuc transduction and preloading with MNP, BAEC were
harvested and locally delivered to an isolated stented segment of
each rat's carotid artery in the presence or absence of a magnetic
field (FIG. 16F). The stented vessel was temporarily tied off at
both ends (stop-flow delivery technique) while the MNP-loaded BAEC
were delivered to the stented section for a brief period of
approximately 15 seconds (FIG. 16F). The cell suspension was then
evacuated from the artery, and the magnetic field was maintained
for an additional 5 minutes before the circulation was allowed to
resume. The animals were recovered and studied 48 hours later, and
as expected, significantly greater transgene expression (p=0.045)
was demonstrated using local perivascular luciferin administration
followed by bioluminescent in vivo optical imaging, in animals that
had been administered with MNP-loaded BAEC in the presence of a
uniform magnetic field compared to a control group not subjected to
magnetic delivery conditions (FIG. 16F). It is also noteworthy that
bioluminescent whole body imaging scans of the animals in these
studies revealed an absence of transgene activity except within the
stented carotid segments (data not shown).
[0177] Magnetically targeted delivery of MNP-loaded BAEC without
interruption of the stented carotid blood flow was also
investigated by injecting the MNP-loaded BAEC expressing Luc over
the course of 1 minute through a catheter positioned in the aortic
arch with exposure to a uniform magnetic field for 5 minutes (FIG.
16G). Specific targeting to the deployed stents due to the applied
field was demonstrated after 48 hours by bioluminescent imaging
(FIG. 16G), with no detectable Luc activity present in stented
arterial segments that were not exposed to a magnetic field
(p=0.005). Furthermore, there was an absence of bioluminescence in
distal sites (data not shown) in these studies as well.
Luc-positive immunostaining confirmed the presence of transgene
activity in the intimal and medial regions of the stented arterial
segments that were exposed to magnetic cell targeting (data not
shown).
Example 13
Use of a MRI Homogenous Magnetic Field to Target Magnetic
Nanoparticle-Loaded Cells to a 316L Stent
[0178] A model experiment was carried out to demonstrate the
feasibility of targeting cells loaded with magnetic nanoparticles
(MNP) to steel stents using the homogeneous magnetic field present
in a magnetic resonance imaging (MRI) system. The field present in
the imager, 1.5 Tesla (T) is 15-fold greater than the highest
fields used in other studies (1000 Gauss, or 0.1 Tesla).
Furthermore, prior studies used 304 steel stents that were
magnetized in a 0.1 Tesla field, whereas 316L steel stents were not
magnetized at this level of field strength. Furthermore, it should
be noted that the majority of steel stents used today clinically
are 316L steel, and thus this model experiment is particularly
clinically relevant.
[0179] The experiment was carried out as follows: Bovine arterial
endothelial cells (BAEC) were preloaded with red fluorescent
polylactic acid (PLA) MNP prepared as described above on day -1.
The cells were trypsinized, resuspended in 5 ml of cell culture
medium (DMEM supplemented with 10% FBS) before the experiment, and
divided in two halves. Stainless steel 316 grade stents (Crown,
Cordis, Warrenton, N.J.) were deployed in flexible
polyvinylchloride tubes, to simulate arterial deployment, attached
to syringes. The cell suspension was extruded from the syringe
through the tube with the stent within it over a 1 min period
(collecting the cell suspension in the 2nd syringe) with or without
an exposure to a homogenous magnetic field (1.5 Tesla) within the
core of a MRI imager. The stents were imaged by fluorescent
microscopy using an inverted fluorescent microscope immediately
after the experiment before and after stent removal from the tubes.
The results shown in FIG. 17 demonstrate red fluorescent cells
present on all of the 316L stent struts of the stent samples that
were exposed to the 1.5 T field. However, the control stent, which
had cells (plus fluorescent MNP) injected through the stented
polyvinylchloride tubing demonstrated only rare red fluorescent
cells. Thus, these studies demonstrate that the homogenous field
present within a MRI imager can magnetize a 316L stent and thereby
enable magnetic cell targeting. These results show that MNP
targeting by simply injecting a suspension of MNP (without loading
them into cells), would also target a 316L stent in the 1.5 T
field.
Example 14
Superparamagnetic Polymeric Nanoparticles Efficiently Enhance
Non-Viral Nucleic Acid Delivery
[0180] Non-viral delivery of nucleic acids for therapeutic purposes
remains a challenge mainly due to a comparatively low efficacy. We
addressed this problem by using non-viral gene carriers possessing
magnetic targeting properties. The achievable via magnetic force
targeted delivery of nucleic acids may provide a clinically viable
solution for effective and non-toxic gene transfer. In our previous
work we developed formulations of polylactide (PLA)-based
biodegradable nanoparticles (NP) surface modified with branched
polyethylenimine (PEI 25K). Recent scientific literature showed
that deacylation of commercial preparations of linear PEI
dramatically boosted its gene delivery efficiency due to increase
in the number of protonatable nitrogens, which presumably results
in a tighter condensation of nucleic acid and a better endosomal
escape of the PEI/nucleic acid complexes. The present studies
investigated the hypothesis that non-viral gene transfer can be
enhanced via magnetically driven delivery of superparamagnetic NP
formulated with deacylated linear PEI. The linear PEI synthesized
by acid-catalyzed hydrolysis of 200-kDa poly(2-ethyl-2-oxazoline)
and adjusted to pH7 was used to formulate iron oxide laden NP by
means of modified emulsification-solvent evaporation methodology.
NP containing 35% iron oxide by weight had an average size of
360.+-.25 nm, zeta-potential of 43.+-.3 mV and exhibited
superparamagnetic properties (magnetic remnance less than 0.5% of
their magnetic saturation value). The ability of linear PEI-NP
formulation to deliver nucleic acids was examined in vitro in
cultured A10, rat aortic smooth muscle cells (SMC) and bovine
aortic endothelial cells (BAEC), using green fluorescent protein
(GFP) as a reporter gene. NP formulated with branched PEI were used
for comparison. NP complexed with nucleic acids were applied to
cells for 15 min under magnetic field (500 G) in serum-containing
cell culture medium. In one set of experiments, GFP encoding
plasmid DNA was delivered to the cells and the transfection
efficiency was measured fluorimetrically 2, 4 and 8 days post
treatment. Intracellular NP levels were directly dose dependent in
examined NP concentration range for both PEI formulations. The GFP
expression reached its maximal level for both PEI formulations at
day 4 resulting in 2.5-3 times higher GFP levels for both cell
types transfected with linear PEI-NP formulation. In another set of
experiments, enhanced GFP (eGFP) short interfering RNA (siRNA) was
delivered to the cells and the suppression of eGFP expression in
lentivirus transduced smooth muscle and endothelial cells as well
as cell viability (by AlamarBlue) were measured fluorimetrically 5
days post treatment. In GFP silencing experiments, efficient eGFP
suppression was achieved using magnetic NP formulated with either
branched or linear PEI. The eGFP suppression in A10 cells depended
directly on the NP dose for both formulation types. The suppression
of eGFP was directly siRNA dose dependent in the case of linear
PEI-NP and inversely dependent for branched PEI-NP resulting in a
maximal suppression of 40% for both NP types. In BAEC, the eGFP
suppression depended directly on the NP dose for the branched
PEI-NP only. The eGFP suppression was not dependent on the siRNA
doses for both NP types resulting in a maximal suppression of 50%
for both NP formulations. Studied NP/siRNA complexes did not
significantly compromise cell survival showing more than 90% of
viable cells 5 days post treatment at maximal NP dosages for both
NP and cell types. It is concluded that magnetically responsive
linear PEI-NP demonstrated increased delivery efficiency of plasmid
DNA versus branched PEI-NP while in the gene silencing experiments
no difference in capacity to suppress genes for both types of NP
was observed.
Example 15
Magnetically Directed Catalase-Containing Calcium Oleate
Nanoparticles Efficiently Protect Endothelial Cells from Oxidative
Stress In Vitro
[0181] Considerations of large enzyme nanocarrier design are
multifold. Conditions of particle synthesis and subsequent
purification should allow efficient loading of protein mass while
sustaining enzymatic activity. In order for nanocarriers of large
enzymes such as catalase to be effective targeted antioxidant
therapeutics, the carriers should have the capacity to not only
load active enzyme, but also to provide protection from
proteolysis. It is desirable to devise a stable, biocompatible
nanocarrier that would load protein efficiently without organic
solvents or high sheer emulsion methods. In order to preserve
protein activity, water soluble constituents were used that would
form calcium oleate-based MNP in aqueous media, and eliminate
exposure of protein to damage by sheer, solvent exposure, and oil
and water interfaces.
[0182] These studies were carried out to assess the capacity of MNP
to load ample and active enzymes, and to characterize the effect of
variables on the properties of catalase-loaded MNP, including their
size, magnetic behavior, protein loading efficiency and
functionality. Protection from proteolytic degradation and release
of the protein over time in vitro were examined. Finally, the
magnetically guided internalization of MNP, their antioxidant
activity and capacity to prevent ROS-mediated cell death were
studied in cell culture in comparison to non-magnetic controls or
free catalase.
[0183] Reagents. Ferric chloride hexahydrate, ferrous chloride
tetrahydrate, sodium oleate (99% pure), Pluronic.RTM. F127,
xanthine, xanthine oxidase, and pronase were all purchased from
Sigma-Aldrich (St Louis, Mo.). Uranyl acetate was from Electron
Microscopy Sciences. Catalase and Cu, Zn superoxide dismutase, both
from bovine liver, were purchased from Calbiochem (La Jolla,
Calif.). Iodogen and Dylight 488 were purchased from Pierce
Biotechnology (Rockford, Ill.). Other reagents were purchased from
Fisher Scientific (Pittsburgh, Pa.).
[0184] Enzyme preparation and iodination. Solid bovine liver
catalase was dissolved in DI water and dialyzed (Slide-a-lyzer
dialysis cassette, Thermo Scientific, Rockford Ill.) in sodium free
phosphate buffer. Superoxide dismutase (SOD) was dissolved in PBS
to desired concentrations. Final protein concentrations were
determined from calibration curves of BSA using a standard Bradford
assay measured by UV absorbance at 595 nm (Cary 50 UV-vis, Varian,
Palo Alto, Calif.).
[0185] Catalase and SOD were radiolabeled with Na-.sup.125I (Perkin
Elmer, Boston, Mass.) using the Iodogen (Pierce Biotech., Rockford,
Ill.) method as described by the manufacturer, and purified from
unbound iodine using gel permeation chromatography (Biospin 6
Columns, Bio-Rad Labs, Hercules, Calif.). One modification was
necessary for labeling SOD; the enzyme contains only two tyrosine
residues, consequently the extent of radiolabeling at pH 7.4 is
poor. By using Tris buffer at pH 8.4 histidine residues were tagged
(pK.sub.A 6.5) and radiolabeling was increased by over 4.times..
The extent of labeling and amount of free iodine was determined for
both proteins using a standard trichloroacetic acid (TCA) assay. A
2 .mu.l aliquot of labeled enzyme, 1.0 ml 3% BSA and 0.2 ml 100%
TCA were vortexed and incubated at RT for 15 mins. Precipitated
protein was separated from free iodine supernatant by
centrifugation (15 mins, 4.degree. C., 2100 g) and measured using a
Wizard 1470 gamma counter (Wallac Oy, Turku, Finland).
[0186] Fluorescent labeling of catalase was carried out as
described by the manufacturer through amine reactive labeling using
N-hydroxysuccinimide (NHS) ester moiety to form a reactive
acylating reagent.
[0187] MNP formulation and characterization. Nanocrystalline iron
oxide was prepared by co-precipitation of ferrous and ferric
chlorides (62.5 and 170 mg, respectively) from ethanol solution
(2.5 ml) with an equivalent amount of aqueous sodium hydroxide (0.5
N, 5.0 ml). Iron oxide was maturated by incubating it for 1 min at
90.degree. C., then washed twice with deionized (DI) water
(Direct-Q 5 System, Millipore, Billerica, Mass.) by magnetic
decantation on ice, and finally resuspended in 5 ml of an aqueous
solution containing 225 mg of sodium oleate by heating to
90.degree. C. under argon followed by bath sonication (5 min each)
repeated in two cycles. The obtained ferrofluid was filtered
through a sterile PVDF membrane with a 5 .mu.m cut-off.
[0188] To prepare enzyme-loaded MNP, protein was added to the
ferrofluid at a specified amount. A controlled aggregation of the
ferrofluid was carried out in the presence of Pluronic.RTM. F-127
(20 mg) as a stabilizer by dropwise addition of an equal volume of
aqueous calcium oleate (0.1 M). MNP were washed twice by magnetic
decantation and finally resuspended in aqueous solution of glucose
(5% w/v). Radioactive-labeled formulations were prepared by
admixing a fraction of .sup.125I labeled catalase to the protein
prior to the controlled aggregation step. Formulations of
enzyme-impregnated non-magnetic nanoparticles or blank MNP used as
controls were prepared as described above without incorporation of
iron oxide or enzyme, respectively.
[0189] Particle size, concentration and magnetic behavior. Particle
size was measured by dynamic light scattering (DLS, 90Plus Particle
Sizer, Brookhaven Instruments, Holtsville, N.Y.) and transmission
electron microscopy (JEOL JEM-100CX TEM West Chester, Pa.).
Particle size distributions and mean hydrodynamic radii of samples
diluted 200-400.times., were derived from the second order
diffusion coefficient from the Stokes Einstein equation. Particle
number concentration was derived by mass balance of experimentally
determined density of the sample solution, dry weight, and size of
the particles.
[0190] For transmission electron microscopy (TEM), 2-5 .mu.l of MNP
sample diluted 20.times.in 0.2 .mu.m filtered DI water was added to
individual TEM mesh grids (Formvar Film 200 mesh, Electron
Microscopy Sciences, Hatfield, Pa.), excess sample was wicked with
filter paper. Grids were dried in a vacuum desiccator for at least
1 hr before they were imaged with an accelerating voltage of 80
keV.
[0191] To determine the magnetic behavior of MNP 5 .mu.l of the
suspension were air-dried on a cover-glass slide, and hysteresis
measurements were made using an alternating gradient magnetometer
(Princeton Measurements Corp., NJ).
[0192] Iron concentration. The iron retained in the particles was
measured in triplicate samples against a calibration curve
constructed from a 2:1 molar mixture of ferrous and ferric
chlorides in a range of 0.1-25.0 mg/ml. Each dilution of 10 .mu.l
was added to 1.0 ml HCl (6 M) and 10 .mu.l H.sub.2O.sub.2 (3 wt %)
and allowed to react in the dark for 1 hr. Light absorption was
read at 410 nm.
[0193] Enzyme loading. The incorporation of protein in MNP was
determined by measuring the distribution of the radiolabeled SOD or
catalase between magnetically separated MNP and the external
aqueous phase using a gamma counter. Percentage retained is defined
as the quotient of the activity in the final sample to that of the
original suspension adjusted for volume changes.
[0194] Enzyme activity. The catalase activity was determined using
a standard hydrogen peroxide degradation assay. PBS-buffered 5 mM
H.sub.2O.sub.2 solution (990-998 .mu.l) was added to a quartz
cuvette and the absorbance at 242 nm was read at room temperature.
Catalase containing particles were diluted to a final catalase
concentration of .about.0.01-0.50 .mu.g/ml corresponding to the
linear region of the calibration plot where the slope of the decay
curve was proportional to the concentration of the catalase added.
Two to ten .mu.l of MNPs were typically diluted to make a total
volume of 1.0 ml. The concentration of the H.sub.2O.sub.2 was
monitored versus time and the activity of the catalase was
calculated from the slope of the decay curve where 1 unit
activity=23 (.DELTA. Abs/t).
[0195] SOD activity was determined using the ferricytochrome C
assay. The cytochrome C assay uses xanthine and xanthine oxidase to
generate superoxide anion with cytochrome C acting as an indicating
scavenger which competes with SOD. A solution containing 50 mM
phosphate buffer, pH 7.8, 0.1 .mu.M EDTA, 50 .mu.M xanthine, 20
.mu.M cytochrome C and 10 .mu.l sample. The reaction was initiated
by the addition of 10 .mu.l of 0.2 U/ml xanthine oxidase. The
absorbance was monitored at 550 nm. One unit of SOD is defined as
the amount of enzyme that inhibits the rate of cytochrome C
reduction by 50% at pH 7.8 and 25.degree. C.
[0196] Protection and activity of MNP-encapsulated catalase. The
capacity of MNP to protect the catalase cargo was measured using a
proteolysis assay. Samples were incubated for 60 min at 37.degree.
C. with shaking in a 0.2 wt % buffered Pronase, a robust mixture of
proteinases which completely digests proteins into individual amino
acids. The amount of catalase retained by MNP post proteolysis was
determined following MNP separation by centrifugation (20 min,
4.degree. C. at 16.1 g) using the radioactivity assay described
above. The enzymatic activity of MNP-bound catalase retained over
time was measured in comparison with free catalase.
[0197] Catalase in vitro release from MNP. The release kinetics of
catalase from MNP in biological fluids at relevant physiological
temperature was measured by monitoring free catalase in the release
medium using the radioactivity assay. Equal volumes of particle
suspensions and mouse plasma were combined and placed in a
37.degree. C. shaker bath. Aliquots were taken over a 48 hour
period and MNP were separated from the medium using 0.2 .mu.m
centrifugal filter units (Millipore, Billerica Mass.). A correction
was made for the fraction of MNP determined in the filtrate
(<10%). The radioactivity of MNP-bound catalase retained by the
filters and free protein in the medium were measured using a gamma
counter.
[0198] Cell culture. Bovine aortic endothelial cells (BAECs) were
obtained and cultured in DMEM (Mediatech, Inc., Herndon, Va., USA)
supplemented with 10% fetal calf serum. Primary human umbilical
vein endothelial cells, 4th passage, (HUVECs, Clonectics, San
Diego, Calif.) grown to near confluence were cultured on 1%
gelatin-coated 24 or 96 well plates. Cells were maintained in M199
media (Gibco, Grand Island, N.Y.) supplemented with 15% fetal
bovine serum and 100 ug/ml heparin (Sigma), 0.1% endothelial cell
growth supplement (Upstate, Lake Placid, N.Y.), 0.1 .mu.g/ml
Glutamax, and 1.0% antibiotic-antimycotic (Gibco).
[0199] Magnetically guided delivery of MNP to BAECs. BAECs seeded
at confluence on a 96-well plate were incubated with MNP for 5 min
with/without the presence of a high gradient magnetic field using a
96-well magnetic separator with an average cross-sectional force
density of 5.6 T.sup.2/m as a magnetic field source (LifeSep.TM.
96F, Dexter Magnetic Technologies, Fremont, Calif., USA). The cells
were then washed twice, incubated with fresh cell culture medium
and examined microscopically for MNP internalization 4 hr post
treatment.
[0200] Magnetically enhanced protection of HUVECs from oxidative
stress by MNP. Confluent HUVECs seeded on 24-well plates were
incubated with MNP at 37.degree. C. with or without a magnetic
exposure for 15 min. MNP were then aspirated and cells rinsed with
fresh cell culture medium. Non-magnetic catalase-loaded
nanoparticles or blank MNP (no catalase) were used as controls.
Cells were treated with 10 mM H.sub.2O.sub.2 diluted in cell
culture media for 5 hours, rinsed with fresh media, then stained
for 15 min with a 2 .mu.M solution of Calcein AM (Invitrogen, CA)
in PBS supplemented with Ca.sup.2+ and Mg.sup.2+. The fluorescence
of viable cells was measured after washing at .lamda.em/.lamda.ex
of 485 nm/535 nm.
[0201] Results
[0202] MNP physiochemical properties (Particle size). Particle size
of the catalase loaded MNPs determined by digital analysis of
multiple TEM images (example in FIG. 18A) showed an average size of
303+/-38 nm. Dynamic light scattering (DLS) of equivalent
formulations showed a mean particle size of 340+/-29 nm (FIGS. 18C
and 18D). Per dynamic light scattering measurements, SOD loaded
particles had a hydrodynamic diameter of 350+/-10 nm.
[0203] MNP physicochemical properties (Magnetic properties). The
MNP iron concentration was determined to be .about.21 wt % as
measured by colorimetric assay. The magnetic behavior of the MNPs
is shown in FIG. 18B. The magnetic moment at saturation (Ms) is
14.3 emu/g. The magnetic remanence (Mr), the magnetization retained
after the magnetic field is removed, is 0.65 emu/g. The retention
of magnetization as a percentage, Mr/Ms, is therefore 4.5%. The
closed hysteresis loop in FIG. 18B shows that the particles
immediately return to equilibrium with the removal of the magnetic
field.
[0204] Enzyme mass and activity loading. As a percentage of added
protein retained by the purified particles, the mass loading of SOD
in MNP was 39+/-1%, 34+/-1% for 0.5 and 1.0 mg addition of protein
respectively (FIG. 19A). This corresponds to approximately 7500 and
15000 SOD molecules per particle as calculated from mass loaded
(FIG. 19B). Loading of catalase over different mass additions is
shown in Table 1.
TABLE-US-00001 TABLE 1 MNP properties versus catalase addition.
Catalase % Catalase mass Diameter % Catalase % Catalase activity
added (mg) (nm) mass loaded mass protected retained 0 336 .+-. 15
0.2 341 .+-. 29 24.1 .+-. 9.8% 29 .+-. 1.0% 29.4 .+-. 1.0% 2 365
.+-. 29 20.4 .+-. 0.6% 11.4 .+-. 0.4% 23.1 .+-. 0.6% 4 399 .+-. 14*
33.0 .+-. 5.0% 22.7 .+-. 2.1% 33.9 .+-. 4.8% 6 385 .+-. 3.0** 28.0
.+-. 3.0% 25.9 .+-. 2.3% 20.2 .+-. 4.2% Error is standard
deviation; n .gtoreq. 3. Size difference *p = 0.0145, **p = 0.0017
compared to blank MNPs.
[0205] Retention of activity of SOD in MNPs at both mass loadings
averaged 17.2+1/-2% of added, which corresponds to an average of
47% activity retained of mass loaded (FIG. 19C). Catalase activity
in MNPs retained reaches a maximum of about 12 kUnits at 4 mg mass
addition (FIG. 19B) which corresponds to about 34% of activity
retained (Table 1). Other mass additions ranged from 20-29% with
the minimum activity loaded found with the maximum mass addition 6
mg (Table 1).
[0206] MNPs shield catalase mass and activity in vitro. The mass of
catalase protected from proteolysis versus mass addition ranged
from near 12% to 29% as shown in Table 1. The relationship between
catalase mass loaded and protected is shown in FIG. 21A. MNPs
retained 20% of starting activity by 24 hours of exposure to
proteolytic enzymes compared to total deactivation of free enzyme
by 30 mins (FIG. 21B).
[0207] The stability of MNPs as defined by retention of catalase
with exposure to plasma is shown in FIG. 22. Particles released
near to 15% of catalase at 48 hours of exposure to plasma at
37.degree. C. compared to a nearly equivalent release with the
control solution.
[0208] Magnetically driven MNP delivery to endothelial cells in
vitro. MNPs incubated with endothelial cells exposed to a magnetic
field for 10 min are shown in FIGS. 23A and 23B. The contrast
micrograph in 23A shows the MNPs within the cytosol of the
endothelial cells surrounding the nuclei. The green fluorescence in
FIG. 23B indicates the protein cargo of the particles delivered to
the cells. FIG. 23C shows the catalase of the MNPs within the cells
with a 5 min exposure. Association of the nanocarriers with cells
without exposure to a magnetic field is shown in FIGS. 23D and
23E.
[0209] Protection of endothelial cells from oxidative stress.
Fluorescence intensity was used to quantify the percentage of
protection by various treatments (FIG. 24A). Magnetically delivered
catalase within MNPs showed a protective effect of 62.+-.12% cell
viability relative to untreated cells when exposed to 10 mM
hydrogen peroxide for 5 hours as shown in FIG. 24B. No statistical
difference existed between the protective effects of the MNPs
without magnetic guidance, the carriers without catalase, or with
free catalase added with carriers.
[0210] Summary. This study describes a unique biocompatible, large
protein nanocarrier system which loads active enzyme efficiently,
without excessive lose of activity for both SOD and catalase, and
provides the enzymatic activity protection from proteolysis in with
the catalase formulation, a larger and more labile enzyme, and
therefore more challenging to protect. Furthermore, via magnetic
targeting the carrier system demonstrated a therapeutic potential
by combating a severe oxidative insult in vitro. This novel
approach to targeted enzyme delivery can not only be translated to
other therapeutics, large molecules, peptides, and nucleotide
applications, but as demonstrated by the capacity of nanocarriers
to retain cargo in plasma, shows the viability and robustness to
explore surface modification for potential immunotargeting. The
attributes of this carrier system described could be translated to
numerous pathologies related by oxidative stress.
Example 16
Antibody Targeting of Catalase Containing Magnetic Nanoparticles In
Vitro and In Vivo
[0211] These studies were undertaken to test the capacity of these
magnetic nanocarriers (MNP) to load and deliver active antioxidant
enzymes to endothelial targets in vitro and in vivo.
[0212] While antioxidant enzymes such as catalase can alleviate
oxidative stress, they have little intrinsic affinity for target
sites in vivo and are vulnerable to proteolysis and
reticuloendothelial (RES) clearance. To solve these problems,
catalase (MW.about.250 kDa) was encapsulated into biocompatible,
calcium oleate-based magnetic nanoparticles using a controlled
precipitation of aqueous phases as described in detail in Example
15 (See "MNP formulation and characterization"). The two-step
process of MNP formulation is shown schematically in FIG. 25.
[0213] Calcium cations complex oleate anions, forming particles (an
average diameter .about.400 nm by DLS) that are surface stabilized
by Pluronic.RTM. F127 surfactant. Catalase associates with forming
complexes presumably through hydrophobic and charge interactions.
The magnetic responsiveness of the nanoparticles enables their
rapid separation from unincorporated substances, thereby
facilitating purification of the nanoparticle formulation. Loading
efficiency is 20-30% with 80% of that activity retained.
Approximately 20% of MNP-loaded catalase was resistant to
proteolysis in vitro by a non specific protease mixture,
pronase.
[0214] For targeting MNPs to endothelial cells, Pluronic.RTM. F127
surfactant was dual biotinylated to incorporate
streptavidin-conjugated targeting antibody to endothelial antigen,
PECAM (Ab62) (Table 2). The affinity of streptavidin (SA) to
surface biotinylated MNP was measured vs. control (FIG. 26A).
TABLE-US-00002 TABLE 2 MNP properties versus extent of
biotinylation. % % % % % bio- Catalase Catalase Catalase Pluronic
tinylated Diameter mass mass activity retained Pluronic (nm) loaded
protected retained overall 0 399 .+-. 14 33 .+-. 5.0% 22.7 .+-.
2.1% 33.9 .+-. 4.8% 19% 2 420 34 18.3 25.1 15% 5 475 33.4 16.2
20.7
[0215] To test targeting and therapeutic potential anti-PECAM vs.
IgG decorated particles were incubated with human umbilical
endothelial cells (HUVECs). Isotope and fluorescence tracing showed
that anti-PECAM(Ab62)/MNP, but not IgG/MNP (control) bind to HUVEC
(FIG. 26) and protect cells from hydrogen peroxide inflicted
oxidative stress (76%.+-.5% protection as measured by release of
.sup.51Cr) (FIG. 27). Intravenous injection of radiolabeled
anti-PECAM(Ab62)/MNP, but not IgG/MNP (control) in C57BL/6 mice led
to a 28-fold higher pulmonary retention of anti-PECAM/MNPs
(212.+-.25% ID/g i.e., 27.6 times higher than IgG/MNP), indicating
efficient targeting to vascular endothelium (FIG. 28).
[0216] These data show the following: (1) Calcium oleate based
magnetic nanocarriers form and incorporate catalase stably; (2)
Magnetic nanocarriers load and protect catalase in terms of mass
and activity; (3) Including biotinylated Pluronic.RTM. F-127 allows
for SA-antibody attachment to MNPs; (4) Surface coating of
anti-PECAM antibodies on MNPS allows for targeted delivery of MNPs
to ECS; (5) Anti-PECAM antibody coated MNPs are endocytosed by
endothelial cells at 37.degree. C.; (6) Both magnetic and antibody
guided MNP delivery provide protection of ECs from oxidative
damage; and, (7) Anti-PECAM antibody coated MNPs specifically
target of lung endothelium. These data suggest a high potential
efficacy of targeting antioxidant enzymes therapies with
catalase-bearing calcium oleate-based nanoparticles.
[0217] The present invention is not limited to the embodiments
described and exemplified above, but is capable of variation and
modification within the scope of the appended claims.
* * * * *