Patent | Date |
---|
Method to produce high temperature oxidation resistant metal matrix composites by fiber density grading Grant 6,214,134 - Eylon , et al. April 10, 2 | 2001-04-10 |
Method to produce high temperature oxidation resistant metal matrix composites by fiber diameter grading Grant 5,578,148 - Eylon , et al. November 26, 1 | 1996-11-26 |
Method for increasing the fracture resistance of titanium composites Grant 5,403,411 - Smith , et al. April 4, 1 | 1995-04-04 |
Post-consolidation method for increasing the fracture resistance of titanium composites Grant 5,232,525 - Smith , et al. August 3, 1 | 1993-08-03 |
Method to produce hollow titanium alloy articles Grant 5,226,982 - Eylon July 13, 1 | 1993-07-13 |
Method to manufacture titanium aluminide matrix composites Grant 5,104,460 - Smith, Jr. , et al. April 14, 1 | 1992-04-14 |
Method to produce improved property titanium aluminide articles Grant 5,098,650 - Eylon , et al. March 24, 1 | 1992-03-24 |
Method for producing very fine microstructures in titanium aluminide alloy powder compacts Grant 5,098,484 - Eylon , et al. March 24, 1 | 1992-03-24 |
Method for refining the microstructure of beta processed ingot metallurgy titanium alloy articles Grant 5,032,189 - Eylon , et al. July 16, 1 | 1991-07-16 |
Method and titanium aluminide matrix composite Grant 5,030,277 - Eylon , et al. July 9, 1 | 1991-07-09 |
Method to produce superplastically formed titanium alloy components Grant 5,024,369 - Froes , et al. June 18, 1 | 1991-06-18 |
Method for producing alpha titanium alloy pm articles Grant 4,931,253 - Eylon , et al. June 5, 1 | 1990-06-05 |
Method for producing titanium aluminide foil Grant 4,917,858 - Eylon , et al. April 17, 1 | 1990-04-17 |
System for making centrifugally cooling metal powders Grant 4,869,469 - Eylon , et al. September 26, 1 | 1989-09-26 |
Method for developing ultrafine microstructures in titanium alloy castings Grant 4,820,360 - Eylon , et al. April 11, 1 | 1989-04-11 |
Method to produce metal matrix composite articles from rich metastable-beta titanium alloys Grant 4,809,903 - Eylon , et al. March 7, 1 | 1989-03-07 |
Method for refining microstructures of blended elemental titanium powder compacts Grant 4,808,250 - Froes , et al. February 28, 1 | 1989-02-28 |
Method to produce metal matrix composite articles from lean metastable beta titanium alloys Grant 4,807,798 - Eylon , et al. * February 28, 1 | 1989-02-28 |
Method for making centrifugally cooled powders Grant 4,787,935 - Eylon , et al. November 29, 1 | 1988-11-29 |
Method for making rapidly solidified powder Grant 4,762,553 - Savage , et al. August 9, 1 | 1988-08-09 |
Method to produce metal matrix composite articles from alpha-beta titanium alloys Grant 4,733,816 - Eylon , et al. March 29, 1 | 1988-03-29 |
Method for producing very fine microstructures in titanium alloy powder compacts Grant 4,714,587 - Eylon , et al. December 22, 1 | 1987-12-22 |
Method for refining microstructures of titanium ingot metallurgy articles Grant 4,680,063 - Vogt , et al. July 14, 1 | 1987-07-14 |
Method for refining microstructures of blended elemental powder metallurgy titanium articles Grant 4,536,234 - Eylon , et al. August 20, 1 | 1985-08-20 |
Method of ion plating titanium and titanium alloys with noble metals and their alloys Grant 4,181,590 - Fujishiro , et al. January 1, 1 | 1980-01-01 |
Titanium and titanium alloys ion plated with noble metals and their alloys Grant 4,137,370 - Fujishiro , et al. January 30, 1 | 1979-01-30 |