U.S. patent application number 12/404970 was filed with the patent office on 2009-11-12 for superfine fiber creating spinneret and uses thereof.
Invention is credited to Karen Lozano, Kamalaksha Sarkar.
Application Number | 20090280207 12/404970 |
Document ID | / |
Family ID | 41063306 |
Filed Date | 2009-11-12 |
United States Patent
Application |
20090280207 |
Kind Code |
A1 |
Lozano; Karen ; et
al. |
November 12, 2009 |
SUPERFINE FIBER CREATING SPINNERET AND USES THEREOF
Abstract
Apparatuses and methods for the production of superfine
fibers.
Inventors: |
Lozano; Karen; (McAllen,
TX) ; Sarkar; Kamalaksha; (Edinburg, TX) |
Correspondence
Address: |
FULBRIGHT & JAWORSKI L.L.P.
600 CONGRESS AVE., SUITE 2400
AUSTIN
TX
78701
US
|
Family ID: |
41063306 |
Appl. No.: |
12/404970 |
Filed: |
March 16, 2009 |
Related U.S. Patent Documents
|
|
|
|
|
|
Application
Number |
Filing Date |
Patent Number |
|
|
61037184 |
Mar 17, 2008 |
|
|
|
61037193 |
Mar 17, 2008 |
|
|
|
61037209 |
Mar 17, 2008 |
|
|
|
61037216 |
Mar 17, 2008 |
|
|
|
Current U.S.
Class: |
425/382.2 ;
425/464 |
Current CPC
Class: |
D01D 5/18 20130101; D01D
5/06 20130101; D10B 2201/28 20130101; Y10T 428/298 20150115 |
Class at
Publication: |
425/382.2 ;
425/464 |
International
Class: |
D01D 4/02 20060101
D01D004/02; D01D 7/00 20060101 D01D007/00 |
Claims
1. A spinneret comprising: a bottom plate; a top plate; and a
micro-mesh material separating the bottom plate from the top plate,
the spinneret being configured to rotate about a spin axis.
2. The spinneret of claim 1, wherein the micro-mesh material is
stainless steel or plastic.
3. The spinneret of claim 1, wherein the pore size of the
micro-mesh material ranges between 0.01 mm to 3.0 mm.
4. The spinneret of claim 1, wherein the distance spanned by the
micro-mesh material between the bottom plate and the top plate
ranges between 1-10".
5. The spinneret of claim 1, where both plates comprise
substantially similar outer profiles.
6. The spinneret of claim 1, where the spinneret is configured to
withstand temperatures ranging from -20.degree. C. to 2500.degree.
C.
7. An apparatus for creating superfine fibers, comprising: a driver
configured to be rotated at 500 RPM or more; a spinneret coupled to
the driver; and a superfine fiber collection device; where the
apparatus is configured to create superfine fibers by rotating the
spinneret with the driver, and without subjecting the superfine
fibers, during their creation, to either an externally-applied
electric field or an externally-applied gas, and without the
superfine fibers falling into liquid after being created, wherein
the spinneret comprises the spinneret of claim 1.
8. The apparatus of claim 7, where the superfine fiber is a
microfiber.
9. The apparatus of claim 7, where the superfine fiber is a
sub-micron fiber.
10. The apparatus of claim 7, where the superfine fiber is less
than 300 nanometers (nm) in diameter.
11. The apparatus of claim 7, where the superfine fiber is a
nanofiber.
12. The apparatus of claim 7, where the superfine fiber is one
micron or longer.
13. The apparatus of claim 7, where the driver is configured to be
rotated at 5,000-25,000 RPM.
14. The apparatus of claim 7, where the superfine fiber collection
device is a collection wall.
15. The apparatus of claim 14, where the collection wall at least
partially surrounds the spinneret.
16. The apparatus of claim 14, where the collection wall completely
surrounds the spinneret.
17. The apparatus of claim 7, where the superfine fiber collection
device is a collection rod.
18. The apparatus of claim 7, where the superfine fiber collection
device is an elongated structure with open ends and an open
top.
19. The apparatus of claim 7, where the driver comprises a
motor.
20. The apparatus of claim 7, further comprising: a heater
thermally coupled to the spinneret.
21. The apparatus of claim 20, where the heater is an inductive
heater, a resistance heater, an infrared heater, or a
thermoelectric cooler.
22. The apparatus of claim 7, further comprising: a cooler
thermally coupled to the spinneret.
23. The apparatus of claim 22, where the cooler is a thermoelectric
cooler.
24. The apparatus of claim 7, further comprising: an intermediate
wall surrounding the superfine fiber collection device.
25. The apparatus of claim 24, further comprising: a housing
surrounding at least the spinneret, the superfine fiber collection
device, and the intermediate wall, the housing including an inlet
for the introduction of a gas.
26. The apparatus of claim 25, where the housing is insulated.
27. The apparatus of claim 7, where one or more components of the
apparatus is made of stainless steel.
28. The apparatus of claim 7, where the apparatus is configured to
be operated under sterile conditions.
29. The apparatus of claim 7, where the apparatus is configured to
be operated under pressures of 1-760 millimeters (mm) of mercury
(Hg).
30. The apparatus of claim 7, where the apparatus is configured to
be operated under pressures of 761 mm Hg to 4 atmospheres (atm).
Description
RELATED APPLICATIONS
[0001] This application claims the benefit of U.S. Provisional
Application No. 61/037,184, filed Mar. 17, 2008; U.S. Provisional
Application No. 61/037,193, filed Mar. 17, 2008; U.S. Provisional
Application No. 61/037,209, filed Mar. 17, 2008; and U.S.
Provisional Application No. 61/037,216, filed Mar. 17, 2008; all of
which are hereby incorporated by reference in their entireties.
BACKGROUND OF THE INVENTION
[0002] 1. Field of the Invention
[0003] The present invention generally relates to the field of
fiber production, such as superfine fibers of micron and sub-micron
size diameters as well as nanofibers. Superfine fibers may be made
of a variety of materials.
[0004] 2. Description of Related Art
[0005] Fibers having small diameters (e.g., micrometer ("micron")
to nanometer ("nano")) are useful in a variety of fields from
clothing industry to military applications. For example, in the
biomedical field, there is a strong interest in developing
structures based on nanofibers that provide a scaffolding for
tissue growth to effectively support living cells. In the textile
field, there is a strong interest in nanofibers because the
nanofibers have a high surface area per unit mass that provide
light but highly wear-resistant garments. As a class, carbon
nanofibers are being used, for example, in reinforced composites,
in heat management, and in reinforcement of elastomers. Many
potential applications for small-diameter fibers are being
developed as the ability to manufacture and control their chemical
and physical properties improves.
[0006] It is well known in fiber manufacturing to produce extremely
fine fibrous materials of organic fibers, such as described in U.S.
Pat. Nos. 4,043,331 and 4,044,404, where a fibrillar mat product is
prepared by electrostatically spinning an organic material and
subsequently collecting spun fibers on a suitable surface; U.S.
Pat. No. 4,266,918, where a controlled pressure is applied to a
molten polymer which is emitted through an opening of an energy
charged plate; and U.S. Pat. No. 4,323,525, where a water soluble
polymer is fed by a series of spaced syringes into an electric
field including an energy charged metal mandrel having a sheath of
aluminum foil wrapper therearound which may be coated with a PTFE
(Teflon.TM.) release agent. Attention is further directed to U.S.
Pat. Nos. 4,044,404, 4,639,390, 4,657,743, 4,842,505, 5,522,879,
6,106,913 and 6,111,590--all of which feature polymer nanofiber
production arrangements.
[0007] Electrospinning is a major manufacturing method to make
nanofibers. Examples of methods and machinery used for
electrospinning can be found, for example, in the following U.S.
Pat. Nos. 6,616,435; 6,713,011; 7,083,854; and 7,134,857.
SUMMARY OF THE INVENTION
[0008] The present invention is directed to apparatuses and methods
of creating fibers, such as superfine fibers, which include fibers
having diameters ranging from micron to nano in size (e.g.,
micrometer(s), nanometer(s)). The methods discussed herein employ
centrifugal forces to transform material into superfine fibers.
Apparatuses that may be used to create superfine fibers are also
described.
[0009] The methods discussed herein may be adapted to create, for
example, nanocomposites and functionally graded materials that can
be used for fields as diverse as, for example, drug delivery and
ultrafiltration (such as electrets). Metallic and ceramic
nanofibers, for example, may be manufactured by controlling various
parameters, such as material selection and temperature. At a
minimum, the methods and apparatuses discussed herein may find
application in any industry that utilizes micro- to nano-sized
fibers and/or micro- to nano-sized composites. Such industries
include, but are not limited to, the food, drug, materials,
mechanical, electrical, defense, and/or tissue engineering
industries.
[0010] Some embodiments of the present apparatuses may be used for
both melt and solution processes. Some embodiments of the present
apparatuses may be used for making both organic or inorganic fibers
as well. With appropriate manipulation of the environment and
process, it is possible with some embodiments of the present
apparatuses to form superfine fibers of various configurations,
such as continuous, discontinuous, mat, random fibers,
unidirectional fibers, woven and unwoven, as well as fiber shapes,
such as circular, elliptical and rectangular (e.g., ribbon). Other
shapes are also possible. The superfine fiber may be lumen or
multi-lumen.
[0011] By controlling the process parameters of some embodiments of
the present methods, fibers can be made in micron, sub-micron and
nano-sizes, and combinations thereof. In general, the superfine
fibers created will have a relatively narrow distribution of fiber
diameters. Some variation in diameter and cross-sectional
configuration may occur along the length of individual superfine
fibers and between superfine fibers.
[0012] Because of the variety of properties that may be imparted to
the superfine fibers created using some embodiments of the present
apparatuses, such apparatuses may be termed "multi-level variable
fiber spinners." More generally, the present invention concerns
multi-level superfine fiber creation, in certain embodiments.
[0013] Accordingly, one general aspect of the present methods
discussed herein includes a method of creating superfine fibers,
such as nanofibers, comprising: heating a material; placing the
material in a heated structure; and after the placing, rotating the
heated structure at a rate of at least 500 revolutions per minute
(RPM) to create the nanofibers from the material. In some
embodiments of the present methods, the superfine fibers may be
micron fibers, sub-micron fibers, or nanofibers. A "heated
structure" is defined as a structure that has a temperature that is
greater than the ambient temperature. "Heating a material" is
defined as raising the temperature of that material to a
temperature above ambient temperature. In alternate embodiments,
the structure is not heated. Indeed, for any embodiment that
employs a heated structure, a structure that is not heated may
alternatively be employed. In some embodiments, the material is not
heated. It is also to be understood that for any embodiments that
employs heating a material or a heated material, material that is
not heated may alternatively be employed. In some embodiments, the
structure is heated but the material is not heated. In some
embodiments, the structure is heated and the material is not
heated, such that the material becomes heated once placed in
contact with the heated structure. In some embodiments, the
material is heated and the structure is not heated, such that the
structure becomes heated once it comes into contact with the heated
material.
[0014] As noted, the heated structure may be rotated. The heated
structure may also be spun about a spin axis. The heated structure
may be rotated at, for example, 500-25,000 revolutions per minute
(RPM), in certain embodiments, or any range derivable therein. In
certain embodiments, the heated structure is rotated at no more
than 50,000, 45,000, 40,000, 35,000, 30,000, 25,000, 20,000,
15,000, 10,000, 5,000, or 1,000 RPM. In certain embodiments, the
heated structure is rotated at no more than 40,000 RPM. In certain
embodiments, the heated structure is rotated at a rate of
5,000-25,000 RPM.
[0015] A wide range of volumes/amounts of material may be used in
embodiments of the present methods. In addition, a wide range of
rotation times may also be employed. For example, in certain
embodiments, at least 5 milliliters (mL) of material are positioned
in a heated structure, and the heated structure is rotated for at
least 10 seconds. As discussed above, the rotation may be at a rate
of 500-25,000 RPM, for example. The amount of material may range
from mL to liters (L), or any range derivable therein. For example,
in certain embodiments, at least 50-100 mL of the material are
positioned in the heated structure, and the heated structure is
rotated at a rate of 500-25,000 RPM for 300-2,000 seconds. In
certain embodiments, at least 5-100 mL of the material are
positioned in the heated structure, and the heated structure is
rotated at a rate of 500-25,000 RPM for 10-500 seconds. In certain
embodiments, at least 100-1,000 mL of the material are positioned
in the heated structure, and the heated structure is rotated at a
rate of 500-25,000 RPM for 100-5,000 seconds. Other combinations of
amounts of material, RPMs and seconds are contemplated as well.
[0016] In certain embodiments, the heated structure includes at
least one opening and the material is extruded through the opening
to create the nanofibers. In certain embodiments, the heated
structure includes multiple openings and the material is extruded
through the multiple openings to create the nanofibers. These
openings may be of a variety of shapes (e.g., circular, elliptical,
rectangular, square) and of a variety of diameter sizes (e.g.,
0.01-0.80 mm). When multiple openings are employed, not every
opening need be identical to another opening, but in certain
embodiments, every opening is of the same configuration.
[0017] The material may, in certain embodiments, be positioned in a
reservoir of the heated structure. The reservoir may, for example,
be defined by a concave cavity of the heated structure. In certain
embodiments, the heated structure includes at least one opening in
communication with the concave cavity, the nanofiber is extruded
through the opening, the heated structure is rotated about a spin
axis, and the opening has an opening axis that is not parallel with
the spin axis. The heated structure may include multiple openings
in communication with the concave cavity. These openings are
similar to those openings described above. Furthermore, the heated
structure may include a body that includes the concave cavity and a
lid positioned above the body such that a gap exists between the
lid and the body, and the nanofiber is created as a result of the
rotated material exiting the concave cavity through the gap.
[0018] In particular embodiments, the heated structure is thermally
coupled to a heat source that can be used to adjust the temperature
of the heated structure before operation (e.g., before rotating).
Heat sources that may be employed are described below. A wide
variety of temperatures may be achieved, and in certain
embodiments, the heated structure is heated to a temperature less
than 1500.degree. C. before operation. The heated structure may be
heated to temperatures greater than 1500.degree. C. before
operation as well, such as to 2500.degree. C. In certain
embodiments, the heated structure is heated to a temperature less
than 400.degree. C. before operation. In certain embodiments, the
heated structure is heated to a temperature that ranges between one
degree Celsius above ambient temperature and 400.degree. C. before
operation. In particular embodiments, the heated structure is
thermally coupled to a heat source and/or a cooling source that can
be used to adjust the temperature of the heated structure before
operation, a cooling source that can be used to adjust the
temperature of the heated structure before operation, or both a
heat source that can be used to adjust the temperature of the
heated structure during the spinning and a cooling source that can
be used to adjust the temperature of the heated structure before
operation. Cooling sources are described below.
[0019] In any method described herein, the method may comprise
adjusting the temperature of the heated structure during operation
(e.g., during rotating). In certain embodiments, the heated
structure is maintained at a temperature of not more than
1500.degree. C. during operation. The heated structure may be
maintained at temperatures higher than 1500.degree. C. during
operation as well, such as 2500.degree. C. In certain embodiments,
the heated structure is adjusted to a temperature of not more than
400.degree. C. during operation. In certain embodiments, the heated
structure is heated to a temperature that ranges between one degree
Celsius above ambient temperature and 400.degree. C. during
operation. In particular embodiments, the heated structure is
thermally coupled to a heat source and/or a cooling source that can
be used to adjust the temperature of the heated structure during
operation, a cooling source that can be used to adjust the
temperature of the heated structure during operation, or both a
heat source that can be used to adjust the temperature of the
heated structure during operation and a cooling source that can be
used to adjust the temperature of the heated structure during
operation. The heated structure may be cooled to temperatures as
low as, for example, -20.degree. C. An exemplary range of
temperatures for any heated structure described herein is
-20.degree. C. to 2500.degree. C.
[0020] The heated structure may take on a variety of
configurations. For example, the heated structure may comprise a
syringe and a plunger. Any syringe equipped with a plunger as known
to those of skill in the art may be used. The material may be
placed in the syringe. Moreover, instead of a plunger, another
object may be used that prevents unwanted leakage of the material
from the syringe. In certain embodiments, the syringe further
comprises a needle that is attached to the syringe. The gauge (G)
of the needle may range from, for example, 16 G (1.194 mm) to 25 G
(0.241 mm). In certain embodiments, the syringe and plunger are
rotated at a rate of 500-25,000 RPM, or any range derivable
therein. In certain embodiments, at least 10-500 mL of the material
are positioned in the syringe, and the syringe and plunger are
rotated at a rate of 500-25,000 RPM for 10-1,000 seconds. In
particular embodiments, a syringe support device supports the
syringe. The syringe support device may, for example, comprise an
elongated structure with open ends and an open top.
[0021] Any method described herein may further comprise collecting
at least some of the nanofibers that are created. As used herein
"collecting" of superfine fibers, such as nanofibers, refers to
superfine fibers coming to rest against a superfine fiber
collection device, as described herein, as well as removal of
superfine fibers, such as from a superfine fiber collection device,
such as removal by a human or robot. A variety of methods and
superfine fiber (e.g., nanofiber) collection devices may be used to
collect superfine fibers. For example, regarding nanofibers, a
collection wall may be employed that collects at least some of the
nanofibers. In certain embodiments, a collection rod collects at
least some of the nanofibers. The collection rod may be stationary
during collection, or the collection rod may be rotated during
collection. For example, the collection rod may be rotated at
50-250 RPM, in certain embodiments. In certain embodiments, an
elongated structure with open ends and an open top collects at
least some of the nanofibers. As noted above, a syringe support
device may comprise an elongated structure with open ends and an
open top. In certain embodiments, a syringe support device also
collects superfine fibers, such as nanofibers.
[0022] Regarding the nanofibers that are collected, in certain
embodiments, at least some of the nanofibers that are collected are
in a configuration selected from the group consisting of
continuous, discontinuous, mat, woven and unwoven. In particular
embodiments, the nanofibers are not bundled into a cone shape after
their creation. In particular embodiments, the nanofibers are not
bundled into a cone shape during their creation. In particular
embodiments, nanofibers are not shaped into a particular
configuration, such as a cone figuration, using air, such as
ambient air, that is blown onto the nanofibers as they are created
and/or after they are created.
[0023] Present methods may further comprise, for example,
introducing a gas through an inlet in a housing, where the housing
surrounds at least the heated structure. The gas may be, for
example, nitrogen, helium, argon, or oxygen. A mixture of gases may
be employed, in certain embodiments.
[0024] The environment in which the nanofibers are created may
comprise a variety of conditions. For example, any nanofiber
discussed herein may be created in a sterile environment. As used
herein, the term "sterile environment" refers to an environment
where greater than 99% of living germs and/or microorganisms have
been removed. In certain embodiments, "sterile environment" refers
to an environment substantially free of living germs and/or
microorganisms. The nanofiber may be created, for example, in a
low-pressure environment, such as an environment of 1-760
millimeters (mm) of mercury (Hg) of pressure, or any range
derivable therein. In certain embodiments, the nanofiber is created
in a high-pressure environment, such as an environment of 761 mm Hg
to 4 atmospheres (atm) of pressure, or any range derivable therein.
Higher pressures are also possible. In certain embodiments, the
nanofiber is created in an environment of 0-100% humidity, or any
range derivable therein. The temperature of the environment in
which the nanofiber is created may vary widely. In certain
embodiments, the temperature of the environment in which the
nanofiber is created can be adjusted before operation (e.g., before
rotating) using a heat source, a cooling source, or both a heating
source and a cooling source. Moreover, the temperature of the
environment in which the nanofiber is created can be adjusted
during operation using a heat source, a cooling source, or both a
heating source and a cooling source. The temperature of the
environment may be as low as sub-freezing, such as -20.degree. C.,
or lower. The temperature of the environment may be as high as, for
example, 1500.degree. C. Higher temperatures are also employed, in
certain embodiments.
[0025] The material employed in the present methods may comprise
one or more ingredients and may be of a single phase (e.g., solid)
or a mixture of phases (e.g., solid particles in a liquid), before
or after the material is heated. The material may be a fluid. In
certain embodiments, the material comprises a solid before it is
heated. In certain embodiments, the material comprises a liquid
before it is heated. The material may comprise a solvent (e.g.,
water, de-ionized water, dimethylsulfoxide), a solute (e.g.,
polymer pellets, drugs, other chemicals), an additive (e.g.,
thinner, surfactant, plasticizer), or any combination thereof. The
material may comprise a liquid after it is heated. The material may
comprise at least one polymer. The polymer may comprise, for
example, polypropylene, polystyrene, acrylonitrile butadiene
styrene, nylon, polycarbonate, or any combination thereof. The
polymer may be a synthetic (man-made) polymer or a natural polymer.
The material may comprise, for example, at least one metal. Metals
employed in fiber creation are well-known to those of skill in the
art. In certain embodiments, the metal may be selected from the
group consisting of bismuth, tin, zinc, silver, gold, nickel and
aluminum. The material may comprise, for example, at least one
ceramic, such as alumina, titania, silica, or zirconia, or
combinations thereof. The material may comprise a composite, for
example, such as bronze, brass, or a drug combined with a carrier
polymer (e.g., agarose).
[0026] The nanofiber that is created may be, for example, one
micron or longer in length. For example, created nanofibers may be
of lengths that range from 1-9 micrometers to 1-9 millimeters to
1-9 centimeters, or longer. When continuous methods are performed,
nanofibers of up to and over 1 meter in length may be made. In
certain embodiments, the cross-section of the nanofiber is a shape
selected from the group consisting of circular, elliptical and
rectangular. Other shapes are also possible. The nanofiber may be
lumen or multi-lumen. As with the materials described above, the
nanofiber may comprise at least one polymer. The polymer may
comprise, for example, polypropylene, polystyrene, acrylonitrile
butadiene styrene, nylon, beta-lactam, agarose, albumin, or
polycarbonate, or any combination thereof. The nanofiber may
comprise at least one metal. Metals employed in fibers are
well-known to those of skill in the art. The metal may, for
example, be selected from the group consisting of bismuth, tin,
zinc, silver, gold, nickel and aluminum. The nanofiber may, for
example, comprise at least one ceramic, for example. The ceramic
may be alumina, titania, silica, or zirconia, or combinations
thereof, for example. The nanofiber may comprise at least one
composite. The composite may be bronze, brass, or a drug combined
with a carrier polymer (e.g., agarose), for example. The composite
may be a carbon nanotube reinforced polymer composite. In
particular embodiments, the nanofiber comprises at least two of the
following: a polymer, a metal, a ceramic, a drug, and/or a
composite.
[0027] The nanofiber created by the methods described herein may be
a beta-lactam nanofiber. The nanofiber may be a polypropylene
nanofiber. The nanofiber may be acrylonitrile butadiene styrene
nanofiber.
[0028] In particular embodiments, the heated structure employed in
the methods and apparatuses described herein is further defined as
a spinneret. Alternatively, a cooled structure may be further
defined as a spinneret. As used herein, a spinneret is (a) an
object that may hold the material described herein and that may be
spun (e.g., at 500-25,000 RPM), where the material may exit the
spinneret via at least one pathway, or (b) a collection of objects,
where at least one of the collection of objects may hold the
material described herein, where the collection of objects may be
spun together (e.g., at 500-25,000 RPM) and the material may exit
the spinneret via at least one pathway.
[0029] Another general aspect of the present methods discussed
herein includes a method of creating superfine fibers, such as
nanofibers, comprising: heating a material; placing the material in
a cooled structure; and after the placing, rotating the cooled
structure at a rate of at least 500 revolutions per minute (RPM) to
create the nanofibers from the material. The material need not be
heated prior to its placement in the cooled structure, in some
embodiments. Thus, the material may be at an ambient temperature,
or may be cooled (that is, an embodiment may comprise "cooling a
material"). A "cooled structure" is defined as a structure that has
a temperature that is less than the ambient temperature. "Cooling a
material" is defined as lowering the temperature of that material
to a temperature below ambient temperature. It is also to be
understood that for any embodiments that employs cooling a material
or a cooled material, material that is not cooled may alternatively
be employed. In some embodiments, the structure is cooled but the
material is not cooled. In some embodiments, the structure is
cooled and the material is not cooled, such that the material
becomes cooled once placed in contact with the cooled structure. In
some embodiments, the material is cooled and the structure is not
cooled, such that the structure becomes cooled once it comes into
contact with the cooled material. For any embodiment described
herein employing a heated structure, a cooled structure may
alternatively be employed, in some embodiments. A cooled structure
and/or a cooled material may be cooled to as low as, for example,
-20.degree. C., in some embodiments.
[0030] Another general aspect of the present methods discussed
herein includes a method of creating a superfine fiber, comprising:
spinning material to create the superfine fiber; where, as the
superfine fiber is being created, the superfine fiber is not
subjected to an externally-applied electric field or an
externally-applied gas; and the superfine fiber does not fall into
a liquid after being created. As used herein, a "superfine fiber"
is a fiber whose diameter ranges from micron (typically single
digit) to sub-micron (e.g., between micron and nanometer, such as
700 to 900 nanometers) to nano (typically 100 nanometers or less).
In such methods, the material may be spun at, for example,
500-25,000 RPM, or any range derivable therein. In certain
embodiments, the material is spun at no more than 50,000, 45,000,
40,000, 35,000, 30,000, 25,000, 20,000, 15,000, 10,000, 5,000, or
1,000 RPM. In certain embodiments, the material is spun at no more
than 40,000 RPM. In certain embodiments, the material is spun at a
rate of 5,000-25,000 RPM.
[0031] In particular embodiments, a superfine fiber of the present
fibers is not a lyocell fiber. Lyocell fibers are described in the
literature, such as in U.S. Pat. Nos. 6,221,487, 6,235,392,
6,511,930, 6,596,033 and 7,067,444, each of which is incorporated
herein by reference.
[0032] In certain methods of creating a superfine fiber as
described herein, the spinning may comprise spinning material to
form multiple superfine fibers, and where: none of the superfine
fibers that are created is subjected to an externally-applied
electric field or an externally-applied gas during the creation,
and none of the superfine fibers falls into a liquid after being
created. In certain embodiments, the material is spun at no more
than 50,000, 45,000, 40,000, 35,000, 30,000, 25,000, 20,000,
15,000, 10,000, 5,000, or 1,000 RPM. In certain embodiments, the
material is spun at no more than 40,000 RPM. The material may be
spun, for example, at a rate of 5,000-25,000 RPM.
[0033] In certain methods of creating a superfine fiber, at least 5
mL of the material may be spun at a rate of 500-25,000 RPM for at
least 10 seconds. Indeed, a wide range of volumes/amounts of
material may be used in the methods of creating a superfine fiber,
as discussed herein. The amount of material may range from mL to
liters, or any range derivable therein. A wide range of
volumes/amounts of material may be used in the methods discussed
herein. For example, in certain embodiments, at least 50-100 mL of
the material are spun at a rate of 500-25,000 RPM for 300-2,000
seconds. In certain embodiments, at least 5-100 mL of the material
are spun at a rate of 500-25,000 RPM for 10-500 seconds. In certain
embodiments, at least 100-1,000 mL of the material are spun at a
rate of 500-25,000 RPM for 100-5,000 seconds. Other combinations of
amounts of material, RPMs and seconds are contemplated as well.
[0034] In certain methods of creating a superfine fiber as
described herein, the material is housed in a spinneret, and the
spinneret is spun during the spinning. The spinneret may, for
example, include at least one opening and the material is extruded
through the opening to create at least some of the superfine
fibers. In certain embodiments, the spinneret includes multiple
openings and the material is extruded through the multiple openings
to create at least some of the superfine fibers. The openings in
the spinneret may have the same properties as the openings
described above and throughout this application.
[0035] In certain methods that employ a spinneret, at least 50-100
mL of the material are spun at a rate of 500-25,000 RPM for
300-2,000 seconds. In certain embodiments, at least 5-100 mL of the
material are spun at a rate of 500-25,000 RPM for 10-500 seconds.
Indeed, a variety of amounts of material, RPMs and seconds may be
employed in these methods, similar to the methods described
above.
[0036] In certain embodiments, the material is positioned in a
reservoir of the spinneret. In such methods, at least 100-1,000 mL
of the material are spun at a rate of 500-25,000 RPM for 100-5,000
seconds, in certain embodiments. Ranges of volumes of material are
not limited to this range, but may be less than 100 mL and may be
greater than one liter. Varying rotation speeds are also
contemplated, as are lengths of time the material is rotated. In
certain embodiments, the reservoir is defined by a concave cavity
of the spinneret. In particular embodiments, the spinneret includes
at least one opening in communication with the concave cavity, the
superfine fiber is extruded through the opening, the spinneret is
spun about a spin axis, and the opening has an opening axis that is
not parallel with the spin axis. With respect to such an
embodiment, the spinneret may further include multiple openings in
communication with the concave cavity. The spinneret may include a
body that includes the concave cavity and a lid positioned above
the body such that a gap exists between the lid and the body, and
the superfine fiber is created as a result of the spun material
exiting the concave cavity through the gap.
[0037] In certain embodiments, a spinneret of the present
spinnerets may comprise a syringe and a plunger. Any syringe
equipped with a plunger as known to those of skill in the art may
be used. The material may be placed in the syringe. The syringe and
the plunger may be spun at a rate of 500-25,000 RPM, or any range
derivable therein. Moreover, instead of a plunger, another object
may be used that prevents unwanted leakage of the material from the
syringe. In certain embodiments, the syringe further comprises a
needle that is attached to the syringe. The gauge of the needle may
range from, for example, 16 G (1.194 mm) to 25 G (0.241 mm). In
certain embodiments, at least 10-500 mLs of the material are
positioned in the syringe, and the syringe and plunger are rotated
at a rate of 500-25,000 RPM for 10-1,000 seconds. In particular
embodiments, a syringe support device supports the syringe. The
syringe support device may, for example, comprise an elongated
structure with open ends and an open top.
[0038] In certain methods that employ a spinneret, such methods may
comprise adjusting the temperature of the spinneret before the
spinning. For example, the spinneret may be adjusted to a
temperature of between -20.degree. C. and 1500.degree. C. before
the spinning. Temperatures below -20.degree. C. and above
1500.degree. C. are also contemplated, such as 2500.degree. C. In
certain embodiments, the spinneret is adjusted to a temperature of
between 4.degree. C. and 400.degree. C. before the spinning. In
certain embodiments, the spinneret is thermally coupled to a heat
source and/or a cooling source that can be used to adjust the
temperature of the spinneret before the spinning, a cooling source
that can be used to adjust the temperature of the spinneret before
the spinning, or both a heat source that can be used to adjust the
temperature of the spinneret before the spinning and a cooling
source that can be used to adjust the temperature of the spinneret
before the spinning. Heating and cooling sources are described
herein. In certain embodiments, the temperature of the spinneret
may be adjusted during the spinning. During spinning, the spinneret
may be maintained, for example, at a temperature of between
-20.degree. C. and 1500.degree. C., such as between 4.degree. C.
and 400.degree. C. The temperature may be maintained below
-20.degree. C. or above 1500.degree. C. as well, such as
2500.degree. C. In certain embodiments, the spinneret is thermally
coupled to a heat source that can be used to adjust the temperature
of the spinneret during the spinning, a cooling source that can be
used to adjust the temperature of the spinneret during the
spinning, or both a heat source that can be used to adjust the
temperature of the spinneret during the spinning and a cooling
source that can be used to adjust the temperature of the spinneret
during the spinning.
[0039] In embodiments that employ a spinneret, such embodiments may
also comprise introducing a gas through an inlet in a housing,
where the housing surrounds at least the spinneret. The gas may be,
for example, nitrogen, helium, argon, or oxygen. A mixture of gases
may be employed, in certain embodiments.
[0040] Certain methods contemplate collecting at least some of the
superfine fibers that are created. A variety of methods and
equipment pieces may be used to collect superfine fibers. For
example, a collection wall may be employed that collects at least
some of the superfine fibers. In certain embodiments, a collection
rod collects at least some of the superfine fibers. The collection
rod may be stationary during collection, or the collection rod may
be rotated during collection. For example, the collection rod may
be rotated at 50-250 RPM, in certain embodiments. In certain
embodiments, an elongated structure with open ends and an open top
collects at least some of the superfine fibers.
[0041] Regarding the superfine fibers that are collected, in
certain embodiments, at least some of the superfine fibers that are
collected are in a configuration selected from the group consisting
of continuous, discontinuous, mat, woven and unwoven. In particular
embodiments, the superfine fibers are not bundled into a cone shape
during their creation. In particular embodiments, the superfine
fibers are not bundled into a cone shape after their creation. In
particular embodiments, superfine fibers are not shaped into a
particular configuration, such as a cone figuration, using air,
such as ambient air, that is blown onto the superfine fibers as
they are created and/or after they are created.
[0042] The environment in which the superfine fibers are created
may comprise a variety of conditions. For example, any superfine
fiber discussed herein may be created in a sterile environment. The
superfine fiber may be created, for example, in a low-pressure
environment, such as an environment of 1-760 millimeters (mm) of
mercury (Hg) of pressure, or any range derivable therein. In
certain embodiments, the superfine fiber is created in a
high-pressure environment, such as an environment of 761 mm Hg to 4
atmospheres (atm) of pressure, or any range derivable therein.
Higher pressures are also possible. In certain embodiments, the
superfine fiber is created in an environment of 0-100% humidity, or
any range derivable therein. The temperature of the environment in
which the superfine fibers are created may vary widely. In certain
embodiments, the temperature of the environment in which the
superfine fiber is created can be adjusted before the spinning
using a heat source, a cooling source, or both a heating source and
a cooling source. Moreover, the temperature of the environment in
which the superfine fiber is created can be adjusted during the
spinning using a heat source, a cooling source, or both a heating
source and a cooling source. The temperature of the environment may
be as low as sub-freezing, such as -20.degree. C., or lower. The
temperature of the environment may, for example, be as high as
1500.degree. C., or higher, such as 2500.degree. C. Higher
temperatures are also contemplated. The temperature of the
environment in which the superfine fiber is created can be adjusted
before the spinning using a heat source, a cooling source, or both
a heating source and a cooling source. Moreover, the temperature of
the environment in which the superfine fiber is created can be
adjusted during the spinning using a heat source, a cooling source,
or both a heating source and a cooling source.
[0043] In methods involving creating, or creation of, superfine
fibers, the material may comprise one or more ingredients and may
be of a single phase (e.g., solid) or a mixture of phases (e.g.,
solid particles in a liquid), before or after the material is
heated. In certain embodiments, the material comprises a solid
before it is heated. In certain embodiments, the material comprises
a liquid before it is heated. The liquid may comprise a solvent, a
solute, an additive, or any combination thereof. The material may
comprise a liquid after it is heated. The material may comprise at
least one polymer. The polymer may comprise, for example,
polypropylene, polystyrene, acrylonitrile butadiene styrene, nylon,
polycarbonate, or any combination thereof. The polymer may be a
synthetic (man-made) polymer or a natural polymer. The material may
comprise, for example, at least one metal. The metal may be
selected from the group consisting of bismuth, tin, zinc, silver,
gold, nickel and aluminum. The material may comprise, for example,
at least one ceramic. For example, the ceramic may be alumina,
titania, silica, or zirconia, or combinations thereof. The material
may comprise a composite, for example. For example, the composite
may be bronze, brass, or a drug combined with a carrier polymer
(e.g., agarose). The composite may be a carbon nanotube reinforced
polymer composite.
[0044] The superfine fiber that is created may be, for example, one
micron or longer in length. For example, created superfine fibers
may be of lengths that range from 1-9 microns to 1-9 millimeters,
or longer. When continuous methods are performed, superfine fibers
of up to and over 1 meter in length may be made. In certain
embodiments, the cross-section of the superfine fiber is a shape
selected from the group consisting of circular, elliptical and
rectangular. Other shapes are also possible. The superfine fiber
may be lumen or multi-lumen. As with the materials described above,
the superfine fiber may comprise at least one polymer. The polymer
may comprise, for example, polypropylene, polystyrene,
acrylonitrile butadiene styrene, nylon, beta-lactam, agarose,
albumin, or polycarbonate, or any combination thereof. The
superfine fiber may comprise at least one metal. The metal may, for
example, be selected from the group consisting of bismuth, tin,
zinc, silver, gold, nickel and aluminum. The superfine fiber may,
for example, comprise at least one ceramic, for example. The
ceramic may be alumina, titania, silica, or zirconia, or
combinations thereof, for example. The nanofiber may comprise at
least one composite. The composite may be a carbon nanotube
reinforced polymer composite, for example. In particular
embodiments, the superfine fiber comprises at least two of the
following: a polymer, a metal, a ceramic, a drug, and/or a
composite.
[0045] The superfine fiber created by the methods described herein
may be a microfiber. Such microfibers may, for example, comprise
beta-lactam, agarose, or albumin. In certain embodiments, the
superfine fiber is a sub-micron fiber. The superfine fiber may be,
for example, a nanofiber. The superfine fiber may be less than 300
nanometers in diameter, in some embodiments. The superfine fiber
may be less than 100 nanometers in diameter, in some embodiments.
The superfine fiber may be greater than 500 nanometers but less
than ten microns in diameter, in certain embodiments. The superfine
fiber may, for example, a beta-lactam nanofiber or a polypropylene
nanofiber.
[0046] Other general aspects of the present methods contemplate a
method of creating a superfine fiber, comprising: spinning material
at a rate of 500-25,000 RPM to create the superfine fiber. For
example, the rate the material is spun may be 5,000-25,000 RPM. The
material may be heated before spinning. The superfine fiber may be
a nanofiber, in certain embodiments.
[0047] Another general aspect of the present methods contemplates a
method of creating a superfine fiber comprising: creating a
superfine fiber that is one micron or longer. The superfine fiber
may be a nanofiber, in certain embodiments.
[0048] A method of creating a superfine fiber comprising: creating
the fiber in an environment of 761 mm Hg to 4 atm of pressure, is
also contemplated. The superfine fiber may, in certain embodiments,
be a nanofiber.
[0049] Furthermore, another general aspect of the present methods
contemplates a method of creating a superfine fiber comprising:
creating the fiber in an environment of 0-100% humidity. The
superfine fiber may be a nanofiber, in certain embodiments.
[0050] Some of the present apparatuses take the form of a spinneret
comprising: a plate having: a centrally-oriented reservoir; a fluid
exit pathway in fluid communication with the reservoir; and a fluid
exit opening in fluid communication with the fluid exit pathway;
and a cover coupled to the plate; where the spinneret is configured
such that, during operation, material in the reservoir flows
through the fluid exit pathway and out of the spinneret through the
fluid exit opening to create a superfine fiber. The plate may have,
for example, multiple fluid exit pathways, each in fluid
communication with the reservoir; and one fluid exit opening in
fluid communication with each respective fluid exit pathway; and
where the spinneret is configured such that, during operation,
material in the reservoir flows through the fluid exit pathways and
out of the fluid exit openings to create superfine fibers. The
cover may, for example, include a fluid injection inlet through
which fluid can be injected to reach the centrally-oriented
reservoir. The cover may comprise a plate, and both plates of this
spinneret may have substantially similar outer profiles. Moreover,
such a spinneret may further comprise a holding plate to which both
the plate and the cover are coupled in a stacked relationship. The
spinneret may comprise, for example, metal, plastic, or both. The
spinneret may be configured to withstand temperatures ranging from
-20.degree. C. to 2500.degree. C., for example.
[0051] Other embodiments of the present spinnerets contemplate a
spinneret comprising: a syringe having a plunger; and a syringe
support device that includes a syringe support cavity in which at
least a portion of the syringe will be positioned when the
spinneret is operated, the spinneret being configured to rotate
about a spin axis. The spinneret may comprise, for example, metal,
plastic, or both. The spinneret may be configured to withstand
temperatures ranging from -20.degree. C. to 2500.degree. C., for
example.
[0052] Yet another embodiment of the present spinnerets
contemplates a spinneret comprising: a body having a concave cavity
configured to receive a molten material, the body including one or
more openings in communication with the concave cavity; where the
body is configured to rotate about a spin axis, each opening
includes an opening axis extending through and centered in that
opening, and each opening axis is oriented at an angle ranging from
.+-.15 degrees to the spin axis. In certain embodiments, a lid may
be configured to be positioned over the concave opening. Such a lid
may be configured to cover and enclose the concave cavity. The
concave body may be configured to receive, for example, at least
100-1,000 mL of material. This range is not restrictive, however:
the concave body may be configured to receive less than 100 mL or
greater than 1,000 mL, if desired. The spin axis may be centered
within the concave cavity, in certain embodiments. The spinneret
may comprise metal, or plastic, or both. The spinneret may be
configured to withstand temperatures ranging from -20.degree. C. to
2500.degree. C., for example.
[0053] A further embodiment of the present spinnerets contemplates
a spinneret comprising: a body having a concave cavity configured
to receive a molten material; and a lid positioned above the body
such that a gap exists between the lid and the body. The body and
the lid may be configured to spin about a spin axis that is
centered within the concave cavity. The concave body may be
configured to receive, for example, at least 100-1,000 mL of
material. This range is not restrictive, however: the concave body
may be configured to receive less than 100 mL or greater than 1,000
mL, if desired. The spinneret may comprise metal, or plastic, or
both. The spinneret may be configured to withstand temperatures
ranging from -20.degree. C. to 2500.degree. C., for example.
[0054] Yet another embodiment of the present spinnerets
contemplates a spinneret comprising a bottom plate; a top plate;
and a micro-mesh material separating the bottom plate from the top
plate, the spinneret being configured to rotate about a spin axis.
The micro-mesh material may be, for example, stainless steel or
plastic. The pore size of the micro-mesh material may range
between, for example, 0.01 mm to 3.0 mm (e.g., 0.01, 0.05, 0.10,
0.20, 0.30, 0.40, 0.50, 0.75, 0.10, 0.20, 0.30, 0.40, 0.50, 0.75,
1.0, 1.5, 2.0, 2.5 or 3.0 mm or higher, or any range derivable
therein). The pore sizes may be uniform throughout the mesh or may
vary. The distance spanned by the micro-mesh material between the
bottom plate and the top plate may range between 1-10'', in certain
embodiments. Both plates may, in certain embodiments, comprise
substantially similar outer profiles. The spinneret may be
configured to withstand temperatures ranging from -20.degree. C. to
2500.degree. C., for example.
[0055] When referring to "substantially similar" in the context of
plates of spinnerets of the present spinnerets, it is meant that
one plate's diameter is within 10% of the diameter of another.
[0056] The present invention also concerns apparatuses. For
example, certain embodiments of the present apparatuses contemplate
an apparatus for creating superfine fibers, comprising: a driver
configured to be rotated at 500 RPM or more, a spinneret coupled to
the driver; and a superfine fiber collection device; where the
apparatus is configured to create superfine fibers by rotating the
spinneret with the driver, and without subjecting the superfine
fibers, during their creation, to either an externally-applied
electric field or an externally-applied gas, and without the
superfine fibers falling into liquid after being created. The
superfine fiber, for example, may be a microfiber or a sub-micron
fiber. The superfine fiber, for example, may be less than 300
nanometers in diameter, in certain embodiments. The superfine fiber
may be a nanofiber, for example. The driver may be configured to be
rotated at 500-25,000 RPM, such as 5,000-25,000 RPM. The driver may
be configured to be rotated at less than 40,000 RPM, for example.
The spinneret of the apparatus, in certain embodiments, comprises a
concave cavity. The spinneret may further comprise a lid. The
spinneret may further comprise at least one plate. For example, the
spinneret may comprise at least three plates. The spinneret may
comprise a syringe. Indeed, the spinneret may be any spinneret as
described herein.
[0057] Apparatuses may comprise a collection device to collect the
superfine (e.g., micron, sub-micron, or nano) fibers. For example,
a superfine fiber collection device employed to collect such fibers
may be a collection wall. The collection wall may, for example, at
least partially surround the spinneret. The collection wall may
completely surround the spinneret. The superfine fiber collection
device may be a collection rod. The collection rod may be
configured to be rotated during operation. The superfine fiber
collection device may be an elongated structure with open ends and
an open top. The superfine fiber collection device may also be a
syringe support device.
[0058] Other features of an apparatus as described herein include,
for example, a driver that comprises a motor. An apparatus may also
comprise a heater thermally coupled to the spinneret. The heater
may be, for example, an inductive heater, a resistance heater, an
infrared heater, or a thermoelectric cooler. Other heaters are also
contemplated. The apparatus may further comprise a cooler thermally
coupled to the spinneret. The cooler may be, for example, a
thermoelectric cooler. Other coolers are also contemplated. An
apparatus may comprise an intermediate wall surrounding the
superfine fiber collection device. Such an apparatus may further
comprise, for example, a housing surrounding at least the
spinneret, the superfine fiber collection device, and the
intermediate wall, the housing including an inlet for the
introduction of a gas. The housing may be insulated. One or more
components of any apparatus described herein may be made of metal,
plastic, stainless steel, or any combination thereof.
[0059] Any apparatus or component thereof as described herein
(e.g., a spinneret) may be configured to operate in a continuous
manner. Moreover, any method described herein may comprise
continuous creation of superfine fibers. The term "continuous"
refers to the uninterrupted operation of an apparatus or component
thereof for at least 10, 15, 20, 25, 30, 35, 40, 45, 50, 55, 60
seconds or longer, or 5, 10, 20, 30, 60, 90, 120, 180, 240, 480
minutes or longer, or 0.5, 1, 2, 3, 4, 5, 6, 7, 8, 9, 10 or more
days, or any range derivable therein, or the uninterrupted creation
of superfine fibers for at least 10, 15, 20, 25, 30, 35, 40, 45,
50, 55, 60 seconds or longer, or 5, 10, 20, 30, 60, 90, 120, 180,
240, 480 minutes or longer, or 0.5, 1, 2, 3, 4, 5, 6, 7, 8, 9, 10
or more days, or any range derivable therein. Regarding "continuous
creation of superfine fibers", this phrase is not restricted to the
continuous creation of a single superfine fiber: "continuous
creation of superfine fibers" also refers to the continuous
creation of multiple superfine fibers over time, where new
superfine fibers are continuously being created over time. In
continuous operation, material may be added to a spinneret
continuously, or added in batches. For any embodiment which recites
a particular operation for a time range (e.g., "spinning a
spinneret for 100-5,000 seconds", or "rotating a heated structure
for 10-100 seconds", and the like), it is implied that operation
for that time period is continuous, unless otherwise noted.
[0060] Any apparatus described herein may be configured to be
operated under sterile conditions. As used herein, the term "under
sterile conditions" refers to conditions where greater than 99% of
living germs and/or microorganisms have been removed, such as from
the components of the apparatus and the environment of the interior
of the apparatus. In certain embodiments, "sterile conditions"
refers to conditions substantially free of living germs and/or
microorganisms.
[0061] Any apparatus described herein may be configured to be
operated under pressures of 1-760 millimeters (mm) of mercury (Hg).
Any apparatus described herein may be configured to be operated
under pressures of 761 mm Hg to 4 atmospheres (atm).
[0062] Also contemplated by the present invention are superfine
fibers, such as a superfine fiber made using a method described
herein. Such a superfine fiber may be a micron-sized fiber, a
sub-micron sized fiber, or a nanofiber. Superfine fibers made using
the apparatuses described herein are also contemplated. Such a
superfine fiber may be a micron-sized fiber, a sub-micron sized
fiber, or a nanofiber.
[0063] Particular superfine fibers are also contemplated.
Non-limiting examples of such superfine fibers include: a
beta-lactam nanofiber, a polypropylene nanofiber, and an
acrylonitrile butadiene styrene nanofiber.
[0064] In some embodiments, the superfine fibers created by the
methods and devices described herein have a diameter of at least
one of (and/or one selected from the group consisting of): 1-100
nanometers, 1-500 nanometers, 100-500 nanometers, 1-10 microns,
1-100 microns (micrometers), 1 nanometer-100 microns, and 1
nanometer-200 microns.
[0065] It is specifically contemplated that any limitation
discussed with respect to one embodiment of the invention may apply
to any other embodiment of the invention. Furthermore, any
composition of the invention may be used in any method of the
invention, and any method of the invention may be used to produce
or to utilize any composition of the invention.
[0066] The use of the term "or" in the claims is used to mean
"and/or" unless explicitly indicated to refer to alternatives only
or the alternative are mutually exclusive, although the disclosure
supports a definition that refers to only alternatives and
"and/or."
[0067] As used herein the specification, "a" or "an" may mean one
or more, unless clearly indicated otherwise. As used herein in the
claim(s), when used in conjunction with the word "comprising," the
words "a" or "an" may mean one or more than one. As used herein
"another" may mean at least a second or more.
[0068] Any embodiment of any of the present methods and apparatus
may consist of or consist essentially of--rather than
comprise/include/contain/have--the described steps, elements and/or
features. Thus, in any of the claims, the term "consisting of" or
"consisting essentially of" may be substituted for any of the
open-ended linking verbs recited above, in order to change the
scope of a given claim from what it would otherwise be using the
open-ended linking verb.
BRIEF DESCRIPTION OF THE FIGURES
[0069] The following figures illustrate by way of example and not
limitation. Identical reference numerals do not necessarily
indicate an identical structure. Rather, the same reference numeral
may be used to indicate a similar feature or a feature with similar
functionality. Not every feature of each embodiment is labeled in
every figure in which that embodiment appears, in order to keep the
figures clear.
[0070] FIG. 1 depicts an embodiment of the present spinnerets that
includes a single plate with multiple peripheral openings.
[0071] FIG. 2 depicts an embodiment of the present spinnerets that
includes three plates with multiple peripheral openings.
[0072] FIG. 3 depicts an embodiment of the present spinnerets that
includes a syringe, plunger and various needles as well as a
syringe support device.
[0073] FIG. 4 depicts an embodiment of the present spinnerets that
includes a syringe secured to a syringe support device, where the
syringe is equipped with a needle and a plunger.
[0074] FIG. 5 depicts an embodiment of the present syringe support
devices. This syringe support device may also be a superfine fiber
collection device.
[0075] FIG. 6 depicts an embodiment of the present spinnerets that
includes a syringe secured to a syringe support device, where the
syringe is equipped with a needle and a plunger.
[0076] FIG. 7 depicts an embodiment of the present syringe support
devices. This syringe support device may also be a superfine fiber
collection device.
[0077] FIG. 8 depicts an embodiment of the present spinnerets that
includes a reservoir that is a concave cavity.
[0078] FIG. 9 depicts an embodiment of the present spinnerets that
includes a top plate and a bottom plate, where the top and bottom
plates are separated by a micro-mesh material.
[0079] FIG. 10 depicts an embodiment of the present superfine fiber
collection devices.
[0080] FIG. 11 depicts an embodiment of the present superfine fiber
collection devices.
[0081] FIG. 12 depicts an embodiment of the present spinnerets (see
FIG. 1) depicted in motion where superfine fibers are collected on
an embodiment of the present superfine fiber collection devices
(see FIG. 10).
[0082] FIG. 13 depicts an embodiment of the present spinnerets (see
FIG. 2) depicted in motion where superfine fibers are collected on
an embodiment of the present superfine fiber collection devices
(see FIG. 10).
[0083] FIG. 14 depicts an embodiment of the present spinnerets (see
FIG. 4) depicted in motion where superfine fibers are collected on
an embodiment of the present superfine fiber collection devices
(see FIG. 10).
[0084] FIG. 15 depicts an embodiment of the present spinnerets (see
FIG. 8) depicted in motion where superfine fibers are collected on
an embodiment of the present superfine fiber collection devices
(see FIG. 10).
[0085] FIG. 16 depicts an embodiment of the present spinnerets (see
FIG. 9) depicted in motion where superfine fibers are collected on
an embodiment of the present superfine fiber collection devices
(see FIG. 10).
[0086] FIG. 17 depicts an embodiment of the present spinnerets (see
FIG. 1) depicted in motion where superfine fibers are collected on
multiple embodiments of the present superfine fiber collection
devices (see FIG. 1).
[0087] FIGS. 18-24 depict different embodiments of the present
apparatuses.
[0088] FIG. 25 depicts a photograph (3000.times.) of non-woven
bismuth superfine fibers of single digit micron diameter, produced
using melt spinning wherein a spinneret according to FIG. 1 was
spun at 4,500 RPM at 300.degree. C. (spinneret temperature) for 5
minutes.
[0089] FIG. 26 depicts a photograph (.about.4390.times.) of
non-woven polyethylene oxide (PEO) superfine fibers of micron,
sub-micron and nano diameters, produced using solution spinning
wherein a spinneret according to FIG. 1 was spun at 4,000 RPM at
50.degree. C. (spinneret temperature) for 5 minutes, wherein fibers
were collected on a superfine fiber collection device according to
FIG. 10. The material that was spun was 5% by weight PEO in
de-ionized water.
[0090] FIG. 27 depicts a photograph (2000.times.) of single fiber
polyethylene oxide (PEO) superfine fibers of sub-micron and nano
diameters, produced using melt spinning wherein a spinneret
according to FIG. 1 was spun at 4,000 RPM at 50.degree. C.
(spinneret temperature) for 5 minutes, wherein fibers were
collected on a superfine fiber collection device according to FIG.
10. The material that was spun was 5% by weight PEO in de-ionized
water.
[0091] FIG. 28 depicts a photograph of mat polystyrene (PS)
superfine fibers of single digit micron and nano diameters,
produced using melt spinning wherein a spinneret according to FIG.
4 and FIG. 5 was spun at 5,000 RPM at 240.degree. C. (spinneret
temperature) for 5 minutes using a spinneret according to FIG. 1,
wherein fibers were collected on a superfine fiber collection
device according to FIG. 10. The material that was spun was PS 818
polystyrene from Total Petrochemicals.
[0092] FIG. 29 depicts a photograph of polycarbonate superfine
fibers.
[0093] FIG. 30 depicts a photograph of composite superfine fibers
comprising polycarbonate and blue dye.
DESCRIPTION OF ILLUSTRATIVE EMBODIMENTS
[0094] The term "coupled" is defined as connected, although not
necessarily directly, and not necessarily mechanically. The terms
"a" and "an" are defined as one or more unless this disclosure
explicitly requires otherwise. The term "substantially" is defined
as being largely but not necessarily wholly what is specified, as
understood by a person of ordinary skill in the art. In one
non-limiting embodiment, the term substantially refers to ranges
within 10%, preferably within 5%, more preferably within 1%, and
most preferably within 0.5% of what is specified.
[0095] The terms "comprise" (and any form of comprise, such as
"comprises" and "comprising"), "have" (and any form of have, such
as "has" and "having"), "include" (and any form of include, such as
"includes" and "including") and "contain" (and any form of contain,
such as "contains" and "containing") are open-ended linking verbs.
As a method or apparatus that "comprises," "has," "includes" or
"contains" one or more steps or elements possesses those one or
more steps or elements, but is not limited to possessing only those
one or more steps or elements. Likewise, an element of an apparatus
that "comprises," "has," "includes" or "contains" one or more
features possesses those one or more features, but is not limited
to possessing only those one or more features. For example, a
spinneret comprising a body having a concave cavity configured to
receive a molten material and a lid positioned above the body such
that a gap exists between the lid and the body is a spinneret
having a body that includes the specified features but is not
limited to having only those features. Such a body may also
include, for example, a hole, such as a threaded hole centered at
the base of the spinneret that may be coupled to a joint, such as a
universal threaded joint.
[0096] Furthermore, an apparatus, structure, or portion of an
apparatus or structure that is configured in a certain way is
configured in at least that way, but it may also be configured in
ways other than those specifically described.
[0097] Embodiments of the present methods and apparatuses use
centrifugal force to create superfine fibers having various sizes
and properties. Embodiments of the present apparatuses and methods
may be used, for example, in the biotechnology, medical device,
food engineering, drug delivery, military, and/or electrical
industries, or in ultra-filtration and/or micro-electric mechanical
systems (MEMS).
A. FIBERS
[0098] Fibers represent a class of materials that are continuous
filaments or that are in discrete elongated pieces, similar to
lengths of thread. Fibers are of great importance in the biology of
both plants and animals, e.g., for holding tissues together. Human
uses for fibers are diverse. For example, they may be spun into
filaments, thread, string, or rope. They may be used as a component
of composite materials. They may also be matted into sheets to make
products such as paper or felt. Fibers are often used in the
manufacture of other materials.
[0099] The superfine fibers discussed herein are a class of
materials that exhibit a high aspect ratio (e.g., at least 100 or
higher) with a minimum diameter in the range of micrometer
("micron") (typically single digit) to sub-micrometer
("sub-micron") (e.g., between micrometer and nanometer, such as 700
to 900 nanometers) to nanometer ("nano") (typically 100 nanometers
or less). FIGS. 25-30 show non-limiting examples of some superfine
fibers created using certain of the present methods and
apparatuses. While typical cross-sections of the superfine fibers
are circular or elliptic in nature, they can be formed in other
shapes by controlling the shape and size of the openings in a
spinneret (described below). Non-limiting examples of superfine
fibers that may be created using methods and apparatuses as
discussed herein include polymers (natural or synthetic (that is,
man-made)), polymer blends, biomaterials (e.g., biodegradable and
bioresorbable materials), metals, metallic alloys, ceramics,
composites and carbon superfine fibers. Non-limiting examples of
specific superfine fibers made using methods and apparatuses as
discussed herein include polypropylene (PP), acrylonitrile
butadiene styrene (ABS), nylon, bismuth, polyethylene oxide (PEO)
and beta-lactam superfine fibers. Superfine fibers may comprise a
blending of multiple materials. Superfine fibers may also include
holes (e.g., lumen or multi-lumen) or pores. Multi-lumen superfine
fibers may be achieved by, for example, designing one or more exit
openings to possess concentric openings. In certain embodiments,
such openings may comprise split openings (that is, wherein two or
more openings are adjacent to each other; or, stated another way,
an opening possesses one or more dividers such that two or more
smaller openings are made). Such features may be utilized to attain
specific physical properties, such as thermal insulation or impact
absorbence (resilience). Nanotubes may also be created using
methods and apparatuses discussed herein.
[0100] Superfine fibers may be analyzed via any means known to
those of skill in the art. For example, Scanning Electron
Microscopy (SEM) may be used to measure dimensions of a given
fiber. For physical and material characterizations, techniques such
as differential scanning calorimetry (DSC), thermal analysis (TA)
and chromatography may be used.
B. MULTI-LEVEL VARIABLE FIBER SPINNERS
[0101] The present apparatuses are configured to create superfine
fibers using centrifugal force. Some embodiments of the present
apparatuses may be characterized as "multi-level variable fiber
spinners" or "variable fiber spinners", and comprise certain
components, as described in more detail below.
[0102] 1. Spinnerets
[0103] As defined above, a spinneret as used herein is (a) an
object that may hold the material described herein and that may be
spun (e.g., at 500-25,000 RPM), where the material may exit the
spinneret via at least one pathway, or (b) a collection of objects,
where at least one of the collection of objects may hold the
material described herein, where the collection of objects may be
spun together (e.g., at 500-25,000 RPM) and the material may exit
the spinneret via at least one pathway.
[0104] Typical dimensions for non-syringe-type spinnerets are in
the range of several inches (e.g., 3-8'' in diameter) in diameter
and 1-2'' in height. For example, with respect to spinnerets that
comprise one or more plates, plate diameters may range from, e.g.,
3-8'' in diameter. Typical values for fluid path exit opening
diameters, which are often circular but not restricted to such a
shape, are as follows: syringes (e.g., FIG. 4, FIG. 6) 0.01 mm to
1.0 mm; micro-mesh pores (e.g., FIG. 9) 0.01 mm to 3.0 mm (e.g.,
0.05 mm to 2.0 mm); non-syringe gaps (e.g., FIG. 8) less than 1 mm
to several (e.g., 3-8) mm. Lengthwise, exit openings are typically
straight and typically 1-3 millimeters (e.g., FIG. 1, FIG. 2) to
several (e.g., 3-8) centimeters (e.g., the needles of FIG. 4 and
FIG. 6) in length. Each of these variables are flexible.
[0105] Generally speaking, a spinneret helps control various
properties of the superfine fibers, such as the cross-sectional
shape and diameter size of the superfine fibers. More particularly,
the speed and temperature of a spinneret, as well as the
cross-sectional shape, diameter size and angle of the one or more
openings in a spinneret, all may help control the cross-sectional
shape and diameter size of the superfine fibers. Lengths of
superfine fibers produced may also be influenced by spinneret
choice.
[0106] The temperature of the spinneret may influence superfine
fiber properties, in certain embodiments. Both resistance and
inductance heaters may be used as heat sources to heat a spinneret.
In certain embodiments, the spinneret is thermally coupled to a
heat source that can be used to adjust the temperature of the
spinneret before the spinning, or during the spinning, or both
before the spinning and during the spinning. Moreover, in certain
embodiments, the spinneret is cooled. For example, the spinneret
may be thermally coupled to cooling source that can be used to
adjust the temperature of the spinneret before the spinning, during
the spinning, or before and during the spinning. Temperatures of a
spinneret may range widely. For example, a spinneret may be cooled
to as low as -20.degree. C. or heated to as high as 1500.degree. C.
Temperatures below and above these exemplary values are also
possible, such as, for example, 2500.degree. C. In certain
embodiments, the temperature of a spinneret before and/or during
spinning is between 4.degree. C. and 400.degree. C. The temperature
of a spinneret may be measured by using, for example, an infrared
thermometer or a thermocouple.
[0107] The speed at which a spinneret is spun may also influence
superfine fiber properties. The speed of the spinneret may be fixed
while the spinneret is spinning, or may be adjusted while the
spinneret is spinning. Those spinnerets whose speed may be adjusted
may, in certain embodiments, be characterized as "variable speed
spinnerets." The RPMs of a spinneret may vary, or be varied, as low
as 500 RPM (or lower) or as high as 25,000 RPM (or higher).
[0108] Another spinneret variable includes the material(s) the
spinneret is made of. Spinnerets may be made of a variety of
materials, including metal (brass, aluminum, stainless steel)
and/or plastic. The choice of material depends on, for example, the
temperature the material is to be heated to, or whether sterile
conditions are desired.
[0109] Spinnerets come in a wide range of shapes and sizes, and
some are commercially available. For example, spinnerets that are
employed in commercially available cotton candy machines may be
used, in certain embodiments. Certain embodiments of the present
spinnerets are described in more detail below.
[0110] Certain spinnerets have openings through which material is
extruded during spinning. Such openings may take on a variety of
shapes (e.g., circular, elliptical, rectangular, square,
triangular, fanciful, or the like) and sizes: diameter sizes of
0.01-0.80 mm are typical. The angle of the opening may be varied
between .+-.15 degrees. The openings may be threaded. An opening,
such as a threaded opening, may hold a needle, where the needle may
be of various shapes, lengths and gauge sizes. Threaded holes may
also be used to secure a lid over a cavity in the body of a
spinneret. The lid may be positioned above the body such that a gap
exists between the lid and the body, and a superfine fiber is
created as a result of the spun material exiting the cavity through
the gap. Spinnerets may also be configured such that one spinneret
may replace another within the same apparatus without the need for
any adjustment in this regard. A universal threaded joint attached
to various spinnerets may facilitate this replacement. Moreover,
spinnerets may be configured to operate in a continuous manner.
[0111] Another type of the present spinnerets comprises a syringe
that is spun. Syringes are commercially available and come in a
variety of sizes. A plunger typically is used to hold material in
the syringe, although other stoppers may be used for this purpose.
On the end opposite of the plunger or stopper is a hole: this hole
may be threaded, and a needle may be attached to this hole. A
variety of needles are commercially available, including needles of
various lengths and gauges. Different needles may be used with a
single syringe by exchanging them. A syringe is typically secured
to a syringe support device, such that the syringe and the syringe
support device are spun together.
[0112] One of the present spinnerets is shown in FIG. 1. Spinneret
100 comprises a top plate 101 that is riveted (or may be otherwise
coupled) to bottom plate 103. Bottom plate 103 acts as a reservoir
in which material may be placed. A reservoir cover plate 105 may be
put over the bottom plate 103 to control spillage and also to
provide openings 106 for fluid to escape from the reservoir.
Reservoir cover plate 105 has a circular opening to allow
introduction of material to be spun. For this type of spinneret,
typical amounts of material range from 50-100 mL, but amounts less
than this may be used as well as amounts greater than this, as the
size of the reservoir and the spinneret may each vary. Lining the
perimeter of the reservoir is a material exit path 104: while the
spinneret is spinning, material will generally follow this path. In
other words, material exits openings 106 and then escapes the
spinneret along 104. Material exits the spinneret through one or
more openings 106. Stated otherwise, top plate 101 and/or bottom
plate 103 have one or more peripheral openings 104 around the
perimeter of the reservoir, as shown. In some embodiments, the one
or more peripheral openings 104 comprise a plurality of peripheral
openings. In some embodiments, the one or more peripheral openings
104 comprise a peripheral gap between top plate 101 and bottom
plate 103, that may in some embodiments, for example, be adjusted
by adjusting the distance between the top plate 101 and the bottom
plate 103. In this way, as the spinneret 100 is rotated, as is
described in more detail below, the material can pass through
openings 106 and travel to the one or more peripheral openings 104,
through which the material can exit the spinneret. The hole 107 is
configured to attach to a driver, such as through a universal
threaded joint. Suitable drivers include commercially available
variable electric motors, such as a brushless DC motor. The spin
axis 108 of this spinneret extends centrally and vertically through
the hole 107, perpendicular to the top plate 101. This spinneret
may be used for melt spinning or solution spinning. In certain
embodiments, a spinneret of this type is spun for 300-2,000 seconds
to form superfine fibers. Spinneret 100 may also be operated in a
continuous mode for longer amounts of time.
[0113] Another type of spinneret of the present spinnerets is shown
in FIG. 2. Spinneret 200 comprises a cover plate 201, a base plate
202, and a holding plate 203, the latter of which is shown threaded
with a holding plate screw 204. The cover plate features holes 205
through which plate securing screws 206 may be employed to secure
the three plates together along with the plate securing nuts 207.
The cover plate also features a material injection inlet 208. A
reservoir 209 in the base plate 202 for holding material is joined
to multiple channels 210 such that material held in the reservoir
209 may exit the spinneret through the openings 211. For this type
of spinneret, typical amounts of material range from 5-100 mL, but
amounts less than this may be used as well as amounts greater than
this, as the size of the reservoir and the spinneret may each vary.
The spin axis of this spinneret 212 extends centrally and
vertically through the reservoir 209, perpendicular to each of the
three plates 201, 202 and 203. This spinneret may be used for melt
spinning or solution spinning. In certain embodiments, a spinneret
of this type is spun for 10-500 seconds to form superfine fibers.
This spinneret may also be operated in a continuous mode for longer
amounts of time.
[0114] FIG. 3 shows another embodiment of the present spinnerets.
Spinneret 300 comprises a syringe 301 equipped with a plunger 302
and a variety of needles 303 that may optionally be connected to
the syringe 301 at the opening 304. The syringe 301 may be placed
atop the syringe support device 305. The syringe support device 305
may also serve as a superfine fiber collection device, as discussed
herein. The wedge 306 may optionally be positioned between the
syringe 301 and the syringe support device 305 in order to alter
the angle at which the material is ejected from the syringe 301. A
threaded joint 307, such as a universal threaded joint, is shown
attached to the syringe support device 305.
[0115] FIG. 4 shows a spinneret, such as spinneret 300, in
assembled form. A syringe 301 equipped with a plunger 302 and a
needle 403 is secured to a syringe support device 404 using two
clamps 405. Typically, 10-500 mL of material are placed in the
syringe, but this amount may vary depending on the size of syringe.
The syringe support device comprises two walls 406 and a base 407.
The walls 406 may be straight or cylindrical (curved). Superfine
fibers may collect on the exterior of walls 406 as they exit a
spinneret like spinneret 300: thus this syringe support device may
also act as a superfine fiber collection device. A threaded joint
408, such as a universal threaded joint, is shown attached to the
syringe support device 404 at the hole 409. The spin axis 410 of
this spinneret extends centrally and vertically through the hole
409. This spinneret may be used for solution spinning. In certain
embodiments, a spinneret of this type is spun for 10-1,000 seconds
to form superfine fibers. This spinneret may also be operated in a
continuous mode for longer amounts of time.
[0116] A syringe support device 500 that may also act as a
superfine fiber collection device is shown in FIG. 5. The device
comprises two walls 501 and a base 502 onto which a syringe may be
placed. The walls 501 may be cylindrical (curved). Base 502
includes a hole 503 is configured to attach to a driver, such as
through a universal threaded joint. Superfine fibers may collect on
the exterior of walls 501 as they exit a spinneret like spinneret
300: thus this syringe support device may also act as a superfine
fiber collection device.
[0117] FIG. 6 shows spinneret 600, which comprises a syringe 301
equipped with a plunger 302 and a needle 403. The syringe 301 is
held by the syringe support device 604 through tension between
opposing cylindrical walls 605. Non-limiting mechanisms for
attachment may include a snap fit or an adhesive joint. The syringe
support device 604 may also act as a superfine fiber collection
device by collecting superfine fibers as they exit spinneret 600,
such as on the exterior of walls 605. A threaded joint 606, such as
a universal threaded joint, is shown attached to the syringe
support device 604 at the hole 607. The spin axis 608 of this
spinneret extends centrally and vertically through the hole 607.
Spinneret 600 may be used for solution spinning. Typically, 10-500
mL of material are placed in the syringe, but this amount may vary
depending on the size of syringe. In certain embodiments, a
spinneret of this type is spun for 10-1,000 seconds to form
superfine fibers. This spinneret may also be operated in a
continuous mode for longer amounts of time.
[0118] FIG. 7 shows a syringe support device 700 that may act as a
superfine fiber collection device. Syringe support device 700
includes opposing arcuate (curved) walls 701 configured to contact
the cylindrical outer wall of a syringe, and a base 702 that
includes a hole 703. Superfine fibers may collect on the exterior
of walls 701 as they exit a spinneret like spinneret 300: thus this
syringe support device may also act as a superfine fiber collection
device.
[0119] Yet another spinneret of the present spinnerets is shown in
FIG. 8. Spinneret 800 includes a reservoir 801 in the shape of a
concave cavity is centered within the wall 802 of the spinneret.
Typically, 100-1,000 mL of material are placed in the reservoir,
but amounts less than this may be used as well as amounts greater
than this, as the size of the reservoir and the spinneret may each
vary. Spinneret 800 also includes lid 803, which includes threaded
holes 804 that allow the lid 803 to be secured to the reservoir 801
using one or more screws 805. Not every threaded hole 804 need be
used for securing the lid to the reservoir 801: at least one hole
804 may also act as an opening through which material may exit
during spinning. In certain embodiments, material may exit the
reservoir 801 via a gap between the lid 803 and the reservoir. A
threaded joint 806, such as a universal threaded joint, is shown
attached to the base of the spinneret. The spin axis 807 of this
spinneret extends centrally and vertically through the reservoir
801. This spinneret may be used for melt spinning or solution
spinning. In certain embodiments, a spinneret of this type is spun
for 10-5,000 seconds to form superfine fibers. This spinneret may
also be operated in a continuous mode for longer amounts of
time.
[0120] FIG. 9 depicts spinneret 900 including a top plate 901 and a
bottom plate 902 separated by a micro-mesh material 903. The
micro-mesh material may comprise, for example, stainless steel or
plastic. Such micro-mesh material may be obtained from commercial
sources, such as MSC Industrial Supply Co. (cat. no. 52431418). The
distance spanned by the micro-mesh between top plate 901 and bottom
plate 902 may range, for example, between 1-10'' (e.g., 1'', 2'',
3'', 4'', 5'', 6'', 7'', 8'', 9'', or 10'', or any value or range
therein). A hole 904 in the bottom plate 902 that extends through a
bottom connector 905 allows for connection for a threaded joint,
such as a universal threaded joint. Spinneret 900 is typically used
for melt spinning. Solid granules (e.g., polymer beads) may be
placed in the bottom plate 902, which acts as storage, rather than
a reservoir as with certain other spinnerets. However, it is
possible to modify this bottom plate 902 to act a reservoir for
liquid material by raising the solid wall of this plate. With such
a modification, it is possible to use this spinneret for solution
spinning. The spin axis 906 of this spinneret extends centrally and
vertically through the hole 904. This spinneret may also be
operated in a continuous manner.
[0121] 2. Superfine Fiber Collection Devices and Methods
[0122] Superfine fibers created using the present methods or the
present apparatuses may be collected using a variety of superfine
fiber collection devices. Three exemplary devices are discussed
below, and each of these devices may be combined with one
another.
[0123] The simplest method of superfine fiber collection is to
collect the fibers on the interior of a collection wall that
surrounds a spinneret (see, e.g., collection wall 1000 shown in
FIG. 10). Superfine fibers are typically collected from collection
walls similar to collection wall 1000 as unwoven superfine
fibers.
[0124] The aerodynamic flow within the chamber influences the
design of the superfine fiber collection device (e.g., height of a
collection wall or rod; location of same). Aerodynamic flow may be
analyzed by, for example, computer simulation, such as
Computational Fluid Dynamics (CFD).
[0125] The spinning spinneret develops an aerodynamic flow within
the confinement of the apparatuses described herein. This flow may
be influenced by, for example, the speed, size and shape of the
spinneret as well as the location, shape, and size of the superfine
fiber collection device. An intermediate wall placed outside the
collection wall may also influence aerodynamic flow. The
intermediate wall may influence the aerodynamic flow by, for
example, affecting the turbulence of the flow. Placement of an
intermediate wall may be necessary in order to cause the superfine
fibers to collect on a superfine fiber collection device. In
certain embodiments, placement of an intermediate wall is
determined by a method comprising operating a spinneret in the
presence of a superfine fiber collection device and an intermediate
wall, observing whether or not superfine fibers are collected on
the superfine fiber collection device, and if they are not, then
moving the intermediate wall (e.g., making its diameter smaller or
larger, or making the intermediate wall taller or shorter) to
perform the experiment again to see if superfine fibers are
collected. Repetition of this process may occur until superfine
fibers are collected on the superfine fiber collection device.
[0126] A stagnation zone may develop at, for example, the site of
the spinning spinneret (such as centered at the spinning
spinneret). A spinneret is typically designed such that it does not
disturb the stagnation zone. One knows when a spinneret is not
designed properly with respect to the stagnation zone because
superfine fibers will not form correctly (e.g., they will not form
in a desired manner). For example, regarding the embodiments of the
present invention shown in FIG. 5 and FIG. 7, these embodiments
were designed with a purpose of collecting mat superfine fibers. If
mat superfine fibers were not collected, one reason was likely that
the embodiment was disturbing the stagnation zone. Thus, with
respect to the embodiments of FIG. 5 and FIG. 7, it was determined
that to minimize disturbance of the stagnation zone, typically the
syringe support device/superfine fiber collection device should be
about the size of the syringe, .+-.20% (in terms of both diameter
and length). In certain embodiments employing syringes, design of a
syringe support device may be done using this parameter in
mind.
[0127] Typically, fibers are collected on the collection wall or
settle onto other designed structure(s) of stagnation zone. It is
important to realize that temperature plays an important role on
the size and morphology of fibers. If the collection wall, for
example, is relatively hotter than the ambient temperature, fibers
collected on the collection wall may coalesce at this temperature
leading to bundling of nanofibers and/or welding of individual
fibers on several points. To avoid this, in some embodiments, the
temperature of the intermediate wall can be controlled, such as,
for example, by blowing gas (e.g., air, nitrogen) between the two
(intermediate and collection) walls. By controlling the flow rate,
type, and temperature of this blowing gas, it is possible to
control the temperature and morphology of the superfine fibers. Key
design parameters can include wall (height, location, etc.) and gas
(temperature, type, etc.) characteristics.
[0128] The intermediate wall can also be used to control, adjust,
and/or influence the aerodynamic flow within the apparatus.
Aerodynamic flow typically guides the superfine fibers to rest on
one or more superfine fiber collection devices. If, upon formation,
loose superfine fibers float in an apparatus of the present
apparatuses (due to their very small mass) without coming to rest
on one or more superfine fiber collection devices, it is likely
that, for example, the intermediate wall is not positioned
correctly, or the superfine fiber collection device(s) is not
correctly positioned, and/or the aerodynamic flow is not properly
understood. An intermediate wall is typically taller than any
collection wall that may be used (e.g., 1.5 times as high as the
collection wall), and surrounds such a collection wall (e.g., 2-4''
(e.g., 3'') away from the collection wall; or, for example, the
intermediate wall may be 10-30% larger (e.g., 20% larger) than the
collection wall). An intermediate wall may be segmented, and may
have one or more holes in it.
[0129] If the objective is to collect unidirectional and long
superfine fibers, a collection rod may be designed and positioned
at an appropriate distance from the spinneret. An example of this
is collection rod 1100 shown in FIG. 11. One or more collection
rods (like rod 1100) are typically placed at a distance of 5-7''
(e.g., 6'') from the center of the spinneret. One or more
collection rods may be positioned along the perimeter of the
interior of a collection wall. A collection rod may be stationary
during superfine fiber collection, or it may be rotated during
collection. Rods of this nature may be made from any suitable
material that will give them significant rigidity, such as
polycarbonate and metals (e.g., aluminum, stainless steel). In
embodiments of the present apparatuses where the rod or rods will
be rotated, the rods may be secured to a structure like a plate
that is connected, along with the spinneret, to a driver. The
rod-holding plate and spinneret may be geared to each other in way
that allows both to rotate in the same or opposite directions as a
result of the rotation of a single driver. The diameter of a rod is
typically 0.20''-0.30'' (e.g., 0.25''), but a variety of sizes may
be used. The rod may, for example, be rotated at a speed of 50 to
250 RPM.
[0130] Drawings depicting superfine fiber collection in action are
provided in FIGS. 12-17. FIG. 12 shows superfine fiber creation
using spinneret 100 of FIG. 1 that is spinning clockwise about a
spin axis, where material is exiting the spinneret as superfine
fibers 1202 along various pathways 1203. Those superfine fibers are
being collected on the interior of the surrounding collection wall
1000 of FIG. 10.
[0131] FIG. 13 shows superfine fiber creation using spinneret 200
of FIG. 2 that is spinning clockwise about a spin axis, where
material is exiting openings 211 in the spinneret as superfine
fibers 1303 along various pathways 1304. Those superfine fibers are
being collected on the interior of the surrounding collection wall
1000 of FIG. 10.
[0132] FIG. 14 shows superfine fiber creation using spinneret 400
of FIG. 4 that is spinning clockwise about a spin axis, where
material is exiting the needle 403 of the syringe 301 as superfine
fibers 1404 along various pathways 1405. Those superfine fibers are
being collected on the interior of the surrounding collection wall
1000 of FIG. 10 as well as on the syringe support device 500 (with
curved walls) of FIG. 5, such that the syringe support device also
acts as a superfine fiber collection device.
[0133] FIG. 15 shows superfine fiber creation using spinneret 800
of FIG. 8 that is spinning clockwise about a spin axis, where
material that is placed in the reservoir 803 of the spinneret 800
is exiting the openings 804 as superfine fibers 1504 along various
pathways 1505. Those superfine fibers are being collected on the
interior of the surrounding collection wall 1000 of FIG. 10.
[0134] FIG. 16 shows superfine fiber creation using spinneret 900
of FIG. 9 that is spinning clockwise about a spin axis, where
material is exiting the openings of the micro-mesh 903 as superfine
fibers 1603 along various pathways 1604. Those superfine fibers are
being collected on the interior of the surrounding collection wall
1000 of FIG. 10.
[0135] FIG. 17 shows superfine fiber creation using spinneret 100
that is spinning clockwise about a spin axis, where material is
exiting the spinneret as superfine fibers 1702 along various
pathways 1703. Those superfine fibers are being collected on the
collecting rods 1100 (FIG. 11) and on the interior of the
collection wall 1000 (FIG. 10).
[0136] 3. Environment
[0137] The conditions of the environment in which superfine fibers
are created may influence various properties of those fibers. For
example, some metallic superfine fibers, such as iron superfine
fibers, react with ambient air. For such applications, it is
preferable to replace ambient air with an inert gas (e.g., nitrogen
or argon). Humid conditions may detrimentally affect the surfaces
of many polymeric superfine fibers, such as poly(ethylene oxide)
(PEO). Thus, lowering humidity levels is preferable. Similarly,
drugs may be required to be developed under sterile conditions that
are not maintained in ambient conditions: a sterile environment is
therefore preferred in such situations.
[0138] The "environment" refers to the interior space defined by
the housing that surrounds the components of an apparatus as
described herein. For certain uses, the environment may simply be
ambient air. Air may be blown into the environment, if desired. For
other uses, the environment may be subjected to low-pressure
conditions, such as 1-760 mm Hg, or any range derivable therein
using, for example, a vacuum pump. Alternatively, the environment
may be subjected to high-pressure conditions, such as conditions
ranging from 761 mm Hg up to 4 atm or higher using, for example, a
high pressure pump. The temperature of the environment may be
lowered or raised, as desired, through the use of heating and/or
cooling systems, which are described below. The humidity level of
the environment may be altered using a humidifier, and may range
from 0-100% humidity. For certain applications, such as drug
development, the environment may be rendered sterile. If the
components of an apparatus are each made of, for example, stainless
steel, all components may be individually sterilized and assembled,
such as in a clean room. Every operator of such an apparatus must
be appropriately cleaned and covered with gowns and mask. The
sterile environment should be monitored for sterility: this may be
done using methods known in the art.
[0139] 4. Heating and Cooling Sources
[0140] Several types of heating and cooling sources may be used in
apparatuses and methods as discussed herein to independently
control the temperature of, for example, a spinneret, a collection
wall, an intermediate wall, a material, and/or the environment
within an apparatus.
[0141] Three non-limiting types of heat sources that may be
employed include resistance heaters, inductive heaters and IR
(Infra Red) heaters. Peltier or Thermoelectric Cooling (TEC)
devices may be used for heating and/or cooling purposes. Cold gas
or heated gas (e.g., air or nitrogen) may also be pumped into the
environment for cooling or heating purposes. Each of these heaters
and coolers may be purchased from commercial vendors. Conductive,
convective, or radiation heat transfer mechanisms may be used for
heating and cooling of various components of the apparatuses.
[0142] 5. Apparatuses and Their Components
[0143] Various exemplary apparatuses are shown in FIGS. 18-24. It
is to be understood that various components of these apparatuses
(e.g., spinnerets, superfine fiber collection devices, heaters,
coolers, thermal insulation) may be added, subtracted and
interchanged as needed.
[0144] Components of apparatuses may be made from a variety of
materials. In certain embodiments, the components of an apparatus
may be made namely from stainless steel. For example, the
spinneret, collection wall and housing may each be made from
stainless steel. In this situation, the components may be used for,
e.g., low melting metals like tin (232.degree. C.), zinc
(420.degree. C.), silver (962.degree. C.) and alloys thereof. In
certain embodiments, ceramic components may be used for high
melting alloys, such as gold (1064.degree. C.) and nickel
(1453.degree. C.). Manipulation of high melting alloys may require
blanketing the environment of the components with an inert gas,
such as nitrogen or helium, with appropriate sealing of the
housing.
[0145] a. Exemplary Apparatuses
[0146] FIG. 18 shows a partially cut-away perspective view of one
embodiment of the present apparatuses. Apparatus (or system) 1800
includes spinneret 1801, which has peripheral openings 1802 and is
connected to a threaded joint 1803, such as a universal threaded
joint, which, in turn, is connected to a motor 1804 via a shaft
1805. The motor 1804, such as a variable speed motor, is supported
by support springs 1806 and is surrounded by vibration insulation
1807. A motor housing 1808 encases the motor 1804, support springs
1806 and vibration insulation 1807. A heating unit 1809 and is
enclosed within an oven 1810 (e.g., a heat reflector wall) that has
openings 1810a that direct heat (thermal energy) to the spinneret
1801. In the embodiment shown, heating unit 1809 sits on thermal
insulation 1811. Surrounding the oven 1810 is a collection wall
1812, which, in turn, is surrounded by an intermediate wall 1813. A
housing 1814 seated upon a seal 1815 encases the spinneret 1801,
heating unit 1809, oven 1810, thermal insulation 1811, collection
wall 1812 and intermediate wall 1813. An opening 1816 in the
housing 1814 allows for introduction of elements (e.g., gas) into
the internal environment of the apparatus, or allows elements
(e.g., air) to be pumped out of the internal environment of the
apparatus. The lower half of the apparatus is encased by a wall
1817 which is supported by a base 1818. An opening 1819 in the wall
1817 allows for further control of the conditions of the internal
environment of the apparatus. Indicators for power 1820 and
electronics 1821 are positioned on the exterior of the wall 1817 as
are control switches 1822 and a control box 1823. Further
description of these controls is provided below.
[0147] A partially cut-away perspective view of an apparatus that
is substantially similar to the apparatus of FIG. 18 is shown in
FIG. 19. However, in this figure, the openings 1816 and 1819 are
not present. Yet another partially cut-away perspective view of an
apparatus that is substantially similar to the apparatus of FIG. 18
is shown in FIG. 20. However, in this figure, valves 2001 are shown
occupying the openings 1816 and 1819. These valves allow for
controlled introduction and ejection of elements into and out of
the interior environment of the apparatus. An additional partially
cut-away perspective view of an apparatus that is substantially
similar to the apparatus of FIG. 18 is shown in FIG. 21. The
differences in this figure include the addition of a thermoelectric
cooler 2101 that may cool the interior environment of the
apparatus, and the openings 1816 and 1819 are not present. Other
types of coolers may be employed with the apparatus of FIG. 18 as
well. FIG. 22 shows another partially cut-away perspective view of
an apparatus that is substantially similar to the apparatus of FIG.
18. In FIG. 22, the vibration insulation 1808 is replaced by
high-frequency vibration insulation 2201. This allows for higher
RPM spinning rates for a spinneret.
[0148] In FIG. 23, a cut-away perspective view of an apparatus that
is substantially similar to the apparatus of FIG. 18 is shown.
However, the spinneret of FIG. 18 has been replaced by a different
type of spinneret. The spinneret of FIG. 23 is similar in style to
the spinneret of FIG. 4, where a syringe 2301 equipped with a
plunger 2302 and a needle 2303 is held by a syringe support device
2304. Other spinnerets may be employed with the apparatus of FIG.
23 as well.
[0149] FIG. 24 shows a cut-away perspective view of an apparatus
that is substantially similar to the apparatus of FIG. 18 as well,
but in addition to the collection wall 1812, collection rods 2401
are shown. Collection rods may be used in conjunction with a
collection wall to collect superfine fibers, or each type of
collection device may be used separately.
[0150] b. Control System
[0151] A control system of an apparatus (e.g., FIGS. 18, 1822 and
1823) allows a user to change certain parameters (e.g., RPM,
temperature, environment) to influence superfine fiber properties.
One parameter may be changed while other parameters are held
constant, if desired. One or more control boxes in an apparatus may
provide various controls for these parameters, or certain
parameters may be controlled via other means (e.g., manual opening
of a valve attached to a housing to allow a gas to pass through the
housing and into the environment of an apparatus). It should be
noted that the control system can be integral to the apparatus (as
shown in FIGS. 18-24) or can be disposed separately from the
apparatus (e.g., can be modular with suitable electrical
connections).
[0152] In certain methods described herein, material spun in a
spinneret or heated structure may undergo varying strain rates,
where the material is kept as a melt or solution. Since the strain
rate alters the mechanical stretching of the superfine fibers
created, final superfine fiber dimension and morphology may be
significantly altered by the strain rate applied. Strain rates are
affected by, for example, the shape, size, type and RPM of a
spinneret. Altering the viscosity of the material, such as by
increasing or decreasing its temperature or adding additives (e.g.,
thinner), may also impact strain rate. Strain rates may be
controlled by a variable speed spinneret. Strain rates applied to a
material may be varied by, for example, as much as 50-fold (e.g.,
500 RPM to 25,000 RPM).
[0153] Temperatures of the material, spinneret and the environment
may be independently controlled using a control system. The
temperature value or range of values employed by the present
methods typically depend on the application. For example, for many
applications, temperatures of the material, spinneret and the
environment typically range from -4.degree. C. to 400.degree. C.
Temperatures may range as low as, for example, -20.degree. C. to as
high as, for example, 1500.degree. C. For melt spinning of
polymers, a spinneret temperature of 200.degree. C. is used For
melt spinning involving metals, spinneret temperatures of
500.degree. C. or higher may be used. For solution spinning,
ambient temperatures of the spinneret are typically used. In drug
development studies (see below), the spinneret temperature range
may be between, for example, 4.degree. C. and 80.degree. C. When
producing ceramic or metal superfine fibers, the temperatures
utilized may be significantly higher. For higher temperatures, it
will typically be necessary to make appropriate changes in the
materials of the housing of an apparatus and/or the interior
components (e.g., substitution of metal for plastic), or in the
apparatus itself (e.g., addition of insulation). Such changes may
also help avoid undesirable reactions, such as oxidation.
[0154] An example of how the variables discussed herein may be
controlled and manipulated to create particular superfine fibers
regards drug development. Solubility and stability of drugs are two
key considerations in developing drug delivery systems. Both of
these parameters may be simultaneously controlled using the methods
and apparatuses described herein. Solubility of the drug is often
significantly improved by controlling its size: that is, the
smaller the size, the better the solubility. For example,
micron-sized fibers of optically active beta-lactams may be
developed from their crystals (see, e.g., Example 5). At this
significantly reduced size, the solubility of the drug in water is
expected to show significant improvement over larger sized drug
particles due to the higher surface area. Moreover, one may
dissolve a drug in an appropriate solvent that then evaporates,
leaving behind a superfine fiber composed of the drug. One may also
use the methods and apparatuses discussed herein to encapsulate
such a drug in a material which is also spun, thereby forming a
drug-encapsulated superfine fiber. To facilitate the stability of
certain drugs, it may often be necessary to lower the temperature
of the environment below ambient conditions. Since the housing of
an apparatus may be designed with adequate insulation, temperatures
may be lowered as needed, such as -10.degree. C. or below.
C. OVERVIEW OF SUPERFINE FIBER CREATION
[0155] Superfine fibers as discussed herein may be created using,
for example, a solution spinning method or a melt spinning method.
In both the melt and solution spinning methods, a material may be
put into a spinneret which is spun at various speeds until fibers
of appropriate dimensions are made. The material may be formed, for
example, by melting a solute or may be a solution formed by
dissolving a mixture of a solute and a solvent. Any solution or
melt familiar to those of ordinary skill in the art may be
employed. For solution spinning, a material may be designed to
achieve a desired viscosity, or a surfactant may be added to
improve flow, or a plasticizer may be added to soften a rigid
superfine fiber. In melt spinning, solid granules may comprise, for
example, a metal or a polymer, wherein polymer additives may be
combined with the latter. Certain materials may be added for
alloying purposes (e.g., metals) or adding value (such as
antioxidant or colorant properties) to the desired superfine
fibers.
[0156] Non-limiting examples of reagents that may be melted, or
dissolved or combined with a solvent to form a material for melt or
solution spinning methods include polyolefin, polyacetal,
polyamide, polyester, cellulose ether and ester, polyalkylene
sulfide, polyarylene oxide, polysulfone, modified polysulfone
polymers and mixtures thereof. Non-limiting examples of solvents
that may be used include oils, lipids and organic solvents such as
DMSO, toluene and alcohols. Water, such as de-ionized water, may
also be used as a solvent. For safety purposes, non-flammable
solvents are preferred.
[0157] In either the solution or melt spinning method, as the
material is ejected from the spinning spinneret, thin jets of the
material are simultaneously stretched and dried in the surrounding
environment. Interactions between the material and the environment
at a high strain rate (due to stretching) leads to solidification
of the material into fibers, which may be accompanied by
evaporation of solvent. By manipulating the temperature and strain
rate, the viscosity of the material may be controlled to manipulate
the size and morphology of the superfine fibers that are created. A
wide variety of superfine fibers may be created using the present
methods, including novel fibers such as polypropylene (PP)
nanofibers. Non-limiting examples of superfine fibers made using
the melt spinning method include polypropylene, acrylonitrile
butadiene styrene (ABS) and nylon. Non-limiting examples of
superfine fibers made using the solution spinning method include
polyethylene oxide (PEO) and beta-lactams.
[0158] Creation of fibers may take between a few seconds (e.g.,
10-20) to several hours (e.g., 2-7), depending upon the type and
amount of material used. The creation of fibers can be done in
batch modes or in continuous modes. In the latter case, material
can fed continuously into the spinneret and the process can be
continued over days (e.g., 1-4) and even weeks (e.g., 2-4).
D. EXAMPLES
[0159] The following examples are included to demonstrate preferred
embodiments of the present methods and apparatuses. Those of skill
in the art should, in light of the present disclosure, appreciate
that many changes can be made in the specific embodiments disclosed
in these examples and still obtain a like or similar result without
departing from the scope of the invention.
Example 1
Solution Spinning Method of Producing Polyethylene Oxide (PEO)
Nanofibers
[0160] In this example, the material employed was a polymer of a
particular molecular weight and the temperature of the spinneret
was fixed, while the RPM and polymer concentration were both
varied. Thus, the effects of RPM and polymer concentration on
superfine fiber diameters and properties were tested.
[0161] A 3% by weight polyethylene oxide (PEO; MW=900,000 g/mol) in
de-ionized (DI) water was prepared. The temperature for both the
spinneret and the solution was maintained at 50.degree. C. The
temperature of the spinneret was measured using an IR sensor. A
small beaker holding 25 mL of solution was placed on a standard
heating/stirring unit and the temperature of the solution was
brought to 50.degree. C. To minimize evaporation, the beaker was
covered with aluminum foil. The solution was kept in a refrigerator
unless in use. The environment in which the superfine fibers were
created was ambient air at ambient temperature. An aerodynamic wall
(intermediate wall) was placed outside of the collection wall, such
as shown in FIG. 18 through FIG. 22 at a distance of about 3'' from
the collection wall.
Procedure:
[0162] 1. A spinneret according to FIG. 1 was preheated to
50.degree. C. using a resistance heater. A commercially available
IR sensor was used to monitor the temperature. The temperature was
maintained by turning the heat on and off as needed. The
temperature was achieved and maintained typically for roughly 10
minutes before proceeding. [0163] 2. About 50 mL of the PEO
solution was dispensed into the pre-heated spinneret. [0164] 3. The
spinneret was spun at 1,000 RPM for three minutes. [0165] 4.
Superfine fibers collected on a superfine fiber collection device
according to FIG. 10 (a collection wall). [0166] 5. Spinning was
stopped. [0167] 6. The temperature of the spinneret was monitored
(every 10 seconds) from start (that is, when the solution is added
to the spinneret) to finish (that is, when spinning stopped) as the
temperature of the spinneret typically decreased over time. [0168]
7. One or more glass slides (e.g., 6''.times.1.25''.times. 1/16'')
were used to manually collect superfine fiber samples by scooping
the superfine fibers away from the collection wall: one side of the
slide was used to collect the fibers, while the other side was
labeled as needed. [0169] 8. The sample may be saved in a
desiccator, if desired. [0170] 9. The spinneret was disassembled
and cleaned for the next experiment with warm tap water for 15
minutes, followed by a rinse with DI water. [0171] 10. The
spinneret was reassembled and heated again to 50.degree. C. [0172]
11. Steps 2-7 were repeated at 2,000, 3,000, 4,000 and 5,000 RPM.
[0173] 12. Steps 1-9 were repeated using 5% and 7% PEO
solutions.
Results:
[0174] This method afforded nanofibers. Typically, higher PEO
concentrations led to thicker fibers and higher RPMs lead to
thinner fibers.
Example 2
Melt Spinning Method of Producing Polystyrene (PS) Single Digit
Micron Fibers
[0175] In this example, the amount of polymer was controlled, while
the RPM was varied. Thus, the effects of RPM on the size and
properties of the superfine fibers created were examined.
[0176] Polystyrene may be obtained from a variety of commercial
sources in a variety of forms. Here, a commercially available
product (white pellets) from Total Petrochemicals called PS 818 was
employed. It is a high impact polystyrene (HIPS) that has a high
heat resistance and is suitable for injection molding, extrusion
and thermoforming. The environment in which the superfine fibers
were created was ambient air at ambient temperature. An aerodynamic
wall (intermediate wall) was placed outside of the collection wall,
such as shown in FIG. 18 through FIG. 22 at a distance of about 3''
from the collection wall.
Procedure:
[0177] 1. 30 grams of PS 818 white pellets were melted in a
crucible using a standard scientific heater with temperature
control. Depending upon the grade and specific formulation, its
melting temperature varied between 190.degree. C. and 260.degree.
C. [0178] 2. Using a resistance heater, a spinneret according to
FIG. 1 was heated to 240.degree. C. to ensure that the polymer
remained fluid in the spinneret. The temperature was not raised
higher than 260.degree. C. to avoid potential degradation. The
temperature of the spinneret was measured using an IR sensor.
[0179] 3. The molten material (30 mL) were dispensed into the
heated spinneret. [0180] 4. The spinneret was spun at 1,000 RPM for
up to three minutes. [0181] 5. Spinning was stopped. [0182] 6. The
temperature of the spinneret was monitored every 10 seconds, as
described in Example 1, step 5. [0183] 7. Superfine fibers were
collected, as described in Example 1, step 6. [0184] 8. The marked
sample was stored in a desiccator. [0185] 9. The spinneret was
cleaned by heating it to 300.degree. C. and spinning it at 6,000
RPM for few minutes. [0186] 10. The spinneret was reassembled, and
for the next run, the RPM of the spinneret was increased by 500.
[0187] 11. Steps 2-10 were repeated until the RPM reached 6,000
RPM.
Results:
[0188] Single digit micron fibers were produced. The best results
were achieved at 240.degree. C. C and 4,500 RPM
Example 3
TABLE-US-00001 [0189] Table of Exemplary Apparatuses and Uses
Thereof The following table depicts a variety of non-limiting
exemplary apparatuses and possible uses thereof. Melt Spinning
Maximum Minimum Solution Spinneret Spinneret Spinneret Non-limiting
Apparatus Spinneret Collection Spinning, Temperature Temperature
RPM Superfine Fiber Example of Type Type Method or Both (.degree.
C.) (.degree. C.) Range Environment Use 1 FIGS. Wall and/or Both
400 Ambient 500-25,000 Ambient Polymers and 1, 2, 4, 6, 8, 9 rod
their alloys 2 FIGS. Wall and/or Both 400 -20.degree. C. 500-6,000
Ambient Food industry 1, 2, 4, 6, 8, 9 rod, and preferably
biopolymers wall 3 FIGS. Wall and/or Both, but 1,000 Ambient
500-6,000 Ambient Low melting 1, 2, 8, 9 rod typically metals melt
spinning 4 FIGS. Wall and/or Both, but 1,500 Ambient 500-10,000
Ambient, heated, High melting 1, 2, 8, 9 rod typically or cooled;
metals and melt optional alloys spinning introduction of gas 7
FIGS. 4, 6 Wall and/or Solution 400 -20.degree. C. 500-6,000
Sterile Drug and drug rod, spinning delivery system preferably
development wall 8 FIGS. Wall and/or Both Custom Custom Custom
Custom Custom 1, 2, 4, 6, 8, 9 rod
Example 4
Method of Producing Acrylonitrile Butadiene Styrene Nanofibers
[0190] Acrylonitrile Butadiene Styrene (ABS) may be obtained from a
variety of commercial sources in a variety of forms. Here, a
commercially available product (off-white pellets) from Star
Plastic was employed. The specific grade of ABS chosen was a
recycled grade suitable for injection molding. The environment in
which the superfine fibers were created was ambient air at ambient
temperature. Superfine fibers were collected on the collection wall
and the spinneret was a spinneret according to FIG. 1. An
aerodynamic wall was placed outside of the collection wall, such as
shown in FIG. 18 through FIG. 22 at a distance of about 3'' from
the collection wall.
Procedure:
[0191] 1. 300 grams of gray ABS pellets were melted in a crucible
using a standard scientific heater with temperature control.
Depending upon the grade and specific formulation, its melting
temperature varied between 210.degree. C. and 280.degree. C. [0192]
2. Using a resistance heater, the spinneret initial temperature and
RPM were set at 200.degree. C. and 500 RPM, respectively. [0193] 3.
The temperature of the spinneret was continually measured every 10
seconds using an IR sensor and adjusted to the desired temperature
as necessary. [0194] 4. About 30 mL molten material was dispensed
into the heated spinneret to start the experiment. [0195] 5. The
spinneret was set to spinning at 500 RPM. [0196] 6. Temperature was
increased by another 10.degree. C. unless it was more than
300.degree. C. In that case go to Step 25. [0197] 7. RPM of the
spinneret was increased by another 500 RPM unless the RPM exceeded
6,000. In that case go to Step 16. [0198] 8. Spinneret was spun at
the set RPM and temperature for up to three minutes. [0199] 9.
Spinning was stopped. [0200] 10. Collecting wall is inspected for
superfine fibers. If there are no fibers found make a note and go
to Step 18. [0201] 11. Superfine fibers were collected, as
described in Example 1, step 6. [0202] 12. The marked sample was
stored in a desiccator. [0203] 13. Go to Step 18. [0204] 14. The
spinneret was cleaned by heating it to 350.degree. C. or slightly
higher and spinning it at 6,000 RPM for few minutes. [0205] 15. The
spinneret was reassembled and made ready for the next run.
Results:
[0206] Most of the fibers were micron size fibers. Optimal
conditions for superfine fiber production were around 280.degree.
C. and 4,500 RPM.
Example 5
Method of Producing Beta-Lactam Superfine Fibers
[0207] There are several formulations for beta-lactams that are
commercially available or that may be prepared using known
synthetic methods. Here, crystalline powders of a specific
formulation called Optically Inactive Beta-Lactam (OIBL) was used
to develop Beta-Lactam Superfine Fibers (BLSF). Samples were
donated by Professor Bimal Banik, The University of Texas, Pan
American, Department of Chemistry. A 3% by weight OIBL brown powder
was dissolved in DMSO (dimethyl sulfoxide) at room temperature (RT)
in a beaker with the help of magnetic stirrer. To minimize
evaporation, 30 mL of the solution was kept covered in a beaker
with wax paper. Other solutions with varying concentrations of 1%,
5%, 7%, 9% and 10% were similarly made and kept covered at RT. All
the solutions were used during these experiments. The environment
in which the superfine fibers were created was ambient air at
ambient temperature. A spinneret according to FIG. 1 was used and a
superfine fiber collection device according to FIG. 10 was used. An
aerodynamic wall was placed outside of the collection wall, such as
shown in FIG. 18 through FIG. 22 at a distance of about 3'' from
the collection wall.
Procedure:
[0208] 1. The 30 mL OIBL/DMSO solution was poured into the
spinneret, where the spinneret was at RT. [0209] 2. The experiment
commenced with the 30 mL OIBL/DMSO solution with 3% concentration.
[0210] 3. RPM for the spinneret was set at 0 RPM. [0211] 4. The
spinneret was re-set at 1,000 RPM higher than the previous set RPM.
[0212] 5. If the new re-set RPM was more than 5,000 go to step 10.
[0213] 6. Spin the spinneret for three minutes. [0214] 7. Spinning
was stopped to collect superfine fibers. [0215] 8. One or more
glass slides (e.g., 6''.times.1.25''.times. 1/16'') was used to
manually collect superfine fiber samples by scooping out the
superfine fibers from the collection wall. One side of the slide
was used to collect the fibers, while the other side was labeled as
needed. [0216] 9. The sample was saved in a desiccator. [0217] 10.
Steps 3 through 8 were repeated. [0218] 11. Repeat the experiment
with next higher concentration by re-setting RPM at 0 and following
Steps 3 through 9. If all the solutions were used up go next to
Step 11. [0219] 12. The spinneret was disassembled and cleaned for
the next experiment with warm tap water for 15 minutes, followed by
a rinse with DI water.
Results:
[0220] Most of the experiments did not yield superfine fibers in
high quantities. Solutions typically were sputtered over the
collection wall. However, in certain cases, there was aa mixture of
few superfine fibers with a large quantity of sputtered solution.
Best results were obtained using a 5% solution at 4,000 RPM.
Scrutiny under optical microscopes at 200.times. showed that they
were mostly micron size fibers.
Example 6
Method of Producing Polycarbonate Superfine Fibers
[0221] There are several formulations for polycarbonate that are
commercially available or that may be prepared using known
synthetic methods. Here, bulk polycarbonate beads were used to
develop Polycarbonate Superfine Fibers by the melt spinning methods
described herein. The environment in which the superfine fibers
were created was ambient air at a temperature below the melting
temperature of the polymer (polycarbonate). It was attempted to
keep the temperature of this ambient air at RT, such as, for
example, by introducing cooling air by way of an opening (e.g.,
1816 in FIG. 18,) in the housing. However, in certain repetitions
of the procedure below, the temperature of the ambient air rose to
as much as 70.degree. C. In certain repetitions of the procedure
below, a spinneret according to FIG. 1 was used and, in others, a
superfine fiber collection device according to FIG. 8 was used. An
aerodynamic wall was placed outside of the collection wall, such as
shown in FIG. 18 through FIG. 22 at a distance of about 3'' from
the collection wall.
[0222] While many polymers have found applications in various
industries, polycarbonate can be particularly attractive for
certain applications because of its high strength (including
impact), optical clarity, and biocompatibility. Polycarbonate's
usage in medical device industry can also make it particularly
attractive for medical applications such as, for example, medical
devices, implants, and even, drug delivery devices. Some
applications for polycarbonate superfine fibers, for example, can
include electret filters, biocompatible nanofilters and potential
bio-absorbers. Polycarbonate may also be suitable for
bio-absorbers, for example, when mixed with appropriate
bio-absorbents like agarose, as discussed in more detail below.
Additionally, the ability to sterilize polycarbonate by radiation
can be an attractive feature for medical applications.
Procedure:
[0223] 1. Melted (molten) polycarbonate was spun in the spinneret,
where the spinneret was at a temperature above the melting
temperature of the polycarbonate, but below the degradation
temperature of the polycarbonate, such as, for example 300.degree.
C., 350.degree. C., and/or 300-350.degree. C. [0224] 2. RPM for the
spinneret was set at 0 RPM. [0225] 3. The spinneret was re-set to
rotate at a rate, such as, for example, 1,000 RPM, 5,000 RPM, 3,000
RPM, 4,000 RPM, and/or 1,000-5,000 RPM. [0226] 4. The spinneret was
spun for a period of time, such as, for example, three (3) minutes,
thirty (30) minutes, and/or 3-30 minutes. [0227] 5. Spinning was
stopped to collect superfine fibers. [0228] 6. Steps 3 through 5
were repeated.
Results:
[0229] Resulting fibers included single-digit microfibers to
nanofibers. One sample of resulting superfine fibers is depicted in
FIG. 29.
Example 7
Method of Producing Composite Superfine Fibers
[0230] In some embodiments, composite fibers are made by
mechanically mixing polymers prior to and/or during melting prior
to spinning. For example, a primary polymer (e.g., .gtoreq.50% of
mixture) can be mechanically mixed with a secondary or blend
polymer (e.g., .ltoreq.50% of mixture), such as, for example,
before melting the polymers. Where it is desired to limit to
interaction between the polymers to a mechanical interaction
(rather than a chemical interaction), the secondary polymer can be
one that does not chemically interact with the primary polymer.
[0231] For purposes of this example, polycarbonate was used for the
primary polymer and blue polymer dye was used for the secondary
polymer. In other embodiments, the primary polymers can be any
suitable polymers, such as, for example, the polymers mentioned in
this disclosure (e.g., PS, PP, ABS, Agarose, and the like).
Similarly, in other embodiments, the secondary polymer can be any
suitable polymer (or other material), such as, for example, the
polymers mentioned in this disclosure (e.g., PS, PP, ABS, Agarose,
and the like). The mixture included about 95% polycarbonate and
about 5% blue dye. Composite Superfine Fibers were then created by
the melt spinning methods described herein, where the temperature
of the spinneret (and the mixture) was maintained at a temperature
above the highest melting point of the polymers, and below the
lowest degradation temperature of the two polymers. The environment
in which the superfine fibers were created was ambient air at a
temperature below the melting temperature of the mixture (e.g.,
polycarbonate and dye). It was attempted to keep the temperature of
this ambient air at RT, such as, for example, by introducing
cooling air by way of an opening (e.g., 1816 in FIG. 18,) in the
housing. However, in certain repetitions of the procedure below,
the temperature of the ambient air rose to as much as 70.degree. C.
In certain repetitions of the procedure below, a spinneret
according to FIG. 1 was used and, in others, a superfine fiber
collection device according to FIG. 8 was used. An aerodynamic wall
was placed outside of the collection wall, such as shown in FIG. 18
through FIG. 22 at a distance of about 3'' from the collection
wall.
Procedure:
[0232] 1. Melted (molten) mixture of polycarbonate and blue polymer
dye was spun in the spinneret, with the spinneret at a temperature
above the melting temperature of the polycarbonate, but below the
degradation temperature of the polycarbonate, such as, for example
300.degree. C., 350.degree. C., and/or 300-350.degree. C. [0233] 2.
RPM for the spinneret was set at 0 RPM. [0234] 3. The spinneret was
re-set to rotate at a rate, such as, for example, 1,000 RPM, 5,000
RPM, 3,000 RPM, 4,000 RPM, and/or 1,000-5,000 RPM. [0235] 4. The
spinneret was spun for a period of time, such as, for example,
three (3) minutes, thirty (30) minutes, and/or 3-30 minutes. [0236]
5. Spinning was stopped to collect superfine fibers. [0237] 6.
Steps 3 through 5 were repeated.
Results:
[0238] Resulting fibers included single-digit microfibers to
nanofibers. One sample of resulting superfine fibers is depicted in
FIG. 30.
[0239] All of the methods and apparatuses disclosed and claimed
herein can be made and executed without undue experimentation in
light of the present disclosure. Descriptions of well known
processing techniques, components and equipment have been omitted
so as not to unnecessarily obscure the present methods and
apparatuses in unnecessary detail. The descriptions of the present
methods, devices and systems are exemplary and non-limiting.
Certain substitutions, modifications, additions and/or
rearrangements falling within the scope of the claims, but not
explicitly listed in this disclosure, may become apparent to those
of ordinary skill in the art based on this disclosure. Furthermore,
it will be appreciated that in the development of a working
embodiment, numerous implementation-specific decisions must be made
to achieve the developers' specific goals, such as compliance with
system-related and business-related constraints, which will vary
from one implementation to another. While such a development effort
might be complex and time-consuming, it would nonetheless be a
routine undertaking for those of ordinary skill in the art having
the benefit of this disclosure. Additionally, it will be apparent
that certain agents that are both chemically and physiologically
related may be substituted for the agents described herein while
the same or similar results would be achieved. All such similar
substitutes and modifications apparent to those skilled in the art
are within the scope of the invention as defined by the appended
claims. For example, in certain embodiments, spinnerets are shown
as having four openings. In other embodiments, they have seven
openings. As another example, some apparatuses are shown has having
three collection rods. In other embodiments, there are twelve. As
yet another example, spinnerets are shown as rotating clockwise, in
certain embodiments. In other embodiments, the spinnerets rotate
counter-clockwise.
[0240] The claims are not to be interpreted as including
means-plus- or step-plus-function limitations, unless such a
limitation is explicitly recited in a given claim using the
phrase(s) "means for" or "step for," respectively.
REFERENCES
[0241] The following references, to the extent that they provide
exemplary procedural or other details supplementary to those set
forth herein, are specifically incorporated herein by reference.
[0242] U.S. Pat. No. 4,043,331 [0243] U.S. Pat. No. 4,044,404
[0244] U.S. Pat. No. 4,266,918 [0245] U.S. Pat. No. 4,323,525
[0246] U.S. Pat. No. 4,639,390 [0247] U.S. Pat. No. 4,657,743
[0248] U.S. Pat. No. 4,842,505 [0249] U.S. Pat. No. 5,522,879
[0250] U.S. Pat. No. 6,106,913 [0251] U.S. Pat. No. 6,111,590
[0252] U.S. Pat. No. 6,221,487 [0253] U.S. Pat. No. 6,235,392
[0254] U.S. Pat. No. 6,511,930 [0255] U.S. Pat. No. 6,596,033
[0256] U.S. Pat. No. 6,616,435 [0257] U.S. Pat. No. 6,713,011
[0258] U.S. Pat. No. 7,067,444 [0259] U.S. Pat. No. 7,083,854
[0260] U.S. Pat. No. 7,134,857
* * * * *