Patent | Date |
---|
Method for monitoring thixotropy in concrete mixing drum Grant 8,764,272 - Hazrati , et al. July 1, 2 | 2014-07-01 |
Stabilized defoamers for cementitious compositions Grant 8,759,423 - Chen , et al. June 24, 2 | 2014-06-24 |
Stabilized Defoamers For Cementitious Compositions App 20130281577 - CHEN; Ying ;   et al. | 2013-10-24 |
Slump retention in cementitious compositions Grant 8,070,875 - Jeknavorian , et al. December 6, 2 | 2011-12-06 |
Air management in cementitious mixtures having plasticizer and a clay-activity modifying agent Grant 7,972,436 - Ou , et al. July 5, 2 | 2011-07-05 |
Method For Monitoring Thixotropy In Concrete Mixing Drum App 20110029134 - Hazrati; Kati ;   et al. | 2011-02-03 |
Gluconate broth for cement and concrete admixture Grant 7,462,236 - Chun , et al. December 9, 2 | 2008-12-09 |
Slump Retention in Cementitious Compositions App 20080295741 - Jeknavorian; Ara A. ;   et al. | 2008-12-04 |
Method for enhancing flexural bond strength mortar App 20040122144 - Karkare, Milind V. ;   et al. | 2004-06-24 |
Admixture for optimizing addition of EO/PO plasticizers Grant 6,670,415 - Jardine , et al. December 30, 2 | 2003-12-30 |
Air management in cementitious mixtures having plasticizer and a clay-activity modifying agent App 20030136307 - Ou, Chia-Chih ;   et al. | 2003-07-24 |
Admixture composition for optimizing EO/PO plasticizer addition App 20020121229 - Jardine, Leslie A. ;   et al. | 2002-09-05 |
Air management in cementitious mixtures having plasticizer and a clay-activity modifying agent Grant 6,441,054 - Ou , et al. August 27, 2 | 2002-08-27 |
Admixture and method for optimizing addition of EO/PO superplasticizer to concrete containing smectite clay-containing aggregates Grant 6,352,952 - Jardine , et al. March 5, 2 | 2002-03-05 |
Mortar Admixtures And Method Of Preparing Same App 20020005149 - KARKARE, MILIND V. ;   et al. | 2002-01-17 |
Emulsified comb polymer and defoaming agent composition and method of making same Grant 6,139,623 - Darwin , et al. October 31, 2 | 2000-10-31 |
Mortar admixtures and method of preparing same Grant 5,736,600 - Karkare , et al. April 7, 1 | 1998-04-07 |
Nitrogenous strength enhancers for portland cement Grant 5,641,352 - Jeknavorian , et al. June 24, 1 | 1997-06-24 |
Hydraulic cement set-accelerating admixtures incorporating glycols Grant 5,348,583 - Arfaei , et al. September 20, 1 | 1994-09-20 |
Hydraulic cement set-accelerating admixtures incorporating glycols Grant 5,340,385 - Arfaei , et al. August 23, 1 | 1994-08-23 |